Investigation of structural and magnetic properties of rapidly-solidified iron-silicon alloys at ambient and elevated temperatures
Source abstract
Abstract
Abstract We investigated the ambient temperature structural properties (thickness, width, microstructure, and lattice parameter), and the ambient and high temperature (up to 900 K) direct current (DC) magnetic properties—saturation magnetization (MS) and intrinsic coercivity (HCI)—of rapidly-solidified (melt-spun) Fe-x wt.% Si (x = 3, 5, & 8) alloys. The wheel surface speeds selected for the study were 30 m/s and 40 m/s. The ribbons produced at the lower wheel surface speed (30 m/s) were continuous having relatively uniform edges compared to the ribbons produced at the higher wheel surface speed. The thickness and the width of the melt-spun ribbons ranged between ∼15 and 60 μm and 500–800 μm, respectively. The x-ray diffraction spectra of the melt-spun ribbons indicated the presence of disordered α-phase, irrespective of the composition, and the wheel surface speed. The lattice parameter decreased gradually as a function of increasing silicon content from ∼0.2862 nm (Fe-3 wt.% Si) to ∼0.2847 nm (Fe-8 wt.% Si). The wheel surface speed showed an insignificant effect on MS while increased silicon content resulted in a decreasing trend in MS. Elevated temperature evaluation of the magnetization (M-T curves at ∼7.96 kA/m) in the case of Fe-3 & 5 wt.% Si alloy ribbons was distinctly different from that of the Fe-8 wt.% Si alloy ribbons. The curves of the as-prepared Fe-3 wt.% Si and Fe-5 wt.% Si alloy ribbons were irreversible while that of Fe-8 wt.% Si was reversible. The MS for any of the combinations of wheel surface speed and composition decreased monotonically with the increase in temperature (from 300 to 900 K). While HCI increased with the increase in temperature for all the wheel surface speed and composition combination, its nature of increase is distinct for Fe-8 wt.% Si alloy ribbons compared to Fe-3 & 5 wt.% Si alloys ribbons. It appears that rapidly-solidified Fe-3 wt.% Si and Fe-5 wt.% Si alloys ribbons are primarily comprised of the α-phase (disordered phase) while the Fe-8 wt.% Si alloy ribbons are comprised primarily of disordered phase along with minor constituents of an ordered phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties and Applications · Metallic Glasses and Amorphous Alloys · Magnetic properties of thin films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Bozorth · 1993 · 67
2. Advances in Fe-Si properties and their interpretation10.1016/0304-8853(95)01244-3 ↗
3. Cullity · 2009
4. Recent research progresses in grain-oriented silicon-iron10.1016/0304-8853(80)90539-9 ↗
5. A general theory of secondary recrystallization in grain oriented Fe-Si: metallurgical parameters controlling the microstructural evolution10.1016/0304-8853(94)90505-3 ↗
6. A comparison of CGO silicon steels, high-performance domain refines silicon steels and amorphous core materials in distribution transformers by total ownership cost (TOC) modeling10.1088/0031-8949/39/6/020 ↗
7. New ribbon-from metals
8. Rapidly quenched ribbon-form silicon and silicon-iron10.1143/JJAP.18.207 ↗
9. Rapidly quenched ribbon-form silicon-iron alloy with high silicon concentration10.1016/0304-8853(80)90352-2 ↗
10. Magnetic properties of 6.5% silicon iron ribbon produced by splat cooling technique10.1016/0304-8853(80)90576-4 ↗
11. Ribbon-form silicon-iron containing around 6.5 % silicon10.1109/TMAG.1980.1060560 ↗
12. Magnetic properties of rapidly solidified Fe-Si alloys10.1016/0304-8853(81)90082-2 ↗
13. Magnetic properties of rapidly solidified silicon—iron ribbons10.1016/0304-8853(84)90143-4 ↗
14. Production and properties of melt-spun Fe-6.5 wt.% Si ribbons10.1016/0025-5416(88)90295-9 ↗
15. Commercial production of Fe-6.5 wt.% Si sheet and its magnetic properties10.1063/1.342373 ↗
16. Microstructure and magnetic properties of Fe-6.5 wt.% Si alloy obtained by spray forming process10.4028/www.scientific.net/MSF.498-499.111 ↗
17. New Fe-based soft magnetic alloys composed of ultrafine grain structure10.1063/1.342149 ↗
18. Nanocrystalline soft-magnetic materials10.1016/0304-8853(95)01126-9 ↗
19. Magnetic properties and microstructure of nanocrystalline Fe-based alloys10.4028/www.scientific.net/MSF.307.51 ↗
20. Amorphous and nanocrystalline materials for applications as soft magnets10.1016/S0079-6425(99)00002-X ↗
21. The structure and mechanical properties of amorphous and nanocrystalline Fe-Si-B alloys10.1111/j.1365-2818.2006.01680.x ↗
22. Magnetic properties of Fe-Si alloys by power metallurgy10.1109/TMAG.1977.1059575 ↗
23. Microstructure and soft magnetic properties of nanocrystalline Fe-Si powders10.1016/S0925-8388(00)01234-2 ↗
24. Production and annealing of nanocrystalline Fe-Si and Fe-Si-Al alloy powders10.1016/j.msea.2003.11.046 ↗
25. Magnetic properties of high silicon iron sheet fabricated by direct powder rolling10.1016/j.jmmm.2004.04.098 ↗
26. Characterization of mechanically alloyed Fe100-xSix and Fe83.5Si13.5Nb3 nanocrystalline powders10.1016/j.jmatprotec.2007.11.064 ↗
27. Structural and magnetic properties of Fe100-xSix (0 < x < 40) nanocrystalline powders
28. Effect of annealing treatment on soft magnetic properties of Fe-6.5 wt.% Si wide ribbons10.1016/j.jmmm.2009.04.052 ↗
29. Study of order-disorder effect on magnetic properties of rapidly quenched Fe-6.5 wt.% Si alloys10.1088/0031-8949/39/2/013 ↗
30. Ordering influence on magnetic properties of rapidly quenched Fe-6.5 wt.% Si10.1016/0304-8853(90)90554-4 ↗
31. Local atomic environment parameters and magnetic properties of disordered crystalline and amorphous iron-silicon alloys10.1088/0953-8984/4/37/007 ↗
32. Magnetic properties of Si-rich Fe100-x-Six rapidly quenched alloys10.1016/S0304-8853(97)00784-1 ↗
33. Influence of atomic order on magnetic properties of Fe-Si alloys10.1016/j.jmmm.2004.11.496 ↗
34. Order in Fe-Si alloys: a neutron diffraction study10.1016/j.physb.2006.05.364 ↗
35. Fabrication of Fe-6.5 wt.%Si ribbons by melt-spinning method on large scale10.1155/2015/296197 ↗
36. Kubaschewski · 1993 · 380
37. Roy · 2015 · 39
38. Ferreira · 2012
39. Precision lattice constants from X-ray powder photographs10.1063/1.1751937 ↗
40. Errata: precision lattice constants from X-ray powder photographs10.1063/1.1752101 ↗
41. Suryanarayana · 1998 · 153
42. Cullity · 2001 · 376
43. A critical examination of the law of approach to saturation10.1002/pssa.2210660231 ↗
44. Fluid mechanics of spin casting of metals10.1146/annurev.fluid.29.1.373 ↗
45. Sundararajan · 2008 · 793
46. Effect of planar flow melt spinning parameters in ribbon formation in the soft magnetic Fe68.5Si18.5B9Nb3Cu1 alloy10.1007/s11663-011-9476-7 ↗
47. Effects of manufacturing parameters in planar flow casting process on ribbon formation and puddle evolution of Fe-Si-B alloy10.2355/isijinternational.ISIJINT-2015-349 ↗
48. Surface tension of liquid Fe-C-Si alloys10.2355/tetsutohagane1955.60.1_29 ↗
49. Viscosity of liquid Fe-C-Si alloy10.2355/tetsutohagane1955.60.1_38 ↗
50. Atomic radii in crystals10.1063/1.1725697 ↗
51. Constitution of Fe-Si alloys
52. X-ray study of Fe-Si alloys containing 0 to 15 % Si
53. X-ray study of Fe-rich Fe-Si alloys
54. Lattice parameters of Fe-Si alloy single crystals10.1002/pssa.2211060103 ↗
55. Characterization of the evaluation of the solid solubility of Si in sintered Fe-Si alloys using DSC technique10.1016/j.matchar.2006.06.003 ↗