journal article·2025-08

One novel Mg-Y-Ni dilute alloy with an excellent combination of strong high-temperature strength and fast dissolution rate

Yibin An, Chun Xi, Teng Li, Qinghuan Huo

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (94)

Show source-provided references
1. S. Mohapatra, R. Prasad, J. Jain, Temperature dependence of abnormal grain growth in pure magnesium, 283 (2021) 128851.10.1016/j.matlet.2020.128851 ↗
2. Investigation of rapidly decomposable AZ91-RE-xCu (x=0, 1, 2, 3, 4) alloys for petroleum fracturing balls10.1016/j.jpcs.2020.109499 ↗
3. Microstructure, mechanical properties and corrosion properties of Mg-4Zn-xNi alloys for degradable fracturing ball applications10.1016/j.jallcom.2019.02.089 ↗
4. Enhanced mechanical properties and degradation rate of Mg-3Zn-1Y based alloy by cu addition for degradable fracturing ball applications10.1016/j.matlet.2017.02.024 ↗
5. Microstructure, mechanical properties, and corrosion behavior of degradable Mg-Al-Cu-Zn-Gd alloys10.1016/j.jallcom.2016.05.288 ↗
6. A review on magnesium alloys for application of degradable fracturing tools10.1016/j.jma.2022.09.032 ↗
7. Characteristics and corrosion resistance of plasma electrolytic oxidation coatings on AZ31B mg alloy formed in phosphate – silicate mixture electrolytes10.1016/j.corsci.2014.07.038 ↗
8. Corrosion and wear resistance of micro-arc oxidation coating on glass microsphere reinforced mg alloy composite10.1007/s10853-021-06252-y ↗
9. Effect of trace ni addition on microstructure, mechanical and corrosion properties of the extruded Mg–Gd–Y–Zr–Ni alloys for dissoluble fracturing tools10.1016/j.jma.2020.08.019 ↗
10. A novel Mg-Gd-Y-Zn-Cu-Ni alloy with excellent combination of strength and dissolution via peak-aging treatment10.1016/j.jma.2022.05.012 ↗
11. Unveiling the effect of gd content on the dynamic recrystallization behavior and resultant mechanical property of magnesium10.1016/j.msea.2023.145523 ↗
12. Development of a high-strength Mg–11Gd–2Ag (wt%) alloy sheet with extra-low anisotropy10.1016/j.msea.2021.141084 ↗
13. Deformation and fracture mechanisms in WE43 magnesium-rare earth alloy fabricated by direct-chill casting and rolling10.1016/j.msea.2018.04.090 ↗
14. Effects of accumulative rolling reduction on the microstructure characteristic and mechanical properties of Mg-Gd-Y-Zn-Zr sheets processed by hot rolling10.1016/j.msea.2019.138317 ↗
15. Fabrication of magnesium alloy with high strength and heat-resistance by hot extrusion and ageing10.1016/j.msea.2013.04.108 ↗
16. Investigation of hot extruded GW84 alloy on high temperature tensile properties and microstructure evolution10.1016/j.jmrt.2021.04.092 ↗
17. Achieving strength and ductility synergy via a nanoscale superlattice precipitate in a cast Mg-Y-Zn-Er alloy10.1016/j.ijplas.2023.103558 ↗
18. Strength and ductility optimization of Mg–Y–Nd–Zr alloy by microstructural design10.1016/j.ijplas.2014.11.003 ↗
19. Enhanced degradation properties of Mg-Y-Ni alloys by tailoring the LPSO morphology for fracturing tools applications10.1016/j.matchar.2021.111489 ↗
20. Improving the corrosion resistance of MgZn1.2GdxZr0.18 (x = 0, 0.8, 1.4, 2.0) alloys via gd additions10.1016/j.corsci.2020.108962 ↗
21. Enhanced corrosion rate for Mg-xEr-1.6Ni alloys with high er content by regulating the second phase via short-time low-temperature heat treatment10.1016/j.corsci.2023.111227 ↗
22. Effects of fe concentration on microstructure and corrosion of Mg-6Al-1Zn-xFe alloys for fracturing balls applications10.1016/j.jmst.2019.04.012 ↗
23. Effects of alloying elements on microstructure and properties of magnesium alloys for tripling ball10.1007/s11661-015-3053-7 ↗
24. Achieving high strength and rapid degradation in Mg-Gd-Ni alloys by regulating LPSO phase morphology combined with extrusion10.1016/j.jma.2022.07.015 ↗
25. A dissolvable Mg-Gd-Y-Zn-Cu alloy possessing the highest yield strength for the fabrication of fracturing plugging tools10.1016/j.matlet.2023.134053 ↗
26. Effect of the morphology of long-period stacking ordered phase on mechanical properties and corrosion behavior of cast Mg-Zn-Y-Ti10.1016/j.jallcom.2018.06.056 ↗
27. Biocorrosion behavior and cytotoxicity of a Mg–Gd–Zn–Zr alloy with long period stacking ordered structure10.1016/j.matlet.2012.07.030 ↗
28. Role of the LPSO structure in the improvement of corrosion resistance of Mg-Gd-Zn-Zr alloys10.1016/j.jallcom.2018.12.233 ↗
29. Deformation behavior of Mg–Zn–Y alloys reinforced by icosahedral quasicrystalline particles10.1016/S1359-6454(02)00067-8 ↗
30. Optimized combination of room-temperature formability and high-temperature creep property in a dilute-alloyed mg sheet via tailoring nd solute segregation10.1016/j.msea.2024.146562 ↗
31. Overcoming the trade-off between stretch formability and heat resistance in magnesium via alloying dilute neodymium10.1016/j.jallcom.2021.162666 ↗
32. Substantial corrosion resistance improvement in heat-treated Mg–Gd–Zn alloys with a long period stacking ordered structure10.1016/j.matchemphys.2017.09.035 ↗
33. Grain size and texture dependence on mechanical properties, asymmetric behavior and low temperature superplasticity of ZK60 mg alloy10.1016/j.matchar.2015.06.009 ↗
34. Microstructure, mechanical and creep properties of high Ca/Al ratio Mg-Al-Ca alloy10.1016/j.msea.2016.03.001 ↗
35. Microstructure, mechanical behavior and low temperature superplasticity of ECAP processed ZM21 mg alloy10.1016/j.jallcom.2015.03.029 ↗
36. Superplasticity in a commercially extruded ZK30 magnesium alloy10.1016/j.msea.2017.10.093 ↗
37. Tensile deformation behaviors in a Fine-Grained, rolled Mg–3Al–3Sn alloy at room temperature up to 250 °C10.1002/adem.201400415 ↗
38. The microstructural evolution and superplastic behavior at low temperatures of Mg–5.00Zn–0.92Y–0.16Zr (wt%) alloys after hot extrusion and ECAP process10.1016/j.msea.2012.03.116 ↗
39. Unveiling the mechanical response and deformation mechanism of extruded Mg-2.5Nd-0.5Zn-0.5Zr alloy sheet under high-temperature tensile10.1016/j.jallcom.2022.164987 ↗
40. Enhanced mechanical properties and degradation rate of Mg–Ni–Y alloy by introducing LPSO phase for degradable fracturing ball applications10.1016/j.jma.2019.11.010 ↗
41. Effects of copper on the microstructure and properties of Mg-17Al-3Zn alloys10.1002/maco.201408090 ↗
42. Deformation-induced dynamic precipitation of 14H-LPSO structure and its effect on dynamic recrystallization in hot-extruded Mg-Y-Zn alloys10.1016/j.ijplas.2023.103573 ↗
43. Microstructural evolutions and mechanical properties of Mg-xY-2Nd-0.2Zn-0.5Zr (x = 0, 2, 4, 6 and 8) alloy under hot compression10.1016/j.msea.2019.138816 ↗
44. Optimizing the mechanical properties of a Mg-Y-Nd-Zn-Zr alloy via interrupted compression with an intermediate annealing10.1016/j.msea.2021.141102 ↗
45. Achieving exceptionally high strength in binary Mg-13Gd alloy by strong texture and substantial precipitates10.1016/j.scriptamat.2020.10.052 ↗
46. Twinning-induced plasticity with multiple twinning modes and disclinations in mg alloys10.1016/j.ijplas.2023.103595 ↗
47. Control of twin boundary mobility by solute segregation in mg binary alloys10.1016/j.scriptamat.2024.116173 ↗
48. Improving the mechanical properties of an age-hardenable magnesium alloy via regulating precipitate scale and building dislocation configuration10.1007/s11661-023-07198-3 ↗
49. Geometrical criterion for the activation of prismatic slip in AZ61 mg alloy sheets deformed at room temperature10.1016/j.actamat.2005.01.008 ↗
50. Study on edge cracking and texture evolution during 150 °C rolling of magnesium alloys: the effects of axial ratio and grain size10.1016/j.jallcom.2011.08.093 ↗
51. Exceptional fracture toughness in a high-strength mg alloy with the synergetic effects of bimodal structure, LPSO, and nanoprecipitates10.1016/j.scriptamat.2023.115675 ↗
52. Influence of grain size and grain boundary misorientation on the fatigue crack initiation mechanisms of textured AZ31 mg alloy10.1016/j.scriptamat.2021.114304 ↗
53. Contributions of multimodal microstructure in the deformation behavior of extruded mg alloys containing LPSO phase10.1016/j.ijplas.2023.103865 ↗
54. Deformation twinning in a Mg–Al–Gd ternary alloy containing precipitates with a long-period stacking-ordered (LPSO) structure10.1016/j.scriptamat.2014.06.019 ↗
55. Dual influences of deformation-induced w precipitates on dynamic recrystallization and fracture mechanism of the hot-extruded Mg-Y-Zn alloys: an experimental and phase field study10.1016/j.ijplas.2023.103772 ↗
56. Tracing the effects of calcium, stannum and zinc additions on the creep resistance of Mg-Al based alloys10.1007/s11661-023-07050-8 ↗
57. The activity of non-basal slip systems and dynamic recovery at room temperature in fine-grained AZ31B magnesium alloys10.1016/S1359-6454(03)00005-3 ↗
58. Effects of pre-compression on the three-dimensional creep anisotropy of a hot-rolled Mg-4wt%Y binary alloy sheet10.1016/j.msea.2019.138843 ↗
59. Developing a mg alloy with ultrahigh room temperature ductility via grain boundary segregation and activation of non-basal slips10.1016/j.ijplas.2023.103548 ↗
60. Insights into the post-yield microstructure of Mg-Gd-Cu alloy processed by multi-directional forging10.1016/j.jallcom.2025.178966 ↗
61. Superior strength-ductility synergy of Mg-Nd-Zn-Zr alloy rod achieved by drawing at elevated temperatures10.1016/j.ijplas.2024.103944 ↗
62. Uncovering the unexpected changes of creep properties in AZ-series mg alloys10.1016/j.msea.2022.144056 ↗
63. Hall-Petch relationship in mg alloys: a review10.1016/j.jmst.2017.07.022 ↗
64. Analysis on the compressive creep behaviors of Mg-Y alloys with various grain sizes10.1016/j.msea.2024.146448 ↗
65. Solute atom mediated Hall-Petch relations for magnesium binary alloys10.1016/j.scriptamat.2021.114451 ↗
66. Effect of grain size on the tensile deformation of wrought Mg-MM-Al-Zn-Sn alloy10.1016/j.matlet.2007.11.095 ↗
67. Mechanism of high-strength and ductility of Mg-RE alloy fabricated by low-temperature extrusion and aging treatment10.1016/j.matdes.2020.109384 ↗
68. Effect of rolling reduction on microstructure, texture, mechanical properties and mechanical anisotropy of AZ31 magnesium alloys10.1016/j.msea.2014.06.034 ↗
69. Understanding the third element effect on the extruded microstructure and mechanical strength of Mg-1wt%Bi alloy10.1016/j.jallcom.2024.178303 ↗
70. Accomplishing the goal of yield isotropy in magnesium with dilute nickel addition and two-pass extrusion10.1016/j.jallcom.2025.179271 ↗
71. An orowan precipitate strengthening equation for mechanical twinning in mg10.1016/j.ijplas.2018.08.010 ↗
72. Unveiling asymmetric precipitation strengthening during tension and compression via statistical slip activity analysis for an untextured Mg-10Gd-3Y-0.5Zr alloy10.1016/j.ijplas.2025.104354 ↗
73. Anisotropy in the tensile creep behaviors of a hot-rolled Mg-5.5wt%Y alloy sheet10.1016/j.matchar.2020.110843 ↗
74. Short-range order clusters in the long-period stacking/order phases with an intrinsic-I type stacking fault in Mg-Co-Y alloys10.1016/j.scriptamat.2021.114282 ↗
75. Unveiling the collaborative effects of static precipitation and precipitate-free zone on the compressive creep behaviors of Mg-10.5wt%Y binary alloy10.1016/j.matchar.2021.111048 ↗
76. Effects of rare-earth elements gd and y on the solid solution strengthening of mg10.1016/j.jallcom.2009.02.131 ↗
77. Solid solution strengthening in polycrystals of Mg–Sn10.1016/j.jallcom.2010.12.065 ↗
78. The yield point phenomenon in ultrafine-grained dilute Mg-Zn-Y alloys10.1016/j.matlet.2022.133315 ↗
79. Strengthening and toughening mechanisms in Mg–Zn–Y alloy with a long period stacking ordered structure10.1016/j.actamat.2010.05.012 ↗
80. Strengthening mechanisms in magnesium alloys containing ternary I, w and LPSO10.1016/j.jmst.2017.12.005 ↗
81. Impact of grain boundaries on microstructure evolution during deformation of a magnesium tricrystal10.1016/j.msea.2018.11.002 ↗
82. Inherited effect of original loading direction on the annealing behavior of a hot-compressed Mg-1.0wt%Ca sheet10.1016/j.matlet.2023.134816 ↗
83. Atomic structure of γ′′ phase in Mg–Gd–Y–Ag alloy induced by ag addition10.1080/14786435.2019.1606466 ↗
84. Achievement of fine-grained bimodal microstructures and superior mechanical properties in a multi-axially forged GWZ magnesium alloy containing LPSO10.1016/j.jallcom.2019.04.158 ↗
85. Regulating the localized corrosion of grain boundary and galvanic corrosion by adding the electronegative element in magnesium alloy10.1016/j.corsci.2024.112667 ↗
86. Gradient textures induce micro-galvanic corrosion on mg10.1016/j.jallcom.2024.176119 ↗
87. Tension-compression asymmetry and the underlying slip/twinning activity in extruded Mg–Y sheets10.1016/j.ijplas.2020.102878 ↗
88. Revealing anti-corrosion mechanism of low-alloyed Mg-Gd-Zn-Zr alloy with ultra-low corrosion rate10.1016/j.corsci.2025.112931 ↗
89. Insight into dissolution rate-regulated advanced films on Mg-Gd-Sm alloy with high anti-corrosion and discharge properties10.1016/j.actamat.2025.120952 ↗
90. Characterization of a novel 14H-LPSO structure and related elevated-temperature mechanical behaviors in an extruded Mg–Y–Zn–Cu alloy10.1016/j.msea.2019.138786 ↗
91. Effect of heat treatment on corrosion and mechanical properties of Mg-10Y-1.5Zn-0.5Zr alloy10.1007/s11665-022-07238-w ↗
92. Enhanced degradation properties of Mg-Gd-Cu alloys by introducing profuse solute segregated stacking faults phase10.1016/j.intermet.2023.107979 ↗
93. Tailoring the microstructural characteristic and improving the corrosion rate of Mg-Gd-Ni alloy by heat treatment with different volume fraction of LPSO phase10.1016/j.corsci.2022.110806 ↗
94. Modulation of corrosion properties by heat treatment and extrusion with mechanism analysis of high mechanical strength Mg-5.6Dy-3.1Ni alloy10.1016/j.matchar.2024.113662 ↗