journal article·2025-11Open access

Fe–Mn–Co–Al–C duplex high-entropy alloys with high hardness, high strength and good ductility processed via high-pressure torsion

Dmitri V. Louzguine-Luzgin, Kaveh Edalati

Abstract

High-entropy alloys exhibit good mechanical properties, but there is still a demand to develop high-entropy alloys with ultrahigh strength and good ductility. In this study, Fe–Mn–Co–Al–C high-entropy alloys with a duplex FCC + BCC structure were processed by high-pressure torsion (HPT) to induce microstructural defects. They exhibited hardness levels up to 570 HV, exceptional yield and ultimate tensile strength values exceeding 2 GPa with elongation to failure of up to 30% after HPT processing. The best combination of strength and ductility was achieved in the presence of elongated grains, while the generation of equiaxed nanograins led to a reduction of ductility. Short-term aging induced additional hardening to 700–800 HV due to polygonization and partial phase ordering, but no evidence for carbide precipitation was found. Detailed analysis through the Hall-Petch relationship suggests that grain boundary strengthening is the dominant hardening mechanism after HPT processing, despite the presence of solute atoms and formation of dislocations. The combination of ultrahigh strength, good ductility realized by microstructural control through severe plastic deformation by HPT highlights the potential of these alloys for advanced structural applications. • Fe–Mn–Co–Al–C high-entropy alloys were processed by high-pressure torsion (HPT) • HPT yields strong alloys with strength over 2 GPa with up to 30% ductility • Hardness reaches 700–800 HV after severe plastic deformation followed by aging • Differential scanning spectroscopy reveals high stored energy from deformation • Grain refinement and Hall-Petch mechanism appear to be dominant for strengthening
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Entropy Alloys Studies · High-Temperature Coating Behaviors · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (70)

Show source-provided references
1. Microstructural development in equiatomic multicomponent alloys10.1016/j.msea.2003.10.257 ↗
2. Nanostructured high-entropy alloys with multiple principal elements: novel alloy design concepts and outcomes10.1002/adem.200300567 ↗
3. A critical review of high entropy alloys and related concepts10.1016/j.actamat.2016.08.081 ↗
4. High-temperature materials for structural applications: new perspectives on high-entropy alloys, bulk metallic glasses, and nanomaterials10.1557/mrs.2019.257 ↗
5. High-entropy alloys: a critical assessment of their founding principles and future prospects10.1080/09506608.2016.1180020 ↗
6. Mechanical behavior of high-entropy alloys10.1016/j.pmatsci.2021.100777 ↗
7. High-entropy alloys: a critical assessment of their founding principles and future prospects10.1080/09506608.2016.1180020 ↗
8. Mechanical behavior of high-entropy alloys10.1016/j.pmatsci.2021.100777 ↗
9. High temperature deformation behavior and dynamic recrystallization in CoCrFeNiMn high entropy alloy10.1016/j.msea.2015.03.097 ↗
10. Plastic deformation of solid-solution strengthened Hf-Nb-Ta-Ti-Zr body-centered cubic medium/high-entropy alloys10.1016/j.scriptamat.2021.113927 ↗
11. High entropy alloys as a bold step forward in alloy development10.1038/s41467-019-09700-1 ↗
12. Morphology transition from dendrites to equiaxed grains for AlCoCrFeNi high-entropy alloys by copper mold casting and bridgman solidification10.1007/s11661-011-0981-8 ↗
13. Effects of Al addition on structural evolution and tensile properties of the FeCoNiCrMn high-entropy alloy system10.1016/j.actamat.2013.09.037 ↗
14. Solid solution alloys of AlCoCrFeNiTix with excellent room-temperature mechanical properties10.1063/1.2734517 ↗
15. Short-range ordering and its effects on mechanical properties of high-entropy alloys10.1016/j.jmst.2020.06.018 ↗
16. Enhancing mechanical performance and wear resistance of Co-free B2/A2 CrFeNiAl alloy via Cr and Ti adjustment10.1557/s43577-023-00624-2 ↗
17. Solid-solution hardening of a high-Entropy AlTiVCrNbMo alloy10.1134/S0036029514040028 ↗
18. Effect of Nb, Addition on microstructure and thermal and mechanical properties of Fe-Co-Ni-Cu-Cr multiprincipal-element (high-entropy) alloys in as-cast and heat-treated state
19. Investigation of the structure and properties of the Fe-Ni-Co-Cu-V multiprincipal element alloys10.1007/s11661-018-4871-1 ↗
20. Effect of carbon content and annealing on structure and hardness of the CoCrFeNiMn-based high entropy alloys10.1016/j.jallcom.2016.06.103 ↗
21. Effect of thermomechanical processing on microstructure and mechanical properties of the carbon-containing CoCrFeNiMn high entropy alloy10.1016/j.jallcom.2016.09.208 ↗
22. Enhanced strength–ductility synergy in ultrafine-grained eutectic high-entropy alloys by inheriting microstructural lamellae10.1038/s41467-019-08460-2 ↗
23. Fundamental deformation behavior in high-entropy alloys: an overview10.1016/j.cossms.2017.08.003 ↗
24. Decomposition of the single-phase high-entropy alloy CrMnFeCoNi after prolonged, anneals at intermediate temperatures10.1016/j.actamat.2016.04.005 ↗
25. Dynamic precipitation of σ-phase and element partitioning in equiatomic CoCrFeMnNi high-entropy alloy10.1016/j.msea.2021.140739 ↗
26. Effects of annealing treatment on phase composition and microstructure of CoCrFeNiTiAlx high-entropy alloys10.1016/j.intermet.2011.10.010 ↗
27. Investigation of the phase stabilities in AlNiCoCrFe high entropy alloys10.1016/j.jallcom.2016.08.121 ↗
28. Design of a twinning-induced plasticity high entropy alloy10.1016/j.actamat.2015.04.014 ↗
29. The as-cast precipitation-strengthened N-doped Fe40Mn40Co10Cr10 high-entropy alloys10.1016/j.matlet.2022.133756 ↗
30. Chemical composition optimization for austenitic steels of the Fe-Mn-Al-C system10.1361/105994900770345430 ↗
31. High-strength Fe-20Mn-Al-C-based alloys with low density10.2355/isijinternational.50.893 ↗
32. Recrystallization kinetics of an austenitic high-manganese steel subjected to severe plastic deformation10.1134/S0036029516090184 ↗
33. High-strength Fe-20Mn-Al-C-based alloys with low density10.2355/isijinternational.50.893 ↗
34. High-entropy approach starting from a corner of the phase diagram in designing high strength Fe–Mn–Co-based alloys with good tensile ductility10.1557/s43577-021-00190-5 ↗
35. High entropy Fe–Mn–Ni–Co–Al–C alloys from an industrial steel10.1177/02670836231214399 ↗
36. The effect of some late 3d transition metals additions to a Fe–Mn–Al–C alloy on the development of high-entropy alloys10.1016/j.intermet.2024.108589 ↗
37. From high-entropy alloys to high-entropy steels10.1002/srin.201500133 ↗
38. Phase equilibria in Fe-Mn-Al-C alloys10.2355/isijinternational.30.680 ↗
39. Design for Fe-high Mn alloy with an improved combination of strength and ductility10.1038/s41598-017-03862-y ↗
40. Hardening of austenitic nitrogen high-manganese aluminum alloys under heat and thermomechanical treatment10.1007/s11041-016-9946-2 ↗
41. Effect of aging on the microstructure and deformation behavior of austenite base lightweight Fe-28Mn-9Al-0.8C steel10.1016/j.scriptamat.2010.07.036 ↗
42. Microstructure evolution and age-hardening behavior of microalloyed austenitic Fe-30Mn-9Al-0.9C light-weight steels10.1007/s11661-017-4265-9 ↗
43. Nanomaterials by severe plastic deformation: review of historical developments and recent advances10.1080/21663831.2022.2029779 ↗
44. Severe plastic deformation for producing superfunctional ultrafine-grained and heterostructured materials: an interdisciplinary review10.1016/j.jallcom.2024.174667 ↗
45. Structure and mechanical properties of ultrafine-grained metals10.1016/S0921-5093(97)00183-4 ↗
46. Extreme grain refinement by severe plastic deformation: a wealth of challenging science10.1016/j.actamat.2012.10.038 ↗
47. High-pressure torsion for synthesis of high-entropy alloys10.3390/met11081263 ↗
48. Phase transformation and microstructure evolution in ultrahard carbon-doped AlTiFeCoNi high-entropy alloy by high-pressure torsion10.1016/j.matlet.2021.130368 ↗
49. Effects of high pressure torsion on microstructures and properties of an Al0.1CoCrFeNi high-entropy alloy10.1016/j.msea.2015.12.085 ↗
50. Microstructure and mechanical properties of high-entropy alloy Co20Cr26Fe20Mn20Ni14 processed by high-pressure torsion at 77 K and 300 K10.1038/s41598-018-29446-y ↗
51. Review on superior strength and enhanced ductility of metallic nanomaterials10.1016/j.pmatsci.2018.02.002 ↗
52. Cold consolidation of ball-milled titanium powders using high-pressure torsion10.1007/s11661-010-0400-6 ↗
53. A new method for quantitative phase analysis using X-ray powder diffraction: direct derivation of weight fractions from observed integrated intensities and chemical compositions of individual phases10.1107/S1600576716010451 ↗
54. 〈https://www.crystalimpact.com/match/〉.
55. Strain-induced and thermally-reversible BCC to FCC phase transformation in a heavily deformed Fe–Mn–Co–Ni–Cu–Al–C alloy10.1016/j.msea.2025.147991 ↗
56. Brittle intermetallic compound makes ultrastrong low-density steel with large ductility10.1038/nature14144 ↗
57. Microstructure and mechanical properties evolution of the Al, C-containing CoCrFeNiMn-type high-entropy alloy during cold rolling10.3390/ma11010053 ↗
58. Recrystallization behavior of a high-manganese steel: experiments and simulations10.1016/j.actamat.2015.08.057 ↗
59. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
60. Smithells Metals Reference Book, 7th Edition, Ed: E.A. Brandes and G.B. Brook, Butterworth-Heinemann, 1992, p. 450.
61. High-pressure torsion, a new processing route for thermoelectrics of high ZTs by means of severe plastic deformation10.1016/j.actamat.2011.12.023 ↗
62. Ultrastrong nanocrystalline stainless steel and its Hall-Petch relationship in the nanoscale10.1016/j.scriptamat.2018.06.014 ↗
63. Review on the Hall-Petch relation in ferritic steel10.4028/www.scientific.net/MSF.654-656.11 ↗
64. High-pressure torsion of iron with various purity levels and validation of Hall-Petch strengthening mechanism10.1016/j.msea.2018.11.127 ↗
65. Developing a single-phase and nanograined refractory high-entropy alloy ZrHfNbTaW with ultrahigh hardness by phase transformation via high-pressure torsion10.1016/j.jallcom.2024.178274 ↗
66. Microstructure and microhardness of dual-phase high-entropy alloy by high-pressure torsion: twins and stacking faults in FCC and dislocations in BCC10.1016/j.jallcom.2021.162413 ↗
67. Microstructure, mechanical properties and high-temperature sliding wear response of a new Al0.5CrFeNiV0.5 high-entropy alloy
68. Influence of specimen dimensions on the tensile behavior of ultrafine-grained Cu10.1016/j.scriptamat.2008.05.031 ↗
69. Development of Ultrahigh strength and high ductility in nanostructured iron alloys with lattice softening and nanotwins10.1016/j.scriptamat.2012.06.019 ↗
70. High strength and high uniform ductility in a severely-deformed iron alloy by lattice softening and multimodal-structure formation10.1080/21663831.2015.1050126 ↗