Friction stirred materials have unavoidable heterogeneity in the processed microstructure, which is more severe in the transverse direction of the run and deteriorates structural strength . Effect of post friction stir pre-stretching and aging on this microstructural heterogeneity in an Al-Cu-Li alloy sheet is investigated using highly resolved local tensile behaviour . Local stress-strain curves, at 1 mm spacing were obtained using transverse tensile tests accompanied by a continuous strain measurement using digital image correlation and the hybrid model was used for strain hardening analysis. Local mechanical and strain hardening behaviour is correlated with microstructural information obtained from transmission electron microscopy and differential scanning calorimetry . Aging with and without pre-stretch, both effectively increased the global strength, but the aging response was heterogeneous in all the cases due to variation in solute content and the strain hardening ability within the processed region. Direct aging enhanced the microstructural heterogeneity and led to strain localization , while strain hardening during pre-stretch contributed more strength to the weaker regions, enhanced T1 precipitation and thus effectively reduced the strength heterogeneity. This study provides insight into detailed mechanical behaviour information within a friction stir processed material which can be applied to strengthen structures produced with friction stir technology.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. W.M. Thomas, E.D. Nicholas, J.C. Needham, M.G. Murch, P. Templesmith, C.J. Dawes, Friction stir welding, 9125978 (n.d.).
2. Friction stir processing technology: a review10.1007/s11661-007-9459-0 ↗
3. Potentials and strategies of solid-state additive friction-stir manufacturing technology: a critical review10.1016/j.jmapro.2018.09.030 ↗
4. H.Z. Yu, R.S. Mishra, Additive friction stir deposition: a deformation processing route to metal additive manufacturing, Http://Mc.Manuscriptcentral.Com/Tmrl 9 (2020) 71–83. https://doi.org/10.1080/21663831.2020.1847211.10.1080/21663831.2020.1847211 ↗
5. Friction stir welding/processing of metals and alloys: a comprehensive review on microstructural evolution10.1016/j.pmatsci.2020.100752 ↗
6. Surface composites by friction stir processing: a review10.1016/j.jmatprotec.2015.04.019 ↗
7. In-situ investigation on dislocation slip concentrated fracture mechanism of linear friction welded dissimilar Ti17(α+β)/Ti17(β) titanium alloy joint10.1016/j.msea.2023.144991 ↗
8. Controlling deformation and residual stresses in a TIG joint for Invar steel molds10.1016/j.jmrt.2023.10.036 ↗
9. Recent developments in friction stir welding of Al-alloys10.1007/s11665-014-0968-x ↗
10. Effect of localized corrosion on fatigue–crack growth in 2524-T3 and 2198-T851 aluminum alloys used as aircraft materials10.1007/s11665-018-3244-7 ↗
11. The evolution of Al-Li base products for aerospace and space applications10.1007/s11661-012-1155-z ↗
12. Strengthening mechanisms, deformation behavior, and anisotropic mechanical properties of Al-Li alloys: a review10.1016/j.jare.2017.12.004 ↗
13. Quantitative contribution of T1 phase to the strength of Al-Cu-Li alloys10.1007/s10853-021-06432-w ↗
14. Identifying the crystal structure of T1 precipitates in Al-Li-Cu alloys by ab initio calculations and HAADF-STEM imaging10.1016/j.jmst.2022.05.056 ↗
15. S.C. Wang, M.J. Starink, Precipitates and intermetallic phases in precipitation hardening Al–Cu–Mg–(Li) based alloys, Https://Doi.Org/10.1179/174328005×14357 50 (2013) 193–215. https://doi.org/10.1179/174328005×14357.10.1179/174328005X14357 ↗
16. F. de Geuser, B. Malard, A. Deschamps, Microstructure mapping of a friction stir welded AA2050 Al–Li–Cu in the T8 state, Http://Dx.Doi.Org/10.1080/14786435.2014.887862 94 (2014) 1451–1462. https://doi.org/10.1080/14786435.2014.887862.10.1080/14786435.2014.887862 ↗
17. Aging kinetics of friction stir welded Al-Cu-Li-Mg-Ag and Al-Cu-Li-Mg alloys10.1016/j.matdes.2016.07.126 ↗
18. Influence of Cu/Li ratio on the microstructure evolution of bobbin-tool friction stir welded Al–Cu–Li alloys10.1016/j.jmrt.2019.01.014 ↗
19. R.S. Mishra, H. Sidhar, Chapter 3-temperature evolution and thermal management during FSW of 2XXX alloys, Friction Stir Welding of 2XXX Aluminum Alloys Including Al-Li Alloys, Butterworth-Heinemann (2017) 37e46.10.1016/B978-0-12-805368-3.00003-0 ↗
20. Microstructure-strength relationship in friction-stir welded 6061-T6 aluminum alloy10.1016/j.msea.2020.139858 ↗
21. Optimization of processing-microstructure-properties relationship in friction-stir welded 6061-T6 aluminum alloy10.1016/j.msea.2016.03.063 ↗
22. The role of cryogenic quenching on the mechanical properties of FSWed 6061-T6 aluminum alloy10.1016/j.msea.2022.142896 ↗
23. T.Le Jolu, T.F. Morgeneyer, A.F. Gourgues-Lorenzon, Effect of joint line remnant on fatigue lifetime of friction stir welded Al–Cu–Li alloy, Https://Doi.Org/10.1179/136217110×12813393169453 15 (2013) 694–698. https://doi.org/10.1179/136217110×12813393169453.10.1179/136217110X12813393169453 ↗
24. Influence of Cu/Li ratio on the microstructure evolution of bobbin-tool friction stir welded Al–Cu–Li alloys10.1016/j.jmrt.2019.01.014 ↗
25. Microstructure and tensile response of friction stir welded Al–Cu–Li (AA2198-T8) alloy
26. Thermal cycles, microstructures and mechanical properties of AA7075-T6 ultrathin sheet joints produced by high speed friction stir welding10.1016/j.matchar.2022.111873 ↗
27. A review of microstructural changes occurring during FSW in aluminium alloys and their modelling10.1016/j.jmatprotec.2020.116706 ↗
28. Effect of friction stir welding parameters on mechanical properties and microstructure of AA2195 Al–Li alloy welds10.1007/s12666-019-01570-x ↗
29. Effect of post weld artificial aging and water cooling on microstructure and mechanical properties of friction stir welded 2198-T8 Al-Li joints10.1016/j.jmst.2022.01.020 ↗
30. Influence of water cooling on microstructure and mechanical properties of friction stir welded 2014Al-T6 joints10.1016/j.msea.2014.06.093 ↗
31. Improvements of strength and ductility in aluminum alloy joints via rapid cooling during friction stir welding10.1016/j.msea.2012.03.094 ↗
32. In-process cooling of friction stir extruded joints for increased weld performance via compressed air, water, granulated dry ice, and liquid nitrogen10.1016/j.jmapro.2021.06.021 ↗
33. Avoiding abnormal grain growth in thick 7XXX aluminium alloy friction stir welds during T6 post heat treatments10.1016/j.msea.2021.140901 ↗
34. Effect of tool dimensions and parameters on the microstructure of friction stir welded aluminum 7449 alloy of various thicknesses10.1016/j.msea.2016.12.077 ↗
35. Effect of the ageing on precipitation spatial distribution in stationary shoulder friction stir welded AA2050 alloys10.1016/j.matchar.2019.06.006 ↗
36. Microstructure distribution in an AA2050 T34 friction stir weld and its evolution during post-welding heat treatment10.1016/j.actamat.2015.08.068 ↗
37. N.Eswara Prasad, A.A. Gokhale, R.J.H. Wanhill, Aluminum-Lithium Alloys: Processing, Properties, and Applications, (n.d.) 596.
38. Influence of natural ageing and deformation on precipitation in an Al–Cu–Li alloy10.1002/adem.201300098 ↗
39. Quantification of the influence of increased pre-stretching on microstructure-strength relationships in the Al–Cu–Li alloy AA219510.1016/j.actamat.2016.02.017 ↗
40. Sub-zero temperature dependence of tensile response of friction stir welded Al-Cu-Li (AA2198) alloy
41. U.F. Kocks, H. Mecking, Physics and phenomenology of strain hardening: the FCC case, Prog Mater Sci 48 (2003) 171–273. www.elsevier.com/locate/pmatsci (accessed July 11, 2023).10.1016/S0079-6425(02)00003-8 ↗
42. Dislocation-Density–Related Constitutive Modeling
43. The influence of precipitation on the work-hardening behavior of the aluminum alloys AA6111 and AA703010.1007/s11661-003-0007-2 ↗
44. The Li stance on precipitation in Al–Li-based alloys: an investigation by X-ray Raman spectroscopy10.1007/s10853-022-07018-w ↗
45. The influence of Cu/Li ratio on precipitation in Al–Cu–Li–x alloys10.1016/j.actamat.2012.12.041 ↗
46. Quantitative analysis of the influences of pre-treatments on the microstructure evolution and mechanical properties during artificial ageing of an Al–Cu–Li–Mg–Ag alloy10.1016/j.msea.2020.139253 ↗
47. Friction stir welding of 2060–T8 AlLi alloy. Part I: microstructure evolution mechanism and mechanical properties
48. Fracture-mechanism maps and their construction for F.C.C. metals and alloys
49. Void nucleation during ductile rupture of metals: a review10.1016/j.pmatsci.2023.101085 ↗
50. Void-nucleation vs void-growth controlled plastic flow localization in materials with nonuniform particle distributions10.1016/S0020-7683(97)00145-5 ↗
51. Temperature evolution, microstructure, and properties of friction stir welded ultra-thick 6082 aluminum alloy joints10.1007/s00170-020-05422-7 ↗
52. Temperature evolution, material flow, and resulting mechanical properties as a function of tool geometry during friction stir welding of AA608210.1007/s11665-023-08671-1 ↗
53. Friction stir welding of Al alloy 2219-T8: Part I-evolution of precipitates and formation of abnormal Al2Cu agglomerates10.1007/s11661-016-3648-7 ↗
54. 2198 Al–Li plates joined by friction stir welding: mechanical and microstructural behavior10.1016/j.matdes.2009.02.021 ↗
55. Effect of rotation speed to welding speed ratio on microstructure and mechanical behavior of friction stir welded aluminum–lithium alloy joints10.1002/adem.201300147 ↗
56. The use of the pseudo-voigt function in the variance method of x-ray line-broadening analysis10.1107/S0021889896015464 ↗