journal article·2008-04

Effect of aging treatment on microstructure and mechanical properties of Cu–Ag alloys

J. Lin, L. Meng

Journal of Alloys and Compounds· Volume 454· Issue 1-2
Publisher page

Abstract

Abstract Cu–6 wt.%Ag, Cu–12 wt.%Ag and Cu–24 wt.%Ag alloys were prepared by vacuum melting, solution treating at 740 °C for 4 h and aging at 450 °C for different times. The effect of aging treatment was investigated by observing the microstructure and determining the hardness. During aging treatment, discontinuous precipitation reaction can occur along high-angle grain boundaries and continuous precipitation reaction within Cu dendritic arms. Abundant high-angle grain boundaries result in a precipitation reaction that is predominantly discontinuous in Cu–6 wt.%Ag while net-like eutectic colonies surrounding Cu dendritic arms result in a precipitation reaction that is predominantly continuous in Cu–24 wt.%Ag. In Cu–12 wt.%Ag, continuous precipitates within Cu dendrites coexist with discontinuous precipitates next to high-angle grain boundaries. Aging only for 1 h can significantly increase the hardness although the precipitation reaction is insufficient. The increasing rate of the hardness becomes slow as aging time longer than 1 h. The hardness keeps approximately constant for Cu–12 wt.%Ag and Cu–24 wt.%Ag and slightly decreases for Cu–6 wt.%Ag with increasing aging time from 16 to 37 h. The precipitation reaction during aging treatment has more significant hardening benefit to the alloys with lower Ag contents.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Kindo · Physica B · 2001 · 294–295 · 58510.1016/S0921-4526(00)00725-0 ↗
2. Herrmannsdoerfer · J. Low Temp. Phys. · 2003 · 133 · 4110.1023/A:1025680916320 ↗
3. Swenson · IEEE Trans. Appl. Supercond. · 2004 · 14 · 123310.1109/TASC.2004.830538 ↗
4. Spencer · Adv. Eng. Mater. · 2004 · 6 · 123310.1002/adem.200400014 ↗
5. Wood · Acta Mater. · 1997 · 45 · 109910.1016/S1359-6454(96)00220-0 ↗
6. Ortenberg · Physica B · 2001 · 294–295 · 56810.1016/S0921-4526(00)00722-5 ↗
7. Hong · Acta Mater. · 1995 · 43 · 331310.1016/0956-7151(95)00050-6 ↗
8. Sakai · Appl. Phys. Lett. · 1991 · 59 · 296510.1063/1.105813 ↗
9. Freudenberger · Cryogenics · 2006 · 46 · 72410.1016/j.cryogenics.2006.06.002 ↗
10. Grünberger · Physica B · 2001 · 294–295 · 64310.1016/S0921-4526(00)00735-3 ↗
11. Pantsyrnyi · Physica B · 2001 · 294–295 · 66910.1016/S0921-4526(00)00741-9 ↗
12. Benghalem · Acta Mater. · 1997 · 45 · 39710.1016/S1359-6454(96)00152-8 ↗
13. Liu · Mater. Sci. Eng. A · 2006 · 418 · 32010.1016/j.msea.2005.12.001 ↗
14. Herlach · Physica B · 2001 · 294–295 · 50010.1016/S0921-4526(00)00710-9 ↗
15. Thilly · Physica B · 2001 · 294–295 · 64810.1016/S0921-4526(00)00736-5 ↗
16. Liu · J. Alloy. Compd. · 2006 · 425 · 18510.1016/j.jallcom.2006.01.061 ↗
17. Sakai · Acta Mater. · 1997 · 45 · 101710.1016/S1359-6454(96)00248-0 ↗
18. Hong · Acta Mater. · 1998 · 46 · 411110.1016/S1359-6454(98)00106-2 ↗
19. Hong · Mater. Sci. Eng. A · 1999 · 264 · 15110.1016/S0921-5093(98)01097-1 ↗
20. Zhang · Scr. Mater. · 2005 · 52 · 58710.1016/j.scriptamat.2004.11.035 ↗
21. Morris · Scr. Mater. · 1999 · 41 · 112310.1016/S1359-6462(99)00262-6 ↗
22. Raabe · Acta Mater. · 1998 · 46 · 597310.1016/S1359-6454(98)00218-3 ↗
23. Grünberger · Z. Metallk. · 2002 · 93 · 5810.3139/146.020058 ↗
24. Gaganov · Z. Metallk. · 2004 · 95 · 42510.3139/146.017986 ↗