The influence of Mg addition on phase composition and mechanical properties of twin-roll cast Al-steel clad material
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Metallurgy and Material Forming · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Temperature evolution, IMC formation, and resulting bonding efficacy in bimetallic tubular components fabricated by a novel friction stir backward extrusion cladding method10.1016/j.cirpj.2024.04.007 ↗
2. Modeling and analysis of thin-walled Al/steel explosion welded transition joints for shipbuilding applications10.1016/j.marstruc.2020.102843 ↗
3. Formation of the interlock morphology and its role in refill friction stir spot welding of aluminum alloy to steel10.3390/met14111209 ↗
4. Free intermetallic cladding interface between aluminum and steel through friction stir processing10.3390/cryst12101413 ↗
5. Direct spot joining of thin gauge aluminum alloy to stainless steel and joint performance in a corrosion environment10.1016/j.tws.2024.111919 ↗
6. Experimental and numerical investigations of formability of two-ply clad sheet of stainless steel and aluminium alloy10.1007/s12647-024-00765-y ↗
7. Effect of annealing on properties of Al/steel composite plates prepared by surface oxidation treatment before cold roll bonding10.1007/s42243-022-00832-1 ↗
8. Effect of surface treatment on bonding strength of hot rolled steel aluminum clad plate10.1088/1757-899X/1270/1/012016 ↗
9. Enhancing the ballistic resistance of steel/aluminum bilayer armor plates through explosive welding10.1016/j.matdes.2023.112346 ↗
10. Impact of steel substrate preheating on microstructure and properties of twin-roll cast aluminium-steel clad strips10.1016/j.proeng.2017.10.924 ↗
11. Aluminum/steel dissimilar material with high interfacial strength manufactured by additive friction stir deposition10.1016/j.jmapro.2024.11.080 ↗
12. Microstructure, growth kinetics and mechanical properties of interface layer for roll bonded aluminum-steel clad sheet annealed under argon gas protection10.1016/j.vacuum.2018.02.018 ↗
13. Investigation on bonding strength of steel/aluminum clad sheet processed by horizontal twin-roll casting, annealing and cold rolling10.1016/j.matdes.2016.09.061 ↗
14. In situ SEM, TEM, EBSD characterization of nucleation and early growth of pure Fe/pure Al intermetallic compounds10.3390/ma16176022 ↗
15. Formation of Fe5Si3 precipitate in the Fe2Al5 intermetallic layer of the Al/steel dissimilar arc welding joint: a transmission electron microscopy (TEM) study10.1016/j.matchar.2021.111236 ↗
16. Effect of volume ratio on microstructure and properties of layered steel-aluminum low-density composites prepared by hot pressing
17. Forming mechanics of a twin-roll cast AA1100/409L clad sheet after annealing and cold rolling10.2140/jomms.2024.19.251 ↗
18. Fabrication of AlZn4SiPb/Steel clad sheets by roll bonding: their microstructure and mechanical properties10.3390/cryst13020292 ↗
19. Deformation behavior of lightweight clad sheet: Experiment and modeling10.1016/j.msea.2022.143666 ↗
20. Effect of heat treatment on tensile deformation characteristics and properties of Al3003/STS439 clad composite10.1016/j.msea.2013.12.019 ↗
21. Interface-correlated deformation behavior of a stainless steel-Al-Mg 3-ply composite10.1016/j.matchar.2012.10.012 ↗
22. Tensile deformation behaviour of twin-roll cast Al-steel clad sheet studied by in-situ methods10.1016/j.msea.2024.147668 ↗
23. Strengthening mechanisms in an Al-Mg alloy10.1016/j.msea.2009.11.056 ↗
24. Development and applications of aluminum alloys for aerospace industry10.1016/j.jmrt.2023.09.274 ↗
25. Recent progress of Al-Mg alloys: forming and preparation process, microstructure manipulation and application10.1016/j.jmrt.2024.07.051 ↗
26. Synergistic effect of Mg addition on the enhancement of the mechanical properties and evaluation of corrosion behaviors in 3.5 wt% NaCl of aluminum alloys10.1016/j.heliyon.2024.e25437 ↗
27. Effects of high Mg content and processing parameters on Portevin-Le Chatelier and negative strain rate sensitivity effects in Al-Mg alloys10.1016/j.msea.2020.139151 ↗
28. Fatigue and dynamic aging behavior of a high strength Al-5024 alloy fabricated by laser powder bed fusion additive manufacturing10.1016/j.actamat.2021.117312 ↗
29. Revealing the mechanisms of exfoliation corrosion and stress corrosion cracking for an Al-Zn-Mg-Cu alloy after continuous retrogression and re-ageing treatment10.1016/j.corsci.2024.112474 ↗
30. Role of subgrain stripe on the exfoliation corrosion of Al-4.6Mg-3.1Zn (wt%) alloy10.1016/j.corsci.2020.108622 ↗
31. The influence of casting methods on microstructure of Al-Mg-Sc-Zr alloy
32. Thermal stability of dislocation structure and its effect on creep property in austenitic 316L stainless steel manufactured by directed energy deposition10.1016/j.msea.2023.144981 ↗
33. Manufacturing and characterization of twin-roll cast aluminum-steel clad strips
34. 3D-structure of intermetallic interface layer in Al-steel clad material10.1016/j.vacuum.2023.112043 ↗
35. The influence of surface on direction of diffusion in Al-Fe clad material10.1016/j.matchar.2022.112005 ↗
36. Intermetallic phases identification and diffusion simulation in twin-roll cast Al-Fe clad sheet10.3390/ma14247771 ↗
37. Morphology and crystallography of E-(Al18Cr2Mg3) nano dispersoids in 7475 Al alloy10.1016/j.matchar.2024.114224 ↗
38. Crystal structures of small Al-rich Fe alloy particles formed by a gas-evaporation technique10.1080/13642819208221297 ↗
39. Diffusion in solids
40. Kinetic interactions between solid iron and molten aluminium10.1016/S0921-5093(03)00469-6 ↗
41. Enhanced atomic diffusion of Fe-Al diffusion couple during spark plasma sintering10.1016/j.scriptamat.2015.08.012 ↗
42. Growth behavior of Fe2Al5 during reactive diffusion between Fe and Al at solid-state temperatures10.1016/j.msea.2007.01.099 ↗
43. Formatian of the alloy layer in the Fe-Al diffusion couple10.2320/jinstmet1952.30.4_382 ↗
44. The influence of grain structure on intermetallic compound layer growth rates in Fe-Al dissimilar welds10.1007/s11661-017-4352-y ↗
45. Influence of interface structure and stress distribution on fracture and mechanical performance of STS439/Al1050/STS304 clad composite10.1016/j.msea.2019.02.004 ↗
46. Residual stresses in welded structures10.1016/j.ijpvp.2007.10.004 ↗
47. Investigation of cold rolling influence on near surface residual stress distribution in explosive welded multilayer10.1007/s11223-012-9424-z ↗
48. M. Šlapáková, In-situ tensile test in SEM of Al-steel clad material, 〈http://pokova.matfyz.cz/paper/in-situ〉, [Online](2024).
49. On the influence of Mn and Mg additions on tensile properties, microstructure and quality index of the A356 aluminum foundry alloy10.1016/j.prostr.2016.06.280 ↗