journal article·2008-07

Preparation and characterization of autocatalytic low phosphorus nickel coatings containing submicron silicon nitride particles

J.N. Balaraju, K.S. Rajam

Journal of Alloys and Compounds· Volume 459· Issue 1-2
Publisher page

Abstract

This paper addresses the structural characteristics and phase transformation behavior of plain electroless Ni-P and Ni-P-Si3N4 composite coatings. Composite coatings were prepared using a low phosphorus electroless nickel bath containing 1 and 5 g/L submicron silicon nitride particles at pH 6.5 and temperature 85 +/- 2 degrees C. Deposition rate was around 6 mu m/h for both plain and composite coatings. The amount of silicon nitride particles codeposited in the Ni-P matrix is 3.5 wt.% (N1) and 4.5 wt.% (N2) with the addition of I and 5 g/L particles in the bath. Deposit surface composition analysis carried out by energy-dispersive analysis of X-ray (EDX) results shows that plain Ni-P and Ni-P-Si3N4 deposits are having around 3.5 wt.% phosphorus. The X-ray diffraction (XRD) patterns of Ni-P-Si3N4 coatings are very similar to that of plain electroless Ni-P coating in as-deposited condition. Presence of a single high intensity peak at 44.8 degrees 20 which corresponds to Ni(111) peak is present in both deposits. Presence of Ni(2 0 0) and (2 2 0) peaks is also observed in composite coatings apart from Ni(I 1 1) peak. The calculated grain size using Debye-Scherrer method for both deposits is between 11 and 14 nm. It shows that inclusion of silicon nitride particles has a marginal influence on the grain size of the composite coatings. Optical micrographs of deposit cross-sections reveal that particles incorporation is uniform throughout the thickness of the coating. Anodically etched metallographic cross-sections of both deposits revealed no banded/lamellar structure. It shows that the phosphorous content in the deposit is uniform. This was confirmed with the cross-sectional scanning electron microscope (SEM)-EDX carried out on the deposits. A marginal variation in phosphorus concentration is observed. Phase transformation behavior studied at different scanning rates by differential scanning calorimeter (DSC) indicates that there is a slight increase in crystallization temperature around 20 degrees C with the incorporation of silicon nitride particles compared to plain Ni-P coatings. Microhardness measurements made on the cross-section of as-deposited coatings showed that there is about 15% improvement in microhardness with the codeposition of silicon nitride particles in Ni-P matrix.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Electrocatalysts for Energy Conversion · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Mallory · 1990
2. Xiang · Plat. Surf. Finish. · 2001 · 88 · 64
3. Jiaqiang · Surf. Coat. Technol. · 2006 · 200 · 583610.1016/j.surfcoat.2005.08.134 ↗
4. Sarret · Surf. Coat. Technol. · 2006 · 201 · 38910.1016/j.surfcoat.2005.11.127 ↗
5. Jiaqiang · Mater. Lett. · 2005 · 59 · 39110.1016/j.matlet.2004.09.032 ↗
6. Jiaqiang · Plat. Surf. Finish. · 2004 · 91 · 74
7. Sharma · Trans. Indian Inst. Met. · 2003 · 56 · 583
8. Riedel · 1991
9. J.N. Balaraju, Ph.D. thesis, I.I.T. Madras, Chennai, 2000.
10. Balaraju · J. App. Chem. · 2003 · 33 · 807
11. Hamid · Plat. Surf. Finish. · 1999 · 86 · 136
12. Monir Vaghefi · Surf. Coat. Technol. · 2003 · 168 · 25910.1016/S0257-8972(02)00926-X ↗
13. Hui · Plat. Surf. Finish. · 2004 · 91 · 66
14. Alirezaei · Surf. Coat. Technol. · 2004 · 184 · 17010.1016/j.surfcoat.2003.11.013 ↗
15. Balaraju · Surf. Coat. Technol. · 2006 · 200 · 393310.1016/j.surfcoat.2005.03.007 ↗
16. Yucheng · Z. Metallkd. · 2000 · 91 · 788
17. Novakovic · Surf. Coat. Technol. · 2006 · 201 · 89510.1016/j.surfcoat.2006.01.005 ↗
18. Jiaquiang · Surf. Coat. Technol. · 2006 · 200 · 583610.1016/j.surfcoat.2005.08.134 ↗
19. Yating · J. Mater. Sci. · 2005 · 40 · 505710.1007/s10853-005-1807-0 ↗
20. Agarwala · Sadhana · 2003 · 28 · 47510.1007/BF02706445 ↗
21. Apachitei · Surf. Coat. Technol. · 2002 · 149 · 26310.1016/S0257-8972(01)01492-X ↗
22. Hentschel · Acta Mater. · 2000 · 48 · 93310.1016/S1359-6454(99)00371-7 ↗
23. Apachitei · Surf. Coat. Technol. · 2001 · 148 · 28410.1016/S0257-8972(01)01337-8 ↗
24. Keong · J. Mater. Sci. · 2002 · 37 · 444510.1023/A:1020641611389 ↗
25. Balaraju · Mater. Res. Bull. · 2006 · 41 · 84710.1016/j.materresbull.2005.09.024 ↗
26. Rajiv · J. Mater. Sci. · 1993 · 28 · 175810.1007/BF00595742 ↗
27. Jackson · Tans. Inst. Met. Finish. · 1990 · 68 · 7510.1080/00202967.1990.11870871 ↗
28. Bayes · Trans. Inst. Met. Finish. · 1991 · 69 · 14010.1080/00202967.1991.11870910 ↗
29. Zhang · J. Mater. Sci. Lett. · 1998 · 17 · 3710.1023/A:1006537506800 ↗
30. Wu · Surf. Eng. · 2000 · 16 · 50610.1179/026708400101517521 ↗