Synergistic strengthening of AA6061 aluminum alloy by severe plastic deformation combined with low-temperature under-aging
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (68)
Show source-provided references
1. Aluminum alloys for aircraft structures
2. A review on recent developments of aluminum-based hybrid composites for automotive applications10.1007/s42247-021-00186-6 ↗
3. Texture control by thermomechanical processing of aa6xxx Al–Mg–Si sheet alloys for automotive applications—a review10.1016/S0921-5093(01)01968-2 ↗
4. Advances in lightweight composite structures and manufacturing technologies: A comprehensive review10.1016/j.heliyon.2024.e39661 ↗
5. The nanoscale mechanisms of strengthening and ductility enhancement in an Al-Mg-Si-Mn alloy on processing by high-pressure torsion10.1016/j.matchar.2023.113145 ↗
6. Mechanical properties and microstructures of highly Fe-containing Al–Mg–Si alloys processed by severe plastic deformation under high pressure10.2320/matertrans.MT-LA2022054 ↗
7. Deformation-mediated cyclic evolution of precipitates in Al-Mg-Si-Cu alloy by multi-pass ECAP and thermal treatments10.1016/j.jmst.2024.05.075 ↗
8. Developing a high-strength Al-Mg-Si alloy with improved electrical conductivity by a novel ECAP route10.1007/s12540-021-01152-x ↗
9. Enhanced mechanical properties of ARB-processed aluminum alloy 6061 sheets by subsequent asymmetric cryorolling and ageing10.1016/j.msea.2016.08.003 ↗
10. Simultaneous improvement of strength, ductility and corrosion resistance of Al2024 alloy processed by cryoforging followed by ageing10.1016/j.msea.2015.11.032 ↗
11. Microstructure and mechanical properties of ultra-fine grains (ufgs) aluminum strips produced by arb process10.1016/j.jallcom.2008.06.161 ↗
12. Insight to the evolution of nano precipitates by cryo rolling plus warm rolling and their effect on mechanical properties in Al 6061 alloy10.1016/j.msea.2021.141072 ↗
13. Playing with defects in metals10.1038/nmat4929 ↗
14. High stress twinning in a compositionally complex steel of very high stacking fault energy10.1038/s41467-022-31315-2 ↗
15. Strength-ductility synergy induced by high-density stacking faults in aluminum alloy composites with micro/nano hybrid reinforcements10.1016/j.compositesa.2023.107700 ↗
16. Dynamic mechanical responses of the Al0.1CoCrFeNi high entropy alloy at cryogenic temperature10.1016/j.msea.2020.140125 ↗
17. Systematic study of stacking fault energies of random al-based alloys10.1016/S1359-6454(97)00432-1 ↗
18. Formation mechanism of wide stacking faults in nanocrystalline Al10.1063/1.1734689 ↗
19. Nanostructures and deformation mechanisms in a cryogenically ball-milled Al-Mg alloy10.1080/1478643031000152799 ↗
20. Deformation twinning in nanocrystalline aluminum10.1126/science.1083727 ↗
21. Macrodeformation twins in single-crystal aluminum10.1103/PhysRevLett.116.075501 ↗
22. Structural characterization by high-resolution electron microscopy of an Al-Mg alloy processed by high-pressure torsion10.1016/j.msea.2008.02.053 ↗
23. On the widths of stacking faults formed by dissociation of different types of full dislocations in a nanostructured Al alloy10.1016/j.msea.2019.138532 ↗
24. High strength and high ductility behavior of 6061-T6 alloy after laser shock processing10.1016/j.optlaseng.2015.08.004 ↗
25. Enhancing the mechanical properties of 6061 aluminum alloy through the synergistic effects of twins, stacking faults, nanograins and lattice distortions10.1016/j.jmrt.2025.02.242 ↗
26. Pre-precipitate clusters and precipitation processes in Al–Mg–Si alloys10.1016/S1359-6454(99)00033-6 ↗
27. Precipitation sequence of an aged Al-Mg-Si alloy10.2298/JMMB1002171F ↗
28. Precipitation hardening10.1007/BF02670416 ↗
29. Argon · 2007
30. Strengthening mechanisms of Fe nanoparticles for single crystal Cu-Fe alloy10.1016/j.msea.2015.03.081 ↗
31. Brittle intermetallic compound makes ultrastrong low-density steel with large ductility10.1038/nature14144 ↗
32. A precipitation-hardened high-entropy alloy with outstanding tensile properties10.1016/j.actamat.2015.08.076 ↗
33. Ultrastrong steel via minimal lattice misfit and high-density nanoprecipitation10.1038/nature22032 ↗
34. Cu-rich nanoprecipitates modified using Al to simultaneously enhance the strength and ductility of ferritic stainless steel10.1016/j.jmst.2021.12.061 ↗
35. Enhanced strength and ductility in a high-entropy alloy via ordered oxygen complexes10.1038/s41586-018-0685-y ↗
36. Intergranular corrosion of AA6082 Al-Mg-Si alloy extrusion: The influence of trace Cu and grain boundary misorientation10.1016/j.jallcom.2020.157228 ↗
37. Effect of the thickness reduction on intergranular corrosion in an under–aged Al-Mg-Si-Cu alloy during cold–rolling10.1016/j.corsci.2018.07.018 ↗
38. Deformation behavior of nanostructured aluminum alloy processed by severe plastic deformation10.1016/S0921-5093(01)01052-8 ↗
39. Production of ultrafine grain sizes in aluminium sheets by severe plastic deformation using the technique of groove pressing10.1016/j.scriptamat.2005.03.001 ↗
40. Nano grained az31 alloy achieved by equal channel angular rolling process10.1016/j.msea.2011.05.024 ↗
41. Deformation assisted nucleation of continuous nanoprecipitates in Mg-Al alloys10.1016/j.mtla.2019.100583 ↗
42. Enhancing creep formability and comprehensive property in Al–Mg–Si alloy by combinatorial pre-ageing and large pre-deformation10.1016/j.msea.2021.141967 ↗
43. Enhancing mechanical properties of cast ingot Al 6061 Alloy using ECAP process
44. Effects of warm rolling and ageing after cryogenic rolling on mechanical properties and microstructure of Al 6061 alloy10.1016/j.matdes.2012.02.010 ↗
45. Effect of asymmetric rolling on the microstructure and mechanical properties of wrought 6061 aluminum
46. The effects of rolling parameters on the mechanical behavior of 6061 aluminum alloy10.1016/j.msea.2013.04.023 ↗
47. Effect of cryorolling and warm rolling on precipitation evolution in Al 6061 alloy10.1016/j.msea.2014.03.031 ↗
48. Microstructures and mechanical properties of 6061 aluminum alloy processed by accumulative roll-bonding10.1016/S0921-5093(01)01416-2 ↗
49. Grain size effects in aluminum processed by severe plastic deformation10.1016/j.msea.2017.10.077 ↗
50. The mechanism of plastic deformation of crystals. Part I. —theoretical
51. Microstructural evolution, strengthening and thermal stability of an ultrafine-grained Al–Cu–Mg alloy10.1016/j.actamat.2016.02.050 ↗
52. The dissociation of dislocations in the face-centered cubic structure10.1016/0001-6160(63)90023-3 ↗
53. The formation of immobile dislocations during slip10.1080/14786440608520220 ↗
54. Segregation-dislocation self-organized structures ductilize a work-hardened medium entropy alloy10.1038/s41467-025-56710-3 ↗
55. Enhanced strengthening effect via nano-twinning in cryo-rolled FeCoCrNiMo0.2 high-entropy alloys10.1016/j.msea.2023.144676 ↗
56. The deformation and ageing of mild steel: Iii discussion of results10.1088/0370-1301/64/9/303 ↗
57. Effect of rolling on the microstructure and mechanical properties of 6061-t6 ds-fsw plate10.1016/j.msea.2019.138692 ↗
58. Symposium on internal stress in metals and alloys
59. Work hardening of dispersion-hardened crystals10.1080/14786436608224282 ↗
60. Nanoscale precipitates as sustainable dislocation sources for enhanced ductility and high strength10.1073/pnas.1914615117 ↗
61. The interaction mechanisms between dislocations and nano-precipitates in CuFe alloys: A molecular dynamic simulation10.1016/j.ijplas.2022.103317 ↗
62. Nanoprecipitates induced dislocation pinning and multiplication strategy for designing high strength, plasticity and conductivity Cu alloys10.1016/j.scriptamat.2021.113741 ↗
63. Microstructure evolution and mechanical properties of new die-cast Al-Si-Mg-Mn alloys10.1016/j.matdes.2019.108394 ↗
64. Mechanical properties and corrosion behavior of artificially aged Al-Mg-Si alloy10.1016/j.jmrt.2019.11.040 ↗
65. Effect of cryorolling and annealing on recovery, recrystallisation, grain growth and their influence on mechanical and corrosion behaviour of 6082 Al alloy10.1016/j.matchemphys.2015.09.014 ↗
66. Effects of cryorolling, room temperature rolling and aging treatment on mechanical and corrosion properties of 7050 aluminum alloy10.1016/j.msea.2022.143764 ↗
67. Corrosion behavior of a dynamically deformed Al-Mg alloy10.1016/j.electacta.2020.136695 ↗
68. Effects of pre-strain on the surface residual stress and corrosion behavior of an Al-Zn-Mg-Cu alloy plate10.1016/j.matchar.2020.110129 ↗