Solid-state synthesis of Cr2AlC MAX phase from mechanically activated Cr/Al/C powder blends
Source abstract
Abstract
This study focuses on synthesizing the ternary-layered chromium aluminum carbide phase (Cr2AlC MAX) via a milling-assisted solid-state synthesis method. The elemental powders of Cr, Al, and C were processed in a twostage process following mechanical activation (MAc) and annealing. Various parameters in both stages (such as milling time, annealing temperature, and process control agent) were examined to optimize the production of a high-purity Cr2AlC MAX phase. For this purpose, the elemental powders underwent MAc through high-energy ball milling for 1, 3, and 5 h and annealing at temperatures ranging from 700 to 1500 degrees C. The formation mechanism of the Cr2AlC phase was discussed based on detailed characterizations, including differential thermal calorimetry (DSC), X-ray diffraction (XRD), and Rietveld analyses. Additionally, the morphological properties of the synthesized powders were investigated in detail via scanning and transmission electron microscopy (SEM and TEM) techniques. The initial formation of the MAX phase was observed at 700 degrees C, and it was completed with a meager amount of chromium carbide phase at higher temperatures (99.7 % Cr2AlC at 1100 degrees C) depending on the synthesis conditions. In addition, a single-phase Cr2AlC MAX without a carbide impurity was achieved with the addition of SA, which caused an increase in the annealing temperature to 1300 degrees C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Synthesis and characterization of Cr2AlC MAX phase for photocatalytic applications10.1016/j.chemosphere.2021.131281 ↗
2. Complex optimization of arc melting synthesis for bulk Cr2AlC MAX-phase10.1016/j.ceramint.2020.11.119 ↗
3. The MAX phases: unique new carbide and nitride materials10.1511/2001.28.334 ↗
4. The MN+ 1AXN phases: a new class of solids10.1016/S0079-6786(00)00006-6 ↗
5. On the formation mechanisms and properties of MAX phases: a review10.1016/j.jeurceramsoc.2021.02.002 ↗
6. M.W. Barsoum, MAX Phases: Properties of Machinable Ternary Carbides and Nitrides, Wiley, 2013. https://doi.org/10.1002/9783527654581.10.1002/9783527654581 ↗
7. Synthesis and thermal stability of Cr2AlC10.1016/j.jeurceramsoc.2011.01.009 ↗
8. Thermal kinetics involved during the solid-state synthesis of Cr2AlC MAX phase10.1007/s10973-020-09390-8 ↗
9. Towards the synthesis of MAX-phase functional coatings by pulsed laser deposition10.1016/j.apsusc.2007.07.156 ↗
10. MAX phase carbides and nitrides: properties for future nuclear power plant in-core applications and neutron transmutation analysis10.1016/j.nucengdes.2011.12.009 ↗
11. Phase formation and microstructure evolution of plasma sprayed Cr2AlC MAX phase coatings under post annealing10.1016/j.ceramint.2022.05.288 ↗
12. High-temperature synthesis of a cast material with a maximum content of the MAX phase Cr2AlC10.1134/S0020168517030062 ↗
13. Mechanical properties of low temperature synthesized dense and fine-grained Cr2AlC ceramics10.1016/j.jeurceramsoc.2010.08.014 ↗
14. Processing of MAX phases: from synthesis to applications10.1111/jace.17544 ↗
15. Sintering of MAX-phase materials by spark plasma and other methods10.1007/s10853-020-05359-y ↗
16. Effect of sintering method on the microstructure of pure Cr2AlC MAX phase ceramics10.2109/jcersj2.15263 ↗
17. Non-isothermal oxidation kinetics of nano-laminated Cr2AlC MAX phase10.1016/j.jallcom.2018.09.326 ↗
18. Novel Cr2AlC MAX-phase/SiC fiber composites: synthesis, processing and tribological response10.1016/j.jeurceramsoc.2016.09.029 ↗
19. Synthesis of the MAX Phases by pulse discharge sintering10.1111/j.1744-7402.2010.02555.x ↗
20. Pressureless manufacturing of Cr2AlC compound and the temperature effect10.1080/10426914.2020.1819547 ↗
21. Thermodynamic assessments and mechanically activated synthesis of ultrafine Cr 2 AlC MAX phase powders10.1016/j.apt.2016.11.020 ↗
22. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
23. Thermodynamic modeling of Cr–Al–C and Ni–Al–C systems for low-density steels10.1007/s42243-020-00415-y ↗
24. Characterization and reaction mechanism of in-situ micro-laminated Cr2AlC coatings by plasma spraying Cr3C2/Al/Cr powder mixtures10.1016/j.surfcoat.2023.129271 ↗
25. Role of nano-size reinforcement and milling on the synthesis of nano-crystalline aluminium alloy composites by mechanical alloying10.1016/j.jallcom.2010.06.139 ↗
26. Effect of Fe on the sintering and thermal properties of Mo-Cu composites10.1016/j.matdes.2009.09.014 ↗
27. Synthesis of Cr2AlC from elemental powders with modified pressureless spark plasma sintering10.1007/s11595-019-2048-4 ↗
28. The reaction mechanism for the low temperature synthesis of Cr2AlC under electronic field10.1016/j.jallcom.2013.10.152 ↗
29. Al-Cr (Aluminum-Chromium)10.1007/s11669-007-9225-4 ↗
30. Phase formation sequence of Cr2AlC ceramics starting from Cr-Al-C powders10.1016/j.msea.2006.08.064 ↗
31. Synthesis of high-purity, isotropic or textured Cr2AlC bulk ceramics by spark plasma sintering of pressure-less sintered powders10.1016/j.jeurceramsoc.2014.11.008 ↗
32. Synthesis of high purity Cr 2 AlC nanolamellas with improved tribological properties for oil-based additives10.1039/C4RA06719C ↗
33. Effect of composition and processing on phase assembly and mechanical property of Cr2AlC ceramics10.1016/j.msea.2006.11.032 ↗
34. On the synthesis and properties of bulk ternary Cr2AlC ceramics
35. High temperature solution growth and characterization of Cr2AlC single crystals10.1016/j.jcrysgro.2013.09.021 ↗
36. Thermodynamic evaluation of the Al–Cr–C system10.3139/146.101270 ↗
37. Simultaneous synthesis and consolidation of chromium carbides (Cr3C2, Cr7C3 and Cr23C6) by pulsed electric-current pressure sintering10.1016/j.msea.2005.02.062 ↗
38. Phase formation during mechanically activated annealing of nanocrystalline Cr–60at%Al10.1016/j.jallcom.2010.04.046 ↗
39. Determination de la solubilite du carbone dans le chrome par mesure de la resistivite electrique a basse temperature10.1016/0001-6160(85)90208-1 ↗
40. Synthesis and characterization of Cr2AlC ceramics prepared by spark plasma sintering10.1016/j.matlet.2007.02.023 ↗