Multiscale microstructure regulation and synergistic strengthening mechanisms in Ti-6Al-4V alloy via electropulsing treatment

Tingting Bao, Changsheng Tan, Chaowen Huang, Qiang Li, YiDuo Fan, Guojun Zhang, Pengcheng Guo

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Electromagnetic Effects on Materials · Material Properties and Failure Mechanisms · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. C. Hui, The effect of heat treatment on microstructure evolution and tensile properties of selective laser melted Ti6Al4V alloy10.1016/j.jallcom.2018.12.051 ↗
2. Controllable mechanical anisotropy of selective laser melted Ti6Al4V: a new perspective into the effect of grain orientations and primary grain structure10.1016/j.msea.2021.142031 ↗
3. Densification, tailored microstructure, and mechanical properties of selective laser melted Ti-6Al-4V alloy via annealing heat treatment10.3390/mi13020331 ↗
4. Gradient microstructure and mechanical properties of Ti-6Al-4V titanium alloy fabricated by high-frequency induction quenching treatment10.1016/j.matdes.2022.111031 ↗
5. Strength-ductility improvement achieved by introducing heterostructured martensite in a Ti-6Al-4V alloy10.1016/j.matchar.2022.112230 ↗
6. Targeted heat treatment of additively manufactured Ti-6Al-4V for controlled formation of Bi-lamellar microstructures10.1016/j.jmst.2021.01.004 ↗
7. New insight into deformation mechanism for a low-cost titanium alloy during isothermal compression10.1016/j.jallcom.2025.180418 ↗
8. Evolution characteristics of orientation relationships during the co-evolution of α/β phase for Ti alloy10.1016/j.matchar.2023.113111 ↗
9. Strength and ductility-related properties of ultrafine grained two-phase titanium alloy produced by warm multiaxial forging10.1016/j.msea.2011.12.102 ↗
10. A novel low-cost high-strength β titanium alloy: microstructure evolution and mechanical behavior10.1016/j.jallcom.2023.170497 ↗
11. Microstructure and deformation behavior of Ti-6Al-4V alloy by high-power laser solid forming10.1016/j.actamat.2017.04.026 ↗
12. Crack healing in SUS304 stainless steel by electropulsing treatment10.1016/j.jclepro.2015.12.060 ↗
13. Regulating the tensile properties of a nano-lamellar austenitic stainless steel via cryogenic electropulsing10.1002/adem.202101623 ↗
14. Achieving superb mechanical properties in CoCrFeNi high-entropy alloy microfibers via electric current treatment10.1016/j.actamat.2024.120203 ↗
15. Effect of high density electropulsing treatment on formability of TC4 titanium alloy sheet10.1016/S1003-6326(07)60053-3 ↗
16. Effect of electropulsing treatment on microstructure and mechanical properties of intermetallic Al3Ti alloy10.1016/j.jallcom.2017.03.085 ↗
17. Effects of electropulsing on the microstructure and microhardness of a selective laser melted Ti6Al4V alloy10.1016/j.jallcom.2021.160044 ↗
18. Rapidly modifying microstructure and mechanical properties of AA7150 Al alloy processed with electropulsing treatment10.1016/j.jmst.2021.03.060 ↗
19. Effects of short time electric pulse heat treatment on microstructures and mechanical properties of hot-rolled Ti-6Al-4V alloy10.1016/j.msea.2014.08.085 ↗
20. Inducing TiAl3 in titanium alloys by electric pulse heat treatment improves mechanical properties10.1016/j.jallcom.2012.09.082 ↗
21. Introducing ω and O′ nanodomains in Ti-6Al-4V: the mechanism ofaccelerating α → β transformation kinetics via electropulsing10.1016/j.jmst.2023.04.014 ↗
22. Improved mechanical properties of Mg-9Al-1Zn alloy by the combination of aging, cold-rolling and electropulsing treatment10.1016/j.jallcom.2014.11.154 ↗
23. Accelerated recrystallization behavior of commercially pure titanium subjected to an alternating-current electropulse10.1016/j.jmrt.2021.11.045 ↗
24. Difference in recrystallization between electropulsing-treated and furnace-treated NiTi alloy10.1016/j.jallcom.2015.10.239 ↗
25. Healing of fatigue crack in steel with the application of pulsed electric current10.1016/j.mtla.2020.100906 ↗
26. Efficiency improvement of fatigue crack healing by multiple high-density pulsed electric currents: application to austenitic stainless steel10.1016/j.engfracmech.2023.109235 ↗
27. On the thermodynamics and kinetics of electropulsing induced dissolution of β-Mg17Al12 phase in an aged Mg-9Al-1Zn alloy10.1016/j.actamat.2009.06.044 ↗
28. Electric current-induced annealing during uniaxial tension of aluminum alloy10.1016/j.scriptamat.2013.11.019 ↗
29. Strength and ductility improvement of the axial gradient microstructure TC21 titanium alloys manufactured by electropulsing plus step-quenching treatment10.1016/j.jallcom.2024.173979 ↗
30. Enhanced strength-ductility synergy in Ti55531 titanium alloys through gradient microstructural design strategy10.1016/j.msea.2024.146823 ↗
31. Microstructure evolution and mechanical property response of TC11 titanium alloy under electroshock treatment10.1016/j.matdes.2020.109322 ↗
32. Heterostructures enhance simultaneously strength and ductility of a commercial titanium alloy10.1016/j.actamat.2023.119182 ↗
33. Achieving synergy between strength and ductility in metastable β-titanium alloy through a novel multi-morphological microstructure10.1016/j.jallcom.2024.177863 ↗
34. A comparative study on misorientations to determine the extent of recrystallization in pure ETP copper10.1134/S0031918X20140094 ↗
35. Inducing TiAl3 in titanium alloys by electric pulse heat treatment improves mechanical properties10.1016/j.jallcom.2012.09.082 ↗
36. Superior mechanical properties of 40Cr steel obtained by quenching and microstress relieving under electropulsing10.1016/j.msea.2019.138782 ↗
37. Enhanced stability of retained austenites in quenched 25SiMn2MoV steel by electro-pulsing current10.1016/j.msea.2019.138642 ↗
38. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility10.1073/pnas.1517193112 ↗
39. Towards strength-ductility synergy through the design of heterogeneous nanostructures in metals10.1016/j.mattod.2017.02.003 ↗
40. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti-6Al-4V10.1016/j.msea.2013.04.099 ↗
41. Ultrafine duplex microstructure and excellent mechanical properties of TC4 alloy via a novel thermo-mechanical treatment10.1016/j.jallcom.2018.07.141 ↗
42. Low-cost Ti-6Al-4V containing low content nano-carbon solid solution for achieving high strength and good ductility10.1016/j.matchar.2024.114208 ↗
43. Remarkable increase in high-cycle fatigue resistance in a titanium alloy with a fully lamellar microstructure10.1016/j.ijfatigue.2020.105724 ↗
44. In-situ SEM observations of tensile deformation of the lamellar microstructure in TC21 titanium alloy10.1016/j.msea.2012.08.134 ↗
45. Microstructure, mechanical properties and reinforcement mechanism of dual-scale TC4 titanium alloy prepared by cryomilling and plasma activated sintering10.1016/j.msea.2018.08.097 ↗
46. L. Liu, Grain size mismatch dependent crack blunting in bimodal materials10.1007/s11837-023-06118-5 ↗
47. Heterostructured materials10.1016/j.pmatsci.2022.101019 ↗
48. Heterostructures enhance simultaneously strength and ductility of a commercial titanium alloy10.1016/j.actamat.2023.119182 ↗
49. Evolution of the α phase and microhardness for hot isostatic pressed Ti-6Al-4V alloy during multi-pass deformation10.1016/j.matchar.2021.111263 ↗
50. Crystal plasticity modeling of slip activity in Ti-6Al-4V under high cycle fatigue loading10.1016/j.ijplas.2008.08.004 ↗
51. Characterization of deformation in primary α phase and crack initiation and propagation of TC21 alloy using in-situ SEM experiments10.1016/j.msea.2018.03.123 ↗
52. Phase transformation in titanium alloys: a review10.1016/S1003-6326(24)66597-0 ↗