journal article·2026-02Open access

Synergistic improvement in mechanical properties of Mg–Zn–Y alloys with Mille–Feuille structure by prestrain introduction and grain refinement

Shin-ichi Inoue, Yoshihito Kawamura

Abstract

In this study, we attempted to enhance the mechanical properties of the Mille–Feuille (MF)-type Mg–0.4Zn–1.0Y (at.%) alloy prepared by a conventional casting technique. Previous studies have shown that extruded MF-type Mg–0.4Zn–1.0Y (at.%) alloys prepared by rapid solidification exhibit high cluster-arranged nanoplate (CANaP) dispersion, resulting in numerous kinks and demonstrating excellent yield strength with moderate ductility. In contrast, the extruded MF-type Mg–0.4Zn–1.0Y (at.%) alloy produced by casting exhibits low CANaP dispersion, resulting in reduced kink deformation and significantly inferior mechanical properties. CANaPs form owing to the enrichment of L1 2 clusters (Zn 6 Y 8 ) on stacking faults. Therefore, introducing strain before aging treatment is expected to promote CANaP formation. The extruded MF-type Mg–0.4Zn–1.0Y (at.%) alloy with 10% precompression exhibited an approximately 1.7 times increase in the dispersion of CANaPs, increasing kink boundary dispersion. As a result, the extruded MF-type Mg–0.4Zn–1.0Y (at.%) alloy subjected to 10% precompression exhibited a yield strength of 359 MPa and an elongation of 6%. The extruded MF-type Mg–0.4Zn–1.0Y–0.1Zr (at.%) alloy subjected to 10% precompression exhibited a yield strength of 388 MPa and an elongation of 7.2%, demonstrating mechanical properties comparable to those of MF-type alloys produced by rapid solidification. • Precompression before aging treatment helped promote the formation of CANaPs. • The extruded Mg–Zn–Y alloy with 10% precompression exhibited a yield strength of 359 MPa. • With Zr addition, area fraction of high-KAM-region in α-Mg grains increased after precompression. • The extruded Mg–Zn–Y–Zr alloy with precompression exhibited a yield strength of 388 MPa.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Weight loss with magnesium alloys10.1126/science.1182848 ↗
2. The science, technology, and applications of magnesium10.1007/s11837-998-0411-6 ↗
3. Recent magnesium alloy development for elevated temperature applications10.1179/095066004225010497 ↗
4. Review on Research and Development of Magnesium Alloys10.1016/S1006-7191(08)60054-X ↗
5. Tensile properties of extruded ZK60–RE alloys10.1016/S0921-5093(02)00740-2 ↗
6. The effect of precipitates on the mechanical properties of ZK60-Y alloy10.1016/j.msea.2006.01.092 ↗
7. Comparison of the microstructure and mechanical properties of a ZK60 alloy with and without 1.3 wt% gadolinium addition10.1016/j.msea.2006.06.063 ↗
8. Microstructures and tensile properties of Mg–8Gd–0.6Zr–xNd–yY (x + y = 3, mass%) alloys10.1016/j.msea.2006.06.043 ↗
9. Magnesium: properties — applications — potential10.1016/S0921-5093(00)01351-4 ↗
10. Precipitation in magnesium alloy WE54 during isothermal ageing at 250°C10.1016/S1359-6462(99)00084-6 ↗
11. Microstructure evolution in isochronally heat treated Mg-Gd alloys10.1002/(SICI)1521-396X(199910)175:2<491::AID-PSSA491>3.0.CO;2-F ↗
12. Microstructure evolution in a Mg–15Gd–0.5Zr (wt%) alloy during isothermal aging at 250 °C10.1016/j.msea.2006.06.018 ↗
13. Rapidly solidified power metallurgy Mg97Zn1Y2 alloys with excellent tensile strength above 600 MPa10.2320/matertrans.42.1172 ↗
14. Nanocrystalline LPSO Mg-Zn-Y-Al alloys with high mechanical strength and corrosion resistance10.4028/www.scientific.net/MSF.638-642.1476 ↗
15. Microstructure and mechanical properties of extruded Mg-Zn-Y alloys with 14H long period ordered structure10.2320/matertrans.47.959 ↗
16. Formation and mechanical properties of Mg97Zn1RE2 alloys with long-period stacking ordered structure10.2320/matertrans.MER2007142 ↗
17. Effect of long-period stacking ordered phase on mechanical properties of Mg97Zn1Y2 extruded alloy10.1016/j.actamat.2010.07.050 ↗
18. Effect of multimodal microstructure evolution on mechanical properties of Mg-Zn-Y extruded alloy10.1016/j.actamat.2011.02.038 ↗
19. Polytypes of long-period stacking structures synchronized with chemical order in a dilute Mg–Zn–Y alloy10.1080/09500839.2011.609149 ↗
20. The structure of long period stacking/order Mg–Zn–RE phases with extended non-stoichiometry ranges10.1016/j.actamat.2011.09.030 ↗
21. A type of plastic deformation new in metals10.1038/149643a0 ↗
22. Structure and nature of kink bands in zinc
23. Room-temperature ductile carbides10.1007/s11661-999-0325-0 ↗
24. Dislocations, kink bands, and room-temperature plasticity of Ti3SiC210.1007/s11661-999-0172-z ↗
25. High-resolution transmission electron microscopy study of a low-angle boundary in plastically deformed Ti3SiC210.1080/095008399177390 ↗
26. Fully reversible, dislocation-based compressive deformation of Ti3SiC2 to 1 GPa10.1038/nmat814 ↗
27. Controlled microstructures of Al-CuAl2 eutectic composites and their compressive properties
28. Strain fields induced by kink band propagation in Cu-Nb nanolaminate composites10.1016/j.actamat.2017.04.050 ↗
29. Kink deformation in a beta titanium alloy at high strain rate10.1016/j.msea.2017.07.015 ↗
30. Inducement of kink-band formation in directionally solidified Mg/Mg17Al12 eutectic alloy - inspired by the deformation behavior of the long-period stacking ordered (LPSO) phase10.1016/j.msea.2020.140087 ↗
31. Kink-band formation in directionally solidified Mg/Mg2Yb and Mg/Mg2Ca eutectic alloys with Mg/Laves-phase lamellar microstructure10.1016/j.jma.2021.02.006 ↗
32. Control of kink-band formation in mille-feuille structured Al/Al2Cu eutectic alloys10.1016/j.msea.2021.141849 ↗
33. Effects of a preannealing process on the morphology of developed kinks in Mille-Feuille structured Cu/A5052 alloy fabricated by accumulative roll bonding: criteria for kink formation10.2320/matertrans.MT-MD2022003 ↗
34. Tiny kink-band formation in Fe-Co-Mn-Ni-Ti multi-element alloys10.1016/j.jallcom.2025.180487 ↗
35. Kink bands and strengthening of millefeuille-structured magnesium alloys by cluster-arranged nanoplates (CANaPs): The case of Mg-0.4Zn-1.0Y alloy10.1016/j.jallcom.2022.168607 ↗
36. Kawamura · J. Alloy. Compd. · 2025 · 101210.1016/j.jallcom.2025.178454 ↗
37. Advantages of rapid solidification over casting of Mg-0.4Zn-1Y10.1016/j.jma.2024.06.024 ↗
38. Mechanism-based strain gradient plasticity— I. Theory10.1016/S0022-5096(98)00103-3 ↗
39. Geometrically necessary dislocations and strain-gradient plasticity: a few critical issues10.1016/S1359-6462(02)00335-4 ↗
40. About quantitative EBSD analysis of deformation and recovery substructures in pure Tantalum10.1088/1757-899X/89/1/012038 ↗
41. Effect of multimodal microstructure evolution on mechanical properties of Mg–Zn–Y extruded alloy10.1016/j.actamat.2011.02.038 ↗
42. Nanoclusters first: a hierarchical phase transformation in a novel Mg alloy10.1038/srep14186 ↗
43. Quantitative estimation of kink-band strengthening in an Mg–Zn–Y single crystal with LPSO nanoplates10.1080/21663831.2021.1974593 ↗
44. Strengthening of Mg-based long-period stacking ordered (LPSO) phase with deformation kink bands10.1016/j.msea.2019.138163 ↗
45. Strengthening mechanisms acting in extruded Mg-based long-period stacking ordered (LPSO)-phase alloys10.1016/j.actamat.2018.10.016 ↗
46. Numerical investigation of kink strengthening mechanism due to kink band in long-period stacking ordered magnesium alloy10.2320/matertrans.MT-MD2022006 ↗
47. Kink strengthening mechanism due to multiple kink bands in long-period stacking ordered magnesium alloy10.1016/j.commatsci.2025.114428 ↗
48. Microstructure and mechanical properties of caliber rolled Mg–Y–Zn alloys
49. Unveiling the role of DRXed grain orientation configuration in the deformation behavior of Mg alloys with bimodal grain structures10.1016/j.jmst.2025.09.062 ↗
50. Tailoring bimodal grain structure to achieve simultaneous improvement of strength and ductility in magnesium alloys at cryogenic temperatures10.1016/j.jma.2025.09.015 ↗
51. TThe contributions of grain size, dislocation density and twinning to the strength of a magnesium alloy processed by ECAP10.1016/j.msea.2010.09.048 ↗
52. Microstructure and mechanical property tailoring in asymmetrically shear-extruded Mg-2.0Al-0.8Sn-0.5Ca alloys via Zn addition10.3390/cryst15080735 ↗
53. Relation between corrosion behavior and microstructure of Mg–Zn–Y alloys prepared by rapid solidification at various cooling rates10.1016/j.corsci.2008.11.003 ↗
54. Influence of crystallographic orientation and Al alloying on the corrosion behaviour of extruded α-Mg/LPSO two-phase Mg-Zn-Y alloys with multimodal microstructure10.1016/j.corsci.2022.110237 ↗