journal article·2009-11

Influence on luminescent properties of the Sr2MgSi2O7: Eu2+ by Dy3+, Nd3+ co-doping

Haoyi Wu, Yihua Hu, Yinhai Wang, Bodai Zeng, Zhongfei Mou, Liuyong Deng, Wei Xie

Journal of Alloys and Compounds· Volume 486· Issue 1-2
Publisher page

Abstract

Abstract The long afterglow phosphors Sr 1.97 MgSi 2 O 7 : Eu 0.01 2+ , Dy 0.02− x 3+ , Nd x 3+ ( x = 0, 0.01, 0.02) and Sr 1.99 MgSi 2 O 7 : Eu 0.01 2+ were prepared by the high-temperature solid state reaction. The doping Dy 3+ or Nd 3+ has no influence on both the crystal phase and the emission peak. The afterglow of the Sr 2 MgSi 2 O 7 : Eu 2+ is obtained. With the increase of the substitution of Nd 3+ for Dy 3+ , the decay constants of the afterglow decrease. The thermoluminescence curves of the samples which imply the decline of the trap depth correspond to this phenomenon. The increase of the density of the traps and the decline of the trap depth may be due to the introduction of cation vacancies. The substitution of Nd 3+ for Dy 3+ also causes decline of the trap depth for the influence of the disturbances in the crystal decreases.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Luminescence Properties of Advanced Materials · Radiation Detection and Scintillator Technologies · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Chen · J. Lumin. · 2006 · 118 · 7010.1016/j.jlumin.2005.05.011 ↗
2. Omkaram · J. Alloys Compd. · 2009 · 474 · 56510.1016/j.jallcom.2008.06.140 ↗
3. Tan · J. Alloys Compd. · 2009 · 477 · 64810.1016/j.jallcom.2008.10.085 ↗
4. Liu · J. Alloys Compd. · 2009 · 470 · 47310.1016/j.jallcom.2008.03.001 ↗
5. Xu · Ceram. Int. · 2008 · 34 · 211710.1016/j.ceramint.2007.08.012 ↗
6. Pan · J. Lumin. · 2008 · 128 · 197510.1016/j.jlumin.2008.06.009 ↗
7. Liu · J. Alloys Compd. · 2005 · 387 · 6510.1016/j.jallcom.2004.06.061 ↗
8. Jiang · Mater. Lett. · 2004 · 58 · 182510.1016/j.matlet.2003.11.014 ↗
9. Fei · J. Alloys Compd. · 2005 · 390 · 13310.1016/j.jallcom.2004.06.096 ↗
10. Alvani · J. Lumin. · 2005 · 115 · 14710.1016/j.jlumin.2005.03.009 ↗
11. Aitasalo · Radiat. Meas. · 2007 · 42 · 64410.1016/j.radmeas.2007.01.058 ↗
12. Lin · Mater. Chem. Phys. · 2001 · 70 · 15610.1016/S0254-0584(00)00500-9 ↗
13. Yamamoto · J. Lumin. · 1997 · 72–74 · 28710.1016/S0022-2313(97)00012-4 ↗
14. Song · J. Alloys Compd. · 2008 · 458 · 56410.1016/j.jallcom.2007.04.261 ↗
15. Aitasalo · J. Alloys Compd. · 2004 · 380 · 410.1016/j.jallcom.2004.03.007 ↗
16. Jia · J. Appl. Phys. · 2007 · 101
17. Chen · J. Lumin. · 2008 · 128 · 118010.1016/j.jlumin.2007.11.094 ↗
18. Shi · J. Lumin. · 2007 · 122–123 · 1110.1016/j.jlumin.2006.01.066 ↗
19. Lakshminarasimhan · Mater. Res. Bull. · 2008 · 43 · 294610.1016/j.materresbull.2007.12.005 ↗
20. Lin · Appl. Phys. Lett. · 2002 · 86 · 99610.1063/1.1490631 ↗
21. Aitasalo · J. Phys. Chem. B · 2006 · 110 · 458910.1021/jp057185m ↗
22. Yuan · J. Alloys Compd. · 2004 · 377 · 26810.1016/j.jallcom.2004.01.063 ↗
23. Kubo · J. Cryst. Growth · 2005 · 275 · e176710.1016/j.jcrysgro.2004.11.193 ↗
24. Furusho · J. Lumin. · 2008 · 128 · 88110.1016/j.jlumin.2007.11.047 ↗
25. Hölsä · J. Alloys Compd. · 2004 · 374 · 5610.1016/j.jallcom.2003.11.064 ↗