journal article·2010-07

Crystallization behavior and dielectric properties of BaO–ZnO–SrO–CaO–Nd2O3–TiO2–B2O3–SiO2 glass–ceramics

Hsing-I Hsiang, Li-Then Mei, Chi-Shiung Hsi, Wen-Chang Liao, Fu-Su Yen

Journal of Alloys and Compounds· Volume 502· Issue 2
Publisher page

Abstract

Abstract The effects of heating rate on the crystallization and sintering behaviors of glass–ceramics (BaO–ZnO–SrO–CaO–Nd2O3–TiO2–B2O3–SiO2) were investigated in this study. The results showed that the onset of glass shrinkage occurred at around the glass transition temperature. The first crystalline phase, Nd2Ti4O11 was observed at around 775–800 °C. Fully densified glass can be obtained via glass viscous flow before the occurrence of the second crystalline phase, Nd0.66TiO3. With increasing heating rate, the glass transition temperature and crystallization temperature both shift to higher temperature. Sintering at a higher heating rate can retard the Nd0.667TiO3 crystallization of the glass, and thus improves the sintering densification via glass viscous flow during the firing process. The Ba–Zn–Sr–Ca–Nd–Ti–B–Si glass–ceramics sintered at 900 °C with a heating rate of 20 °C/min exhibited a high dielectric constant of 25 and a quality factor of about 1460, which provided a promising candidate for LTCC applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. Baker · Int. J. Appl. Ceram. Technol. · 2005 · 2 · 51410.1111/j.1744-7402.2005.02052.x ↗
2. Lin · IEEE Trans. Micro Theory Technol. · 2004 · 52 · 271810.1109/TMTT.2004.838292 ↗
3. Chang · J. Am. Ceram. Soc. · 1999 · 82 · 172510.1111/j.1151-2916.1999.tb01992.x ↗
4. Lo · J. Am. Ceram. Soc. · 2002 · 85 · 223010.1111/j.1151-2916.2002.tb00440.x ↗
5. Takada · Jpn. J. Appl. Phys. · 2005 · 44 · 662910.1143/JJAP.44.6629 ↗
6. Rangarajan · J. Am. Ceram. Soc. · 2007 · 90 · 78410.1111/j.1551-2916.2006.01470.x ↗
7. Rangarajan · J. Am. Ceram. Soc. · 2009 · 92 · 264210.1111/j.1551-2916.2009.03255.x ↗
8. Chen · J. Mater. Sci.: Mater. Electron. · 2006 · 17 · 87710.1007/s10854-006-0039-7 ↗