This article presents an investigation of the ageing response of modern high-strength aluminium alloy 2519 (Al–5.64Cu-0.33Mn-0.23Mg-0.01Si (wt%)) after cyclic strengthening (CS). The impact of the pre-straining value on the mechanical properties, microstructure and phase composition was elucidated via hardness and tensile testing, analytical transmission and orientation imaging electron microscopy. The results show that cyclic hardening has a significant impact on the ageing behaviour of the alloy. Applying cyclic pre-straining in conjunction with monotonic enhances strength and ductility at once. This novel high-performance treatment results in superior strength-ductility combination. The improved mechanical properties are attributed to the observed changes in microstructure. The introduction of vacancies and dislocations, by repetitive and elastic straining before artificial ageing, leads to great homogeneous structure and an increase in the number density and volume fraction of the main strengthening phases (θ′ and Ω) and clusters/zones. Therefore, this work should suggest a strategy for developing a novel treatment of aluminium alloys with excellent mechanical properties.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Polmear · 2017
2. Fundamentals of Aluminium Metallurgy. Production
3. The interaction of plasticity and diffusion controlled precipitation reactions10.1016/S1359-6462(03)00479-2 ↗
4. Martin · 1998
5. Handbook of Aluminum: Vol. 1
6. Observation of giant diffusivity along dislocation cores10.1126/science.1151771 ↗
7. In situ evaluation of dynamic precipitation during plastic straining of an Al–Zn–Mg–Cu alloy10.1016/j.actamat.2012.01.002 ↗
8. Effect of plastic deformation on the ageing behaviour of an Al–Cu–Mg alloy with a high Cu/Mg ratio10.1016/j.msea.2018.09.017 ↗
9. Ageing response of cold-rolled Al–Cu–Mg alloy10.1016/j.msea.2020.139148 ↗
10. Unusual ageing behaviour of friction-stir welded Al–Cu–Mg alloy10.1016/j.msea.2020.139882 ↗
11. Precipitation strengthening of aluminum alloys by room-temperature cyclic plasticity10.1126/science.aav7086 ↗
12. Training high-strength aluminum alloys to withstand fatigue10.1038/s41467-020-19071-7 ↗
13. Enhanced mechanical properties in an Al-Mg-Cu alloy processed by the combination of cyclic deformation and aging heat treatment10.1016/j.jallcom.2022.165070 ↗
14. The effect of chemical patterning induced by cyclic plasticity on the formation of precipitates during aging of an Al–Mg–Si alloy10.1016/j.msea.2021.141265 ↗
15. Strengthening mechanism of 2219 Al-Cu alloy by room-temperature random vibration10.1016/j.jallcom.2022.167878 ↗
16. Enhancing the strength and sensitization resistance of 5xxx alloys via nanoscale clustering induced by room-temperature cyclic plasticity
17. Quantitative measurements of dynamic precipitation during fatigue of an Al–Zn–Mg–(Cu) alloy using small-angle X-ray scattering10.1016/j.actamat.2014.04.027 ↗
18. Effect of cyclic ageing on the early-stage clustering in Al–Zn–Mg(-Cu) alloys10.1016/j.msea.2022.143280 ↗
19. Metallic Materials Properties Development and Standardization (MMPDS): MMPDS-11, Battelle Memorial Institute, 2016.
20. Aging behavior of an Al–Cu–Mg alloy10.1016/j.jallcom.2018.05.053 ↗
21. Assessment of local deformation using EBSD: quantification of accuracy of measurement and definition of local gradient10.1016/j.ultramic.2011.02.004 ↗
22. Analysis on the dissolution behavior of various size Cu-Mg co-clusters near a fatigue crack tip of underaged Al-Cu-Mg alloy during cyclic loading10.1016/j.jallcom.2016.12.323 ↗
23. Precipitates and intermetallic phases in precipitation hardening Al–Cu–Mg–(Li) based alloys10.1179/174328005X14357 ↗
24. Dynamic precipitation during cyclic deformation of an underaged Al–Cu alloy10.1016/j.msea.2011.06.037 ↗
25. The thermodynamics of and strengthening due to co-clusters: general theory and application to the case of Al–Cu–Mg alloys10.1016/j.actamat.2009.01.021 ↗
26. Role of vacancy–solute complex in the initial rapid age hardening in an Al–Cu–Mg alloy10.1016/S1359-6454(00)00348-7 ↗
27. Low energy dislocation structures produced by cyclic deformation10.1016/0025-5416(86)90281-8 ↗
28. Fundamental factors on formation mechanism of dislocation arrangements in cyclically deformed fcc single crystals10.1016/j.pmatsci.2010.12.001 ↗
29. Ch. 57 Collective behaviour of dislocations in plasticity10.1016/S1572-4859(02)80008-0 ↗
30. Precipitates in aluminium alloys
31. Transforming solid-state precipitates via excess vacancies10.1038/s41467-020-15087-1 ↗
32. Point defect interactions with Guinier-Preston zones in Al-Cu based alloys: vacancy mediated GPZ to θ′-phase transformation10.1016/j.scriptamat.2019.02.024 ↗
33. Classification of the role of microalloying elements in phase decomposition of Al based alloys10.1016/S1359-6454(99)00475-9 ↗
34. Vacancy–solute interactions during multiple-step ageing of an Al–Cu–Mg–Ag alloy10.1016/j.scriptamat.2008.09.011 ↗
35. Microstructural evolution during ageing of Al–Cu–Li–x alloys10.1016/j.actamat.2013.12.001 ↗
36. Influence of dislocation morphology on T1 precipitation of an Al-Cu-Li alloy10.1016/j.jallcom.2023.169463 ↗
37. Improvement of high temperature strength of 2219 alloy by Sc and Zr addition through a novel three-stage heat treatment route10.1016/j.msea.2018.07.003 ↗