Growth kinetics of Ni3Sn4 and Ni3P layer between Sn–3.5Ag solder and electroless Ni–P substrate
Source abstract
Abstract
Abstract Interfacial reactions and growth kinetics of intermetallic compound (IMC) layers formed between Sn–3.5Ag solder and electroless Ni–P substrate were investigated at temperature between 100 and 170 °C for up to 60 days. The IMC formed at the interface was mainly Ni3Sn4. Also, a P-rich Ni (Ni3P) layer was observed as a by-product of the Ni–Sn reaction. The Ni3P layer was between the Ni3Sn4 IMC and the electroless Ni–P deposit layer. The thickness results fitted a power-law relationship with exponent of 0.4 for the Ni3Sn4 layer. The interface between electroless Ni–P and Ni3P was planar and the thickness of the Ni3P layer also was found to increase linearly with the square root of aging time. The thickness of the Ni3Sn4 and Ni3P layer reached about 3 and 2 μm after 60 days of aging at 170 °C, respectively. The activation energy for the growth of the Ni3Sn4 IMC equals 49 kJ/mol.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Intermetallics and Advanced Alloy Properties · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Zeng · Mater. Sci. Eng. R. · 2002 · 38 · 5510.1016/S0927-796X(02)00007-4 ↗
2. Yoon · J. Electron. Mater. · 2003 · 32 · 119510.1007/s11664-003-0011-8 ↗
3. Alam · J. Electron. Mater. · 2002 · 31 · 111710.1007/s11664-002-0051-5 ↗
4. Takemoto · J. Mater. Sci. · 1991 · 32 · 407710.1023/A:1018653924450 ↗
5. Yoon · Mater. Trans. · 2002 · 43 · 182110.2320/matertrans.43.1821 ↗
6. Suganuma · J. Mater. Res. · 1998 · 13 · 285910.1557/JMR.1998.0391 ↗
7. Yoon · J. Alloys Comp. · 2003 · 359 · 20210.1016/S0925-8388(03)00291-3 ↗
8. Jang · J. Appl. Phys. · 2000 · 88 · 635910.1063/1.1321787 ↗
9. Abtew · Mater. Sci. Eng. R. · 2000 · 27 · 9510.1016/S0927-796X(00)00010-3 ↗
10. Wang · Scripta Mater. · 2003 · 49 · 81310.1016/S1359-6462(03)00486-X ↗
11. Yoon · Met. Mater. Int. · 2003 · 9 · 19310.1007/BF03027277 ↗
12. Prakash · J. Electron. Mater. · 2003 · 32 · 93910.1007/s11664-003-0227-7 ↗
13. Alam · J. Appl. Phys. · 2003 · 94 · 410810.1063/1.1602563 ↗
14. Zeng · IEEE Trans. Electron. Pack. Manuf. · 2002 · 25 · 16210.1109/TEPM.2002.801648 ↗
15. Jeon · J. Electron. Mater. · 2002 · 31 · 52010.1007/s11664-002-0109-4 ↗
16. Alam · Microelectron. Reliab. · 2002 · 42 · 106510.1016/S0026-2714(02)00068-9 ↗
17. Flanders · J. Electron. Mater. · 1997 · 26 · 88310.1007/s11664-997-0268-4 ↗
18. Choi · J. Electron. Mater. · 1999 · 28 · 120910.1007/s11664-999-0159-y ↗
19. S.B. Jung, Doctoral Thesis, Osaka University, Japan, 1993.
20. Vianco · J. Electron. Mater. · 1995 · 24 · 149310.1007/BF02655468 ↗
21. Jang · J. Appl. Phys. · 1999 · 85 · 845610.1063/1.370627 ↗
22. Gur · Acta Mater. · 1998 · 46 · 491710.1016/S1359-6454(98)00192-X ↗
23. Tu · Scripta Mater. · 2001 · 44 · 31710.1016/S1359-6462(00)00590-X ↗