Effect of reflow time on interfacial reaction and shear strength of Sn–0.7Cu solder/Cu and electroless Ni–P BGA joints

Jeong-Won Yoon, Sang-Won Kim, Seung-Boo Jung

Journal of Alloys and Compounds· Volume 385· Issue 1-2
Publisher page

Abstract

Abstract The interfacial reaction and shear strength between the eutectic Sn–0.7 wt.% Cu solder and two different kinds of ball grid array (BGA) substrates (Cu and Au/Ni–P/Cu) during reflow at 255 °C for up to 30 min were studied. With the solder joints between the Sn–0.7Cu solder and Cu substrates, a Cu 6 Sn 5 intermetallic compound (IMC) was formed at the interface. In the case of the electroless Ni–P substrate, the IMC formed at the interface was mainly (Cu, Ni) 6 Sn 5 . Also, a P-rich Ni (Ni 3 P) layer was observed as a by-product of the Cu–Ni–Sn reaction. The Ni 3 P layer was between the (Cu, Ni) 6 Sn 5 IMC and the electroless Ni–P layer. The thickness of the Cu 6 Sn 5 , (Cu, Ni) 6 Sn 5 and Ni 3 P layer was found to increase with the reaction time. The growth of the Cu 6 Sn 5 IMC layer for Cu substrate was faster than that of the (Cu, Ni) 6 Sn 5 IMC layer for electroless Ni–P substrate. The Ni content in the (Cu, Ni) 6 Sn 5 IMC layer formed at the interface increased with increasing reaction time. In the ball shear tests, the shear strength value did not change much as a function of reflow time. In all samples, the fracture mainly occurred in the bulk solder. However, for the Sn–0.7Cu/electroless Ni–P joint reflowed for 10 min, the fracture occurred in ductile and slightly brittle mode.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Chen · J. Mater. Res · 2002 · 17 · 26310.1557/JMR.2002.0036 ↗
2. Chen · J. Electron. Mater · 2003 · 32 · 128410.1007/s11664-003-0024-3 ↗
3. Zeng · Mater. Sci. Eng. R · 2002 · 38 · 5510.1016/S0927-796X(02)00007-4 ↗
4. Frear · JOM · 2001 · 53 · 2810.1007/s11837-001-0099-3 ↗
5. He · Acta Mater · 2004 · 52 · 204710.1016/j.actamat.2003.12.042 ↗
6. Yoon · J. Electron. Mater · 2003 · 32 · 119510.1007/s11664-003-0011-8 ↗
7. Wang · Scripta Mater · 2003 · 49 · 81310.1016/S1359-6462(03)00486-X ↗
8. Yoon · Mater. Trans · 2002 · 43 · 182110.2320/matertrans.43.1821 ↗
9. J.W. Yoon, S.B. Jung, J. Alloys Comp. (2004) (in press).
10. Jang · J. Appl. Phys · 2000 · 88 · 635910.1063/1.1321787 ↗
11. Alam · Microelectron. Reliab · 2002 · 42 · 106510.1016/S0026-2714(02)00068-9 ↗
12. Chan · J. Electron. Mater · 2002 · 31 · 111710.1007/s11664-002-0051-5 ↗
13. Zeng · IEEE Trans. Electron. Pack. Manuf · 2002 · 25 · 16210.1109/TEPM.2002.801648 ↗
14. Lee · Mater. Trans · 2002 · 43 · 75110.2320/matertrans.43.751 ↗
15. Yoon · Mater. Trans · 2004 · 45 · 72710.2320/matertrans.45.727 ↗
16. Chen · J. Electron. Mater · 2003 · 32 · 118810.1007/s11664-003-0010-9 ↗
17. Ho · J. Electron. Mater · 2002 · 31 · 58410.1007/s11664-002-0129-0 ↗