Abstract

Abstract The reaction steps in mixtures of 2LiNH2–MgH2 during hydrogen sorption are investigated. Differential scanning calorimetry experiments at various H2 pressures show that the initial decomposition comprises several steps and their transition temperature depends on the applied hydrogen pressure. During the first desorption of the powders, an exothermic phase transition takes place where Mg ( NH 2 ) 2 is partially formed. This is followed by an endothermic decomposition that yields hydrogen. The addition of 2 mol% TiCl 3 to the initial 2LiNH2–MgH2 mixture does not affect the exothermic phase transition but the hydrogen release shifts to lower temperatures. Adding 2 mol% TiCl3 after two hydrogenation cycles to the material has no effect on the desorption properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen Storage and Materials · Ammonia Synthesis and Nitrogen Reduction · Hybrid Renewable Energy Systems

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. Vajo · J. Phys. Chem. B · 2005 · 109 · 371910.1021/jp040769o ↗
2. Chen · Nature · 2002 · 420 · 30210.1038/nature01210 ↗
3. Luo · J. Alloys Compd. · 2005 · 404–406 · 39210.1016/j.jallcom.2005.01.131 ↗
4. Luo · J. Alloys Compd. · 2006 · 407 · 27410.1016/j.jallcom.2005.06.046 ↗
5. Ichikawa · J. Power Sources · 2006 · 159 · 12610.1016/j.jpowsour.2006.04.003 ↗
6. Leng · J. Phys. Chem. B · 2006 · 120 · 1296410.1021/jp061120h ↗
7. Kircher · J. Appl. Phys. · 2004 · 95 · 774810.1063/1.1751634 ↗
8. Xiong · J. Alloys Compd. · 2005 · 398 · 23510.1016/j.jallcom.2005.02.010 ↗
9. Leng · J. Power Sources · 2006 · 156 · 16610.1016/j.jpowsour.2005.03.228 ↗
10. Linde · Z. Anorg. Allg. Chem. · 1974 · 409 · 19910.1002/zaac.19744090209 ↗
11. Kojima · J. Alloys Compd. · 2005 · 395 · 23610.1016/j.jallcom.2004.10.063 ↗
12. Nortake · J. Alloys Compd. · 2005 · 393 · 26410.1016/j.jallcom.2004.09.063 ↗