Influence of Cu distribution on the coercivity of Sm(CobalFe0.25Cu0.06Zr0.02)7.5 magnets during microwave aging process
Source abstract
Abstract
In this study, we investigated the magnetic properties, microstructures, and Cu distribution on the mechanism of coercivity enhancement of Sm(Co balFe 0.25Cu 0.06Zr 0.02) 7.5 magnets during two-step and multistage microwave aging treatments. The intrinsic coercivity, H cj, and maximum energy product, ( BH) max , increase from 15.9 to 24.4 kOe and from 24.3 to 26.5 MGOe, respectively, upon transitioning from two-step to multistage aging. The aged alloys possess a cellular microstructure comprising rhombohedral 2:17 R cell phase and hexagonal 1:5 cell boundary phase after a short microwave aging time of 3 h. The multistage aged alloy exhibits a larger cell size, thicker cell walls, and higher Cu concentration in the 1:5 phase than the two-step aged sample. Elemental mapping reveals Cu atom enrichment at the cell boundary centers and at the 2:17 R/1:5 triple junction of the cell boundary phase, but depletion at the cell boundary edges during multistage aging. First-principles calculations indicate that Cu atoms occupy the Co(2c) sites of a SmCo 5 unit cell and weaken not only the strong Co(2c)–Co(3g) direct exchange-coupling interaction, but also the exchange-coupling interaction between Sm 4 f and Co 3 d electrons, giving rise to low 1:5 phase exchange constant values. Furthermore, the enrichment of Cu atoms at the center of the cell wall and at the 2:17 R/1:5 triple junction of the cell boundary phase produces a gradual increase in the domain wall energy difference as a function of the edge-to-center distance in the cell boundary phase. This enrichment enhances the domain wall pinning strength and increases coercivity. A high concentration and optimal distribution of Cu are critical for achieving a high H cj. The results of this study provide theoretical guidance to future studies on the mechanism controlling the coercivity of Sm 2Co 17-based permanent magnets.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic properties of thin films · Magnetic Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Attractive-domain wall-pinning controlled Sm-Co magnets overcome the coercivity-remanence trade-off10.1016/j.actamat.2018.10.046 ↗
2. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
3. Mechanism of phase transformation in 2:17 type SmCo magnets investigated by phase stabilization10.1016/j.scriptamat.2015.10.041 ↗
4. Correlation of microchemistry of cell boundary phase and interface structure to the coercivity of Sm(Co0.784Fe0.100Cu0.088Zr0.028)7.19 sintered magnets10.1016/j.actamat.2016.12.050 ↗
5. Understanding the role of element grain boundary diffusion mechanism in Nd-Fe-B magnets
6. Intrinsically high magnetic performance in core‐shell structural (Sm,Y)Fe12‐based permanent magnets
7. Grain boundary optimization induced substantial squareness enhancement and high performance in iron-rich Sm-Co-Fe-Cu-Zr magnets10.1016/j.jmst.2020.12.067 ↗
8. The effect of multi-scale Cu distribution regulation on magnetic properties of Sm(CoFeCuZr)z magnets10.1016/j.jmmm.2020.166484 ↗
9. Effect of Cu redistribution in grain boundary on magnetic properties of Sm(Co0.665Fe0.25Cu0.06Zr0.025)7 permanent magnets10.1016/j.jallcom.2018.01.164 ↗
10. Excellent magnetic and mechanical properties of the Sm2Co17-based magnets fabricated via microwave processing10.1016/j.jallcom.2021.159071 ↗
11. Microstructures of precipitation-hardened SmCo permanent magnets10.1063/1.330867 ↗
12. Defects-aggregated cell boundaries induced domain wall curvature change in Fe-rich Sm-Co-Fe-Cu-Zr permanent magnets10.1007/s10853-020-04889-9 ↗
13. Microchemistry and magnetization reversal mechanism in melt-spun 2:17-type Sm-Co magnets10.1063/1.1611641 ↗
14. Cellular structure regulation and coercivity enhancement induced by La2O3 doping in 2:17 type SmCo magnet10.1016/j.jallcom.2020.156589 ↗
15. Optimization of both coercivity and knee-point magnetic field of Sm2Co17-type magnets via solid solution process10.1016/j.jre.2019.11.009 ↗
16. Microstructural analysis during the step-cooling annealing of iron-rich Sm(Co0.65Fe0.26Cu0.07Zr0.02)7.8 anisotropic sintered magnets10.1109/TMAG.2017.2715372 ↗
17. Direct evidence for Cu concentration variation and its correlation to coercivity in Sm(Co0.74Fe0.1Cu0.12Zr0.04)7.4 ribbons10.1016/j.scriptamat.2009.01.006 ↗
18. Influence of Zr and Cu content on the microstructure and coercivity in Sm(CobalFe0.1CuyZrx)8.5 magnets10.1063/1.373330 ↗
19. Effects of copper and zirconium contents on microstructure and magnetic properties of Sm(Co,Fe,Cu,Zr)z magnets with high iron content10.1016/j.jre.2020.03.002 ↗
20. Nanoscale short-range ordering induced cellular structure and microchemistry evolution in Sm2Co17-type magnets10.1016/j.actamat.2020.09.057 ↗
21. Magnetic moments and exchange interaction in Sm(Co,Fe)5 from first-principles10.1016/j.commatsci.2010.10.019 ↗
22. First principles study on the electronic structure and effective exchange interaction of Y(Co1−xCux)510.1063/1.2176316 ↗
23. Cu substituted CeCo5: new optimal permanent magnetic material with reduced criticality10.1016/j.jallcom.2017.06.265 ↗
24. Rapidly solidified Sm-Co-Hf-B magnetic nano-composites: experimental and DFT studies10.1016/j.jmmm.2020.166645 ↗
25. First-principles study on surface stability and interface magnetic properties of SmFe1210.35848/1882-0786/ab7bca ↗
26. The Fe substitution in Nd2(Fe,M)14B (M = Si, Ge and Sn): a first-principles study10.1016/j.commatsci.2013.12.050 ↗
27. Microstructure characteristics and optimization of 2:17-type Sm-Co sintered magnets with different iron content10.1016/j.jmmm.2020.167288 ↗
28. Effects of temperature gradients on magnetic anisotropy of SmCo based films10.1016/j.jallcom.2021.162900 ↗
29. Coercivity temperature dependence of Sm2Co17-type sintered magnets with different cell and cell boundary microchemistry10.1016/j.jmmm.2017.12.058 ↗
30. Microstructural evolution of Sm(Co1−xCux)5 (0<x<0.5) alloys10.1016/S0925-8388(98)00871-8 ↗
31. Correlation between Fe content and z value in Sm(CobalFexCu0.06Zr0.025)z permanent magnets10.1016/j.jmmm.2018.11.008 ↗
32. The microstructure of sintered Sm(Co0.72Fe0.20Cu0.055Zr0.025)7.5 permanent magnet studied by atom probe10.1016/j.actamat.2003.10.015 ↗
33. Influence of the final heat treatment temperature on the magnetic property losses of Sm(Co,Fe,Cu,Zr)z high temperature magnets10.1016/j.jmmm.2021.167763 ↗
34. Thermal expansion and spontaneous magnetorestriction of RCo5 intermetallic compounds10.1016/0921-4526(91)90011-3 ↗
35. Magnetic moments in SmCo5 and SmCo5−xCux films10.1007/s10948-012-1530-4 ↗
36. Enhancement of anisotropy energy of SmCo5 by ceasing the coupling at 2c sites in the crystal lattice with Cu substitution10.1038/s41598-021-89331-z ↗
37. Influence of changes in electronic structure on magnetocrystalline anisotropy of YCo5 and related compounds10.1016/j.jmmm.2019.04.047 ↗
38. Effect of Cu substitution on the magnetic properties of SmCo5 film with perpendicular magnetic anisotropy10.1007/s11664-012-2119-1 ↗
39. Studies of the electronic structures, exchange coupling and magnetic moments of spin and orbital in the compound SmCo510.7498/aps.54.1814 ↗
40. Micromagnetism and the microstructure of high-temperature permanent magnets10.1063/1.1809250 ↗
41. Saturation magnetization and anisotropy fields in the Sm(Co1−xCux)5 phases10.1063/1.355423 ↗
42. Investigation of the magnetic properties and demagnetization process of an extremely high coercive Sm(Co, Cu, Fe, Zr)7.6 permanent magnet. I. Determination of intrinsic magnetic material parameters10.1002/pssa.2211080143 ↗
43. High temperature 2:17 magnets: relationship of magnetic properties to microstructure and processing10.1109/20.908808 ↗
44. Atomic structure and domain wall pinning in samarium-cobalt-based permanent magnets10.1038/s41467-017-00059-9 ↗
45. Influence mechanism of Fe content on the magnetic properties of Sm2Co17-type sintered magnets: microstructure and microchemistry10.1016/j.jallcom.2019.152908 ↗