Enhanced compatibility of Al-modulated Al NiCoFeCr high-entropy alloy and microstructure degradation under static oxygen-saturated lead bismuth eutectic
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: High Entropy Alloys Studies · High-Temperature Coating Behaviors · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (66)
Show source-provided references
1. Handbook on lead-bismuth eutectic alloy and lead properties, materials compatibility
2. Lead–B ismuth eutectic (LBE): a coolant candidate for Gen. IV advanced nuclear reactor concepts10.1002/adem.201300296 ↗
3. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
4. Corrosion scales on various steels after exposure to liquid lead–bismuth eutectic10.1016/j.jnucmat.2013.09.034 ↗
5. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.jnucmat.2017.04.004 ↗
6. Influence of cold work on solution-based attack on 1.4970 (15-15Ti) austenitic steel in static liquid lead-bismuth eutectic at 550 °C and≤ 10−8 mass% dissolved Oxygen
7. Characterization of corrosion phenomena and kinetics on T91 ferritic/martensitic steel exposed at 450 and 550 °C to flowing Pb-Bi eutectic with 10−7 mass% dissolved oxygen10.1016/j.jnucmat.2017.07.031 ↗
8. Insights into the fatigue damage mechanism of T91 steel in liquid lead-bismuth eutectic at 150–550 °C10.1016/j.corsci.2024.112007 ↗
9. Synergy effect of LBE and hydrogenated helium on resistance to LME of T91 steel grade10.1016/S0022-3115(03)00081-3 ↗
10. Local mechanical properties of corrosion layers formed on T91 and SS316L steels after exposure to static liquid LBE at 500 °C for 1000h obtained by nano-indentation10.1016/j.net.2024.03.005 ↗
11. Strain-rate dependent fatigue behavior of T91 steel at 550 °C of liquid lead-bismuth eutectic10.1016/j.corsci.2024.112433 ↗
12. Microstructural characteristics of the internal oxidation zone of ferritic/martensitic steel exposed to LBE at 550 °C for 1000h10.1016/j.jmrt.2024.10.062 ↗
13. Microstructure and corrosion property evolution of a surface-nanostructured 15-15Ti austenitic steel during immersion in liquid LBE at 550 °C
14. E. A, Creep failure of a solution-annealed 15-15Ti steel exposed to stagnant lead-bismuth eutectic at 550 and 600 °C10.1016/j.msea.2020.140230 ↗
15. Creep of 316L austenitic steel at 450–550 °C in static lead-bismuth eutectic covered by argon-hydrogen gas10.1016/j.jnucmat.2021.153344 ↗
16. Characterization and corrosion behavior of Al-added high Mn ODS austenitic steels in oxygen-saturated lead–bismuth eutectic10.1016/j.corsci.2022.110818 ↗
17. Corrosion behaviors of ODS-FeCrAl in oxygen-saturated lead-bismuth eutectic at 550 °C: effects of grain boundaries and minor elements10.1016/j.jnucmat.2023.154710 ↗
18. Oxidation and dissolution behavior of FeCrNiAl based high entropy alloy and alumina-forming austenitic steel exposed to lead-bismuth eutectic (LBE)10.1016/j.corsci.2023.111693 ↗
19. Intergranular precipitation-enhanced wetting and phase transformation in an Al0.4CoCrFeNi high-entropy alloy exposed to lead-bismuth eutectic10.1016/j.corsci.2021.110038 ↗
20. Compatibility and microstructure evolution of Al-Cr-Fe-Ni high entropy model alloys exposed to oxygen-containing molten lead10.1016/j.corsci.2021.109593 ↗
21. Influence of alloying elements (Cu, Ti, Nb) on the microstructure and corrosion behaviour of AlCrFeNi-based high entropy alloys exposed to oxygen-containing molten Pb10.1016/j.corsci.2021.109659 ↗
22. J. Zhu, H. Fu, H. Zhang, A. Wang, H. Li, Z.J.Jo.A. HuCompounds, Microstructure and compressive properties of multiprincipal component AlCoCrFeNiCx alloys, 509 (2011) 3476-3480.10.1016/j.jallcom.2010.10.047 ↗
23. A successful synthesis of the CoCrFeNiAl0.3 single-crystal, high-entropy alloy by Bridgman solidification10.1007/s11837-013-0733-x ↗
24. Degradation of tensile mechanical properties of two AlxCoCrFeNi (x=0.3 and 0.4) high-entropy alloys exposed to liquid lead-bismuth eutectic at 350 and 500°C10.1016/j.jnucmat.2021.153364 ↗
25. Corrosion behavior of FeCr13Alx alloys in static lead-bismuth eutectic (LBE) at 500 °C under saturated/poor oxygen concentrations
26. A study of deformation and strain induced in bulk by the oxide layers formation on a Fe-Cr-Al alloy in high-temperature liquid Pb-Bi eutectic10.1016/j.actamat.2018.03.041 ↗
27. High entropy alloys: a focused review of mechanical properties and deformation mechanisms10.1016/j.actamat.2019.12.015 ↗
28. Orientation relationship of the austenite-to-ferrite transformation in austenitic stainless steels due to dissolution corrosion in contact with liquid Pb-Bi eutectic10.1016/j.scriptamat.2019.03.035 ↗
29. Corrosion behaviour of Al-added high Mn austenitic steels in molten lead bismuth eutectic with saturated and low oxygen concentrations at 45010.1016/j.corsci.2020.108864 ↗
30. Advances in the corrosion behavior of high-entropy alloys in lead-bismuth eutectic system10.1002/adem.202402774 ↗
31. Liquid metal embrittlement of a dual-phase Al0.7CoCrFeNi high-entropy alloy exposed to oxygen-saturated lead-bismuth eutectic10.1016/j.scriptamat.2020.113652 ↗
32. Barrier effect of intergranular precipitation in alumina-forming austenitic steel against dissolution corrosion exposed to lead-bismuth eutectic10.1016/j.corsci.2024.112643 ↗
33. X. Gong, L. Sun, F. Zhang, Y. Yin, X. Huang, H. Gong, Y.J.C.S. LiuEffect of alloying elements on liquid metal embrittlement of pure BCC Fe in contact with liquid lead-bismuth eutectic: Experiments and first principles calculation, 208 (2022) 110522.10.1016/j.corsci.2022.110522 ↗
34. Microstructure evolution and mechanical properties of AlxCoCrFeNi high-entropy alloys by laser melting deposition10.1016/j.vacuum.2020.109875 ↗
35. Prediction of high-entropy stabilized solid-solution in multi-component alloys10.1016/j.matchemphys.2011.11.021 ↗
36. Microstructure, thermophysical and electrical properties in AlxCoCrFeNi (0≤ x≤ 2) high-entropy alloys10.1016/j.mseb.2009.05.024 ↗
37. Solid-solution phase formation rules for multi-component alloys10.1002/adem.200700240 ↗
38. Identification of the Fe3O4–Fe2O3 reaction in liquid lead–bismuth eutectic10.1016/j.pnucene.2023.104884 ↗
39. Studies on phase diagram of Pb–Cr–O system10.1016/j.jnucmat.2008.02.010 ↗
40. Standard molar Gibbs free energy of formation of Pb5CrO8 (s), Pb2CrO5 (s), and PbCrO4 (s)10.1016/j.jct.2009.06.026 ↗
41. Materials development and potential applications of transparent ceramics: a review10.1016/j.mser.2019.100518 ↗
42. Austenite growth and stability in medium Mn, medium Al Fe-C-Mn-Al steels10.1016/j.commatsci.2016.08.041 ↗
43. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Sc, Ti, V, Cu and Zn10.1016/j.apsusc.2010.07.086 ↗
44. Preparation of Cr-N coatings on 316H stainless steel via pack chromizing and gas nitriding, and their resistance to liquid metal corrosion in early stages10.1016/j.surfcoat.2024.130665 ↗
45. Influence of preoxidation on the corrosion of steels in liquid lead-bismuth eutectic, November 200410.5006/1.3299217 ↗
46. Oxide scales formed on Fe–Cr–Al-based model alloys exposed to oxygen containing molten lead10.1016/j.jnucmat.2013.02.044 ↗
47. Stability domain of alumina thermally grown on Fe–Cr–Al-based model alloys and modified surface layers exposed to oxygen-containing molten Pb10.1016/j.jnucmat.2015.12.009 ↗
48. Corrosion resistance of iron-chromium-aluminium steel in eutectic molten salts under thermal cycling conditions10.1016/j.corsci.2020.108798 ↗
49. A comparative study on the corrosion performance of four FeCrAl alloys with different Cr contents in contact with oxygen-saturated LBE10.1016/j.jmrt.2023.02.033 ↗
50. Corrosion behavior of AFA steel in lead-bismuth eutectic alloy with saturated oxygen at 500 °C
51. A study of deformation and strain induced in bulk by the oxide layers formation on a Fe-Cr-Al alloy in high-temperature liquid Pb-Bi eutectic10.1016/j.actamat.2018.03.041 ↗
52. Enhanced crystallization of α-(Cr, Al)2O3 coatings with increasing oxygen pressure10.1016/j.surfcoat.2022.128705 ↗
53. A density functional study of vacancy formation in grain boundaries of undoped α-alumina10.1016/j.actamat.2014.01.059 ↗
54. Diffusion and growth mechanism of Al2O3 scales on ferritic Fe-Cr-Al alloys10.1016/S0921-5093(97)00711-9 ↗
55. Precipitation of α-Cr in B2-ordered NiAl10.1016/S0966-9795(98)00015-6 ↗
56. Phase equilibria of an Al0.5CrFeCoNiCu high entropy alloy10.1016/j.msea.2014.07.059 ↗
57. D.R. LideCRC handbook of chemistry and physics, CRC press, 2004.
58. Corrosion behaviors of FeCrAl alloys exposed to oxygen-saturated static lead bismuth eutectic at 550 °C10.1016/j.corsci.2022.110767 ↗
59. Dissolution and oxidation behaviour of various austenitic steels and Ni rich alloys in lead-bismuth eutectic at 52010.1016/j.jnucmat.2015.11.005 ↗
60. The role of oxide films in preventing liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic10.1016/j.jnucmat.2018.07.018 ↗
61. Design of alumina forming FeCrAl steels for lead or lead–bismuth cooled fast reactors10.1016/j.jnucmat.2012.04.006 ↗
62. Optimizing the coupled effects of Hall-Petch and precipitation strengthening in a Al0. 3CoCrFeNi high entropy alloy10.1016/j.matdes.2017.02.072 ↗
63. Twin boundary-accelerated ferritization of austenitic stainless steels in liquid lead–bismuth eutectic10.1016/j.scriptamat.2016.02.029 ↗
64. The transition from transient oxide to protective Al2O3 scale on Fe–Cr–Al alloys during heating to 100010.1007/s11085-017-9778-5 ↗
65. On high temperature oxidation of chromium: I. Oxidation of annealed, thermally etched chromium at 800–1100 ℃10.1149/1.2129478 ↗
66. Oxidation of arc-evaporated Al1-xCrxN coatings10.1116/1.2738492 ↗