journal article·2025-04

Mechanism of microstructure evolution of DD5 single-crystal superalloy fabricated by dual-wavelength laser powder bed fusion

Linzhi Wang, Runqi Yang, Yikai Xiong, Chenyu Liao, Ting Li, Yanhong Yang, Yuan Sun, Shiyang Wang

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Alloys-by-design: application to nickel-based single crystal superalloys10.1016/j.actamat.2009.08.018 ↗
2. Metal 3D printing as a disruptive technology for superalloys10.1038/s41467-020-16188-7 ↗
3. A review of composition evolution in Ni-based single crystal superalloys10.1016/j.jmst.2020.01.026 ↗
4. Nickel-based superalloys for advanced turbine engines: chemistry, microstructure and properties10.2514/1.18239 ↗
5. Microstructural stability and mechanical properties of a new nickel-based superalloy10.1016/S0921-5093(03)00051-0 ↗
6. Creep behavior and a deformation mechanism based creep rate model under high temperature and low stress condition for single crystal superalloy DD510.1016/j.msea.2020.139414 ↗
7. Effect of misorientation on the fatigue life of nickel-base single crystal superalloy DD5 at 980° C10.1016/j.ijfatigue.2021.106479 ↗
8. Preparation and tensile properties of DD5 single crystal castings10.1007/s12613-016-1281-5 ↗
9. Mechanism of competitive grain growth in directional solidification of a nickel-base superalloy10.1016/j.actamat.2008.02.022 ↗
10. Fast simulation of temperature and phase transitions in directed energy deposition additive manufacturing
11. Temperature gradient at the nozzle outlet in material extrusion additive manufacturing with thermoplastic filament
12. AlMangour · 2019
13. Nucleation ahead of the advancing interface in directional solidification10.1016/S0921-5093(97)80081-0 ↗
14. Epitaxial laser metal forming: analysis of microstructure formation10.1016/S0921-5093(99)00202-6 ↗
15. Single-crystal laser deposition of superalloys: processing–microstructure maps10.1016/S1359-6454(00)00367-0 ↗
16. Steady state columnar and equiaxed growth of dendrites and eutectic10.1016/0025-5416(84)90201-5 ↗
17. Turbine blade tip single crystalline clad deposition with applied remelting passes for well oriented volume extension10.2351/1.4983667 ↗
18. Laser metal deposition strategies for repairing flat and notched substrates made of Ni-based single crystalline superalloys10.2351/1.5096134 ↗
19. Epitaxial laser deposition of single crystal Ni-based superalloy: variation of stray grains10.1016/j.matchar.2019.109982 ↗
20. Control of crystal orientation and continuous growth through inclination of coaxial nozzle in laser powder deposition of single-crystal superalloy10.1016/j.jmatprotec.2015.11.017 ↗
21. Effect of substrate orientation on the columnar-to-equiaxed transition in laser surface remelted single crystal superalloys10.1016/j.actamat.2015.01.063 ↗
22. Effect of substrate orientation on the formation of equiaxed stray grains in laser surface remelted single crystal superalloys: experimental investigation10.1016/j.actamat.2015.11.018 ↗
23. Variation of crystal orientation during epitaxial growth of dendrites by laser deposition10.1016/j.jmst.2017.05.002 ↗
24. Effects of substrate crystallographic orientations on microstructure in laser surface-melted single-crystal superalloy: theoretical analysis10.1007/s40195-016-0442-x ↗
25. Effects of melt-pool geometry on crystal growth and microstructure development in laser surface-melted superalloy single crystals: mathematical modeling of single-crystal growth in a melt pool (part I)
26. Effects of melt convection on stray grain formation in single crystal superalloys during directed energy deposition
27. Hot cracking behavior and mechanism of a third-generation Ni-based single-crystal superalloy during directed energy deposition
28. Microstructure and tensile properties of DD32 single crystal Ni-base superalloy repaired by laser metal forming10.1016/j.jmst.2020.01.003 ↗
29. Effects of process parameters on microstructure and cracking susceptibility of a single crystal superalloy fabricated by directed energy deposition10.1016/j.matdes.2020.109296 ↗
30. Experimental optimization of laser additive manufacturing process of single-crystal nickel-base superalloys by a statistical experiment design method10.1016/j.jallcom.2016.12.109 ↗
31. Microstructure characteristics of a René N5 Ni-based single-crystal superalloy prepared by laser-directed energy deposition
32. Effect of processing current on microstructural evolution and orientation information in Ni-based single crystal superalloy during plasma re-melting10.1016/j.jallcom.2020.158589 ↗
33. Microstructure and grain growth direction of SRR99 single-crystal superalloy by selective laser melting10.1016/j.jallcom.2019.151740 ↗
34. Effect of post-treatment on the microstructure and high-temperature oxidation behaviour of additively manufactured inconel 718 alloy10.1016/j.corsci.2019.06.030 ↗
35. Effect of laser mode and power on the tribological behavior of additively manufactured inconel 718 alloy10.1115/1.4062361 ↗
36. Oxidation performance of inconel 718 alloy fabricated by directed energy deposition10.1007/s11665-023-08785-6 ↗
37. L. Yao, L. Shang, S. Chen, L. Cao, J. LiangEffects of processing parameters on elements segregation behavior and crystallographic orientation of Ni-based superalloys in laser additive manufacturing, 2024..10.21203/rs.3.rs-4646263/v1 ↗
38. A new strategy to inhibit stray grain formation during laser directed solidification of single crystal superalloys10.1016/j.jallcom.2022.163852 ↗
39. Residual stress reduction and surface quality improvement of dual-laser powder bed fusion
40. Energy density analysis on single tracks formed by selective laser melting with CoCrMo powder material10.1007/s00170-013-4902-4 ↗
41. Quantifying equiaxed vs epitaxial solidification in laser melting of CMSX-4 single crystal superalloy10.1007/s11661-022-06929-2 ↗
42. Critical instability at moving keyhole tip generates porosity in laser melting10.1126/science.abd1587 ↗
43. Study of residual stress in selective laser melting of Ti6Al4V10.1016/j.matdes.2020.108846 ↗
44. Residual stress reduction and surface quality improvement of dual-laser powder bed fusion
45. Effect of scanning strategies on residual stress and mechanical properties of Selective Laser Melted Ti6Al4V10.1016/j.msea.2017.11.103 ↗
46. Hot cracking mechanism affecting a non-weldable Ni-based superalloy produced by selective electron Beam Melting10.1016/j.actamat.2017.09.047 ↗
47. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
48. Dendrite growth at the limit of stability: tip radius and spacing10.1016/0001-6160(81)90082-1 ↗
49. Effect of substrate preset temperature on crystal growth and microstructure formation in laser powder deposition of single-crystal superalloy10.1016/j.jmst.2018.04.016 ↗
50. Study on machining performance in grinding of Ni-base single crystal superalloy DD510.1007/s00170-022-09256-3 ↗
51. Microstructure-performance relationships in Ni-based superalloy with coprecipitation of γ’and γ”phases10.1016/j.msea.2022.143954 ↗
52. Different effects of γ′ and η phases on the physical and mechanical properties of superalloys10.1016/j.jallcom.2019.06.249 ↗
53. Repair and manufacturing of single crystal Ni-based superalloys components by laser powder deposition—a review10.2351/1.4862697 ↗
54. The high temperature tensile and creep behaviors of high entropy superalloy10.1038/s41598-017-13026-7 ↗
55. Influence of the γ′ fraction on the γ/γ′ topological inversion during high temperature creep of single crystal superalloys
56. Temperature dependence of element partitioning in rhenium and ruthenium bearing nickel-base superalloys10.1016/j.msea.2010.08.091 ↗
57. Rafting-enabled recovery avoids recrystallization in 3D-printing-repaired single-crystal superalloys10.1002/adma.201907164 ↗
58. Solution heat treatment of the single crystal nickel-base superalloy CMSX-4 fabricated by selective electron beam melting10.1002/adem.201500037 ↗
59. Custom-designed heat treatment simultaneously resolves multiple challenges facing 3D-printed single-crystal superalloys10.1016/j.matdes.2022.111075 ↗
60. Additive manufacturing of CMSX-4 Ni-base superalloy by selective laser melting: influence of processing parameters and heat treatment
61. Solute redistribution during solidification with diffusion in solid phase: a theoretical analysis10.1016/S0022-0248(98)90010-0 ↗