Thermoelectric properties of NaCo2O4
Source abstract
Abstract
Abstract The thermoelectric properties such as the thermal conductivity, electrical resistivity and Seebeck coefficient of NaCo 2 O 4 and NaCo 1.9 M 0.1 O 4 (M=Ti, Rh, Pd) were evaluated in the temperature range from room temperature to 723 K. Polycrystalline samples were prepared by sintering in air followed by hot pressing. The thermal conductivity was calculated from the heat capacity, the experimental density, and the thermal diffusivity measured by the laser flash method. The electrical resistivity and Seebeck coefficient were measured simultaneously using ULVAC ZEM-1 in He atmosphere. The dimensionless figure of merit, ZT , of NaCo 1.9 Pd 0.1 O 4 was higher than that of NaCo 2 O 4 over a wide range of temperatures, and reached ZT =0.045 at 723 K.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Magnetic and transport properties of perovskites and related materials · Advanced Condensed Matter Physics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (7)
Show source-provided references
1. Terasaki · Phys. Rev. B · 1997 · 56 · R1268510.1103/PhysRevB.56.R12685 ↗
2. Japan Thermal Measurement Society, Thermodynamics Database For Personal Computer MALT2.
3. Maxwell · 1891 · Vol. 1
4. A.E. Eucken, Forsch. Gebiete Ingenieurw. B3, Forschungsheft, No. 353, 1932, p. 16.
5. Yakabe · 1997 · 523
6. Kawata · Phys. Rev. B · 1999 · 60 · 1058410.1103/PhysRevB.60.10584 ↗
7. Ando · Phys. Rev. B · 1999 · 60 · 1058010.1103/PhysRevB.60.10580 ↗