journal article·2024-06

Enhanced hydrogen adsorption capability of 2:17-type Sm-Co strips via microstructure modification

Meng Zheng, Yifei Bi, Zhenyu Hou, Chao Wang, Junming Wang, Lei Wang, Ze Duan, Boxi Zhang, Yikun Fang, Minggang Zhu, Wei Li

Publisher page

Abstract

The hydrogenation kinetics of Sm 26.2Co balFe xCu 4.0Zr 2.3 (x = 23, 27 in wt%) strips (Fe23 and Fe27 strips) has been investigated. The phase composition, morphology, surface roughness and the inner pores of the strips also have been studied by XRD, SEM, optical profilometer and non-destructive micro-computerized tomography. Compared to Fe23 and Fe27 strips, heat-treated strips (H-Fe23 and H-Fe27) and corrosion heat-treated strips (HC-Fe23 and HC-Fe27) exhibit a relatively higher hydrogen absorption capability. Fragmentation behavior occurs in HC-Fe23, H-Fe27 and HC-Fe27 strips during hydrogenation. After heat treatment, the grain size and inner pore size increase, leading to the disappearance of fine crystal strengthening and the concentration internal stress. For corrosion-treated strips, increased surface roughness and deeper grooves result in the formation of surface stress concentration, ultimately leading to an increased susceptibility to hydrogen embrittlement. Accordingly, the increase of grain size, inner pore size and rougher surface is beneficial for hydrogenation and hydrogen embrittlement.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen Storage and Materials · Magnetic Properties of Alloys · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Phase separation and chemistry evolution in Fe-rich Sm(CobalFe0.31Cu0.07Zr0.025)7.7 magnets: the effect of initial defect10.1016/j.actamat.2022.118664 ↗
2. Atomic-scale oxidation of a Sm2Co17-type magnet10.1016/j.actamat.2021.117343 ↗
3. The microstructure and magnetic characteristics of Sm(CobalFe0.1Cu0.09Zr0.03)7.24 high temperature permanent magnets10.1016/j.scriptamat.2017.01.026 ↗
4. Identifications of SmCo5 and Smn+1Co5n−1-type phases in 2:17-type Sm-Co-Fe-Cu-Zr permanent magnets10.1016/j.scriptamat.2020.02.028 ↗
5. Sm(Co, Fe, Cu, Zr)z sintered magnets with a maximum operating temperature of 500°C10.1016/j.jmmm.2006.01.107 ↗
6. Twinning, phase boundary structure and development of high coercivity in Fe-rich Sm2Co17-type magnets10.1016/j.jre.2021.01.004 ↗
7. Correlation of mechanical anisotropy with fine grain strengthening for Sm2Co17-type sintered permanent magnets10.1016/j.jre.2021.07.012 ↗
8. Tremendous enhancement of magnetic performance for Sm(CoFeCuZr)z magnet based on multiscale copper redistribution10.1016/j.jre.2021.08.001 ↗
9. Overview of composition and technique process study on 2:17-type Sm–Co high-temperature permanent magnet10.1007/s12598-020-01514-1 ↗
10. Microstructure characteristics and optimization of 2:17-type Sm-Co sintered magnets with different iron content10.1016/j.jmmm.2020.167288 ↗
11. Cellular structure regulation and coercivity enhancement induced by La2O3 doping in 2:17 type SmCo magnet10.1016/j.jallcom.2020.156589 ↗
12. Defects-aggregated cell boundaries induced domain wall curvature change in Fe-rich Sm–Co–Fe–Cu–Zr permanent magnets10.1007/s10853-020-04889-9 ↗
13. Role of primary Zr-rich particles on microstructure and magnetic properties of 2:17-type Sm-Co-Fe-Cu-Zr permanent magnets10.1016/j.jmst.2020.04.018 ↗
14. Role of nanoscale interfacial defects on magnetic properties of the 2:17-type Sm–Co permanent magnets10.1016/j.jallcom.2019.152620 ↗
15. Micron-scale 1:5H-based precipitated phase with the lamellar structure of sintered Sm2Co17-based magnets and its potential application10.1016/j.jmst.2022.12.046 ↗
16. Identification of optimal solid solution temperature for Sm2Co17-type permanent magnets with different Fe contents10.1007/s12598-020-01701-0 ↗
17. The formation mechanism of 1:5H phase in Sm(Co, Fe, Cu, Zr)z melt-spun ribbons with high iron content10.1016/j.jmmm.2019.165939 ↗
18. Effects of copper and zirconium contents on microstructure and magnetic properties of Sm(Co,Fe,Cu,Zr)z magnets with high iron content10.1016/j.jre.2020.03.002 ↗
19. Influence of 1:7H phase stability on the evolution of cellular microstructure in Fe-rich Sm-Co-Fe-Cu-Zr magnets10.1016/j.jallcom.2023.170604 ↗
20. Optimization of both coercivity and knee-point magnetic field of Sm2Co17-type magnets via solid solution process10.1016/j.jre.2019.11.009 ↗
21. Influence of intermediate-heat treatment on the structure and magnetic properties of iron-rich Sm(CoFeCuZr)Z sintered magnets10.1063/1.4906757 ↗
22. Anisotropic Sm-Co nanopowder prepared by induction thermal plasma10.1016/j.jallcom.2021.160633 ↗
23. Shortened processing duration of high-performance Sm-Co-Fe-Cu-Zr magnets by stress-aging10.1016/j.jmst.2021.06.078 ↗
24. Optimization of temperature coefficient of remanence and magnetic properties of sintered Sm0.7Dy0.1Gd0.2(CobalFe0.2Cu0.08Zr0.025)7.2 magnets prepared by strip-casting technique10.1109/TMAG.2013.2274961 ↗
25. Effect of strip casting on microstructure and magnetic properties of 2:17 type Sm-Co sintered magnets
26. Microstructure and magnetic properties of Sm(Co balFe0.28Cu0.06Zr0.02)7.84 magnet prepared by hydrogen decrepitation and mechanical crushing
27. Combination strategy for high-performance Sm(CoFeCuZr)z sintered permanent magnet: Synergistic improvement of the preparation process10.1016/j.actamat.2023.118901 ↗
28. The potential of hydrogen in permanent magnet production10.1016/0022-5088(87)90524-8 ↗
29. Hydrogen decrepitation of a 2/17 sintered magnet at room temperature10.1016/j.jallcom.2006.11.139 ↗
30. Kinetic studies of hydrogen desorption in SmCo 2/17-type sintered magnets10.1016/j.tca.2008.12.021 ↗
31. Effect of hydrogen pressure on hydrogenation and pulverization behavior of Sm(CoFeCuZr)z ingot and strip casting flake10.1016/j.jallcom.2022.167427 ↗
32. Effect of grain size and precipitates on hydrogen embrittlement susceptibility of nickel alloy 71810.1016/j.ijhydene.2023.11.233 ↗
33. Effects of grain size and dislocation density on the susceptibility to high-pressure hydrogen environment embrittlement of high-strength low-alloy steels10.1016/j.ijhydene.2011.10.099 ↗
34. Effect of grain size on the susceptibility of martensitic steel to hydrogen-related failure10.1080/09500830500482316 ↗
35. Hydrogen-enhanced fatigue life analysis of Cr–Mo steel high-pressure vessels10.1016/j.ijhydene.2017.02.103 ↗
36. Effect of hydrogen and stress concentration on the notch tensile strength of AISI 4135 steel10.1016/j.msea.2005.03.008 ↗
37. The effect of stress concentration on hydrogen embrittlement of a low alloy steel10.1016/0010-938X(96)00161-8 ↗
38. Studies on structural transformation and magnetic properties in Sm2Co17 type alloys10.1023/A:1017992132473 ↗
39. Hydrogen storage performances of La-Sm-Mg-Ni alloy prepared by casting and ball milling10.1016/j.jpcs.2022.111165 ↗
40. Hydrogen storage characteristics of Ti1.04Fe0.7Ni0.1Zr0.1Mn0.1Pr0.06 alloy treated by ball milling10.1016/j.jallcom.2022.167024 ↗
41. Microstructure formation and electrical resistivity behavior of rapidly solidified Cu-Fe-Zr immiscible alloys10.1016/j.jmst.2019.10.038 ↗