journal article·2010-08

Influence of pH values on (Nd+Y):Al molar ratio of Nd:YAG nanopowders and preparation of transparent ceramics

Wenbin Liu, Wenxin Zhang, Jiang Li, Huamin Kou, Yiqiang Shen, Liang Wang, Yun Shi, Di Zhang, Yubai Pan

Journal of Alloys and Compounds· Volume 503· Issue 2
Publisher page

Abstract

Abstract The Nd:YAG ceramics were fabricated by vacuum sintering at 1750 °C for 20 h, where the raw nanopowders were synthesized by the co-precipitation method, and calcined at 1050 °C for 2 h. The effect of the pH values of reaction solution on the (Nd + Y):Al mole ratio of the powders was discussed here. It was found that the pH value range of 7.9–8.2 was suitable for the preparation of the Nd:YAG nanopowders. Secondary phases and pores appeared in and between the grains of Nd:YAG ceramic with the (Nd + Y):Al mole ratio of 0.576. The specimens with the (Nd + Y):Al mole ratio range of 0.598–0.603 had fine microstructures, and their transmissions were both over 80% at the near infrared wavelength. If the (Nd + Y):Al mole ratio reached 0.648, many secondary phases occurred along the grain boundaries.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Luminescence Properties of Advanced Materials · Photorefractive and Nonlinear Optics · Solid State Laser Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Sellappan · J. Am. Ceram. Soc. · 2007 · 90 · 363810.1111/j.1551-2916.2007.01913.x ↗
2. Ikesue · J. Am. Ceram. Soc. · 2006 · 89 · 193610.1111/j.1551-2916.2006.01043.x ↗
3. Yagi · Opt. Mater. · 2007 · 29 · 125810.1016/j.optmat.2006.01.033 ↗
4. Lu · Appl. Phys. Lett. · 2000 · 77 · 370710.1063/1.1331091 ↗
5. Su · J. Alloy Compd. · 2008 · 456 · 51810.1016/j.jallcom.2007.04.026 ↗
6. Huang · J. Alloy Compd. · 2009 · 478 · L1610.1016/j.jallcom.2008.11.157 ↗
7. Yang · J. Alloy Compd. · 2009 · 484 · 44910.1016/j.jallcom.2009.04.123 ↗
8. Sun · J. Alloy Compd. · 2004 · 379 · L110.1016/j.jallcom.2004.02.030 ↗
9. Li · J. Alloy Compd. · 2009 · 485 · 56110.1016/j.jallcom.2009.06.026 ↗
10. Hakuta · Mater. Res. Bull. · 2003 · 38 · 125710.1016/S0025-5408(03)00088-6 ↗
11. Chen · J. Alloy Compd. · 2007 · 433 · 32810.1016/j.jallcom.2006.06.084 ↗
12. Wu · J. Alloy Compd. · 2009 · 472 · 57610.1016/j.jallcom.2008.05.031 ↗
13. Su · J. Alloy Compd. · 2009 · 470 · 30610.1016/j.jallcom.2008.02.045 ↗
14. Li · J. Mater. Res. · 2000 · 15 · 186410.1557/JMR.2000.0269 ↗
15. Li · J. Mater. Res. · 2000 · 15 · 151410.1557/JMR.2000.0217 ↗
16. Lu · Jpn. J. Appl. Phys. Lett. · 2000 · 39 · L104810.1143/JJAP.39.L1048 ↗
17. Tong · Mater. Lett. · 2007 · 61 · 428710.1016/j.matlet.2007.01.087 ↗
18. Nien · Mater. Chem. Phys. · 2005 · 93 · 7910.1016/j.matchemphys.2005.02.017 ↗
19. Apte · J. Mater. Res. · 1992 · 7 · 70610.1557/JMR.1992.0706 ↗
20. Ikesue · J. Mater. Sci. · 1999 · 34 · 118910.1023/A:1004548620802 ↗
21. Ikesue · J. Am. Ceram. Soc. · 1997 · 80 · 151710.1111/j.1151-2916.1997.tb03011.x ↗