Effect of interaction between hydrogen and intermetallic compound particles on stress corrosion cracking behavior of 2050 aluminum alloy
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Aluminum Alloy Microstructure Properties · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Evolution of micropores and second phases during hot deformation of 2050 Al-Li alloy10.1016/j.jallcom.2023.173166 ↗
2. Study on hardenability of 2050 Al-Cu-Li alloy ultra-thick plate10.1016/j.jmrt.2024.06.111 ↗
3. Spall strength and equation of states for 2050-T84 Al-Li alloy under shock compression up to 120 GPa10.1016/j.jpcs.2022.111138 ↗
4. Influence of tool pin profiles on waviness and natural frequency during friction stir welding of Al-Li alloys plates
5. Effect of inhomogeneous microstructures on stress corrosion cracking sensitivity of 2050-T84 Al-Li alloy thick plate10.1016/j.corsci.2024.112213 ↗
6. Stress corrosion cracking induced by the combination of external and internal hydrogen in Al-Zn-Mg-Cu alloy10.1016/j.scriptamat.2023.115804 ↗
7. Understanding the environmentally assisted cracking (EAC) initiation and propagation of new generation 7xxx alloys using slow strain rate testing10.1016/j.corsci.2022.110161 ↗
8. Role of retrogression and reaging in suppressing hydrogen-induced transgranular cracking in 7xxx Al alloys10.1016/j.scriptamat.2024.116383 ↗
9. Understanding the role of matrix precipitates on the environmentally assisted cracking behavior of AA 7050 alloy10.1016/j.corsci.2022.110281 ↗
10. Improvement of hydrogen embrittlement and stress corrosion cracking by annealing for Al-4.4Mg-0.6Mn alloy10.1016/S1003-6326(11)61053-4 ↗
11. Effect of varying conditions of exposure to an aggressive medium on the corrosion behavior of the 2050 Al–Cu–Li alloy10.1016/j.corsci.2014.04.042 ↗
12. Effect of creep stress level on hydrogen embrittlement mechanism of Al-Zn-Mg-Cu alloy10.1016/j.msea.2024.147542 ↗
13. Effect of pre-strain on hydrogen embrittlement of 7075 aluminum alloy and molecular dynamics simulation10.1016/j.ijhydene.2024.08.496 ↗
14. Dislocation-aided electrochemical behavior of precipitates in stress corrosion cracking of Al-Zn-Mg-Cu alloys10.1016/j.matchar.2022.112019 ↗
15. Advancing the hydrogen tolerance of ultrastrong aluminum alloys via nanoprecipitate modification10.1016/j.corsci.2024.112471 ↗
16. Simulating hydrogen-controlled crack growth kinetics in Al-alloys using a coupled chemo-mechanical phase-field damage model10.1016/j.actamat.2024.120597 ↗
17. SCC susceptibility of RRA treated high-zinc 7068 aluminum alloy10.1016/j.corsci.2023.111257 ↗
18. Nanoscale perspective on the stress-corrosion cracking behavior of a peak-aged 7XXX-Al alloy10.1016/j.corsci.2024.111904 ↗
19. Analyzing through-thickness corrosion homogeneity of stabilized AA5083 alloy after artificial sensitization10.1016/j.corcom.2024.03.002 ↗
20. The mechanism of hydrogen-facilitated anodic-dissolution-type stress corrosion cracking: theories and experiments10.1080/01418610108216638 ↗
21. Hydrogen mapping in an aluminum alloy using an alternating current scanning electrochemical microscope (AC-SECM)10.1016/j.elecom.2017.05.007 ↗
22. Combined Kelvin probe force microscopy and secondary ion mass spectrometry for hydrogen detection in corroded 2024 aluminium alloy10.1016/j.electacta.2013.02.063 ↗
23. About the role of the hydrogen during stress corrosion cracking of a low-copper Al-Zn-Mg alloy10.1016/j.jallcom.2021.163391 ↗
24. Hydrogen-accelerated spontaneous microcracking in high-strength aluminium alloys10.1038/s41598-020-58834-6 ↗
25. Damage micromechanisms of stress corrosion cracking in Al-Mg alloy with high magnesium content10.1016/j.corsci.2021.109343 ↗
26. Suppressed hydrogen embrittlement of high-strength Al alloys by Mn-rich intermetallic compound particles10.1016/j.actamat.2022.118110 ↗
27. Corrosion properties and mechanisms of friction stir lap welded TiB2/2024 aluminum matrix composite joint10.1016/j.electacta.2024.145306 ↗
28. Insights on the Al-Cu-Fe-Mn intermetallic particles induced pitting corrosion of Al-Cu-Li alloy10.1016/j.corsci.2020.109040 ↗
29. Influence of thermomechanical treatment on the corrosion behaviour of 2A97 Al-Cu-Li alloy10.1016/j.corcom.2023.10.003 ↗
30. A mechanistic study on localized corrosion of sandwich multi-layered aluminium sheet in 3.5 wt% NaCl solution10.1016/j.electacta.2023.143686 ↗
31. Localized corrosion in AA2099-T83 aluminum-lithium alloy: The role of intermetallic particles10.1016/j.matchemphys.2015.05.037 ↗
32. Effect of surface abrasion on pitting corrosion of Al-Li alloy10.1016/j.corsci.2018.04.010 ↗
33. Localized corrosion evolution associated with intermetallic particles in Al-Cu-Li alloys10.1016/j.matchar.2023.113144 ↗
34. Corrosion morphology evolution in 2A97-T6 Al-Cu-Li alloy: the influence of grain-stored energy10.1016/j.matchar.2022.112169 ↗
35. Effect of LDHs on corrosion behavior of 6061 Al alloy in NaCl solution with different dissolved oxygen contents
36. In situ microscopy and electrochemical characteristics of initiation of intergranular corrosion of aging-treated Al–1Mg–0.65Si–0.8Cu alloy in 0.1 M NaCl10.1016/j.corsci.2025.112985 ↗
37. Distribution of intermetallics in an AA 2099-T8 aluminium alloy extrusion10.1016/j.matchemphys.2010.12.014 ↗
38. Dissolution behavior of intermetallic particles in AA2297-T87 during anodizing in adipic-sulfuric acid10.1149/2.0061816jes ↗
39. New insights on the initial local corrosion of composite Al7Cu2Fe/Al20Cu2Mn3 intermetallic particles in 2024-T351 aluminum alloy10.1016/j.corsci.2022.110657 ↗
40. Coupling effect on corrosion behavior of multi-phase AlCuMnFe IMPs in 2050-T84 Al-Li alloy10.1016/j.corsci.2023.111462 ↗
41. Corrosion of AA2024-T3 Part I: localised corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
42. Nanoindentation study of intermetallic particles in 2024 aluminium alloy10.3390/coatings10090846 ↗
43. Revisiting Ag addition in 7xxx aluminum alloys: Insights into its impact on the microstructure and properties of an Al-Zn-Mg-Cu-Zr alloy with a Zn/Mg ratio of 410.1016/j.matchar.2024.114186 ↗
44. Mechanisms of hydrogen embrittlement in high-strength aluminum alloys containing coherent or incoherent dispersoids10.1016/j.corsci.2021.109895 ↗
45. Effects of sensitization on environmentally assisted cracking of AA5083-H128 Al-Mg alloy10.1016/j.jmrt.2023.05.255 ↗
46. A predictive model unifying hydrogen enhanced plasticity and decohesion10.1016/j.scriptamat.2022.114707 ↗
47. Influence of indentation size on the corrosion behaviour of a phosphate conversion coated AZ80 magnesium alloy10.1016/j.jmrt.2021.07.091 ↗
48. Effect of scratch on corrosion resistance of calcium phosphate conversion coated AZ80 magnesium alloy10.1016/S1003-6326(21)65784-9 ↗
49. Stress corrosion behavior and microstructure analysis of Al-Zn-Mg-Cu alloys fabricated by CMT wire arc additive manufacturing with different post-treatments10.1016/j.jallcom.2024.177759 ↗
50. The corrosion behaviour of MAO coated AZ80 magnesium alloy with surface indentation of different sizes10.1016/j.engfailanal.2022.106185 ↗
51. Enhanced heat and corrosion resistance of organic silicone coatings by dual shielding effects of Zn powder10.1016/j.electacta.2024.145329 ↗
52. Nitrate-reducing-bacteria assisted hydrogen embrittlement of X80 steel in a near-neutral pH solution10.1016/j.corsci.2022.110317 ↗
53. Investigation of Kelvin probe force microscopy efficiency for the detection of hydrogen ingress by cathodic charging in an aluminium alloy10.1016/j.scriptamat.2012.11.026 ↗
54. Stress corrosion cracking behaviour of 7xxx aluminum alloys: a literature review10.1016/S1003-6326(16)64220-6 ↗
55. Stress corrosion cracking of a high-strength friction-stir-welded joint of an Al-Zn-Mg-Zr alloy containing 0.25 wt% Sc10.1016/j.corsci.2015.06.031 ↗
56. Localized electrochemical characterization of high strength aluminium alloy at the crack tip in 3.5%NaCl solution10.3724/SP.J.1037.2011.00692 ↗