Abstract

The ability of Laser Powder Bed Fusion (LPBF) to manufacture complex-shaped and semi-finished components, along with the study of metallurgical properties, improves the future design and applications of LPBF-manufactured large AlSi7Mg parts. However, due to the unique microstructure of LPBF parts and the presence of a heated substrate (build platform), the precipitation sequence and mechanical properties vary along the height of the samples. This study investigates the gradient effects induced by a build platform heated to 150 °C on 300 mm-tall AlSi7Mg samples after direct and artificial aging. TEM observations revealed a gradient in precipitation hardening and dislocation densities between the bottom and top regions of as-built samples, which exhibit differences in tensile strengths but not in ductility. Direct aging at 175 °C -1 h successfully homogenized the tensile property values across the height of the billet. Newly formed precipitates balanced the strengthening reduction caused by coarsened precipitates. The artificial aging was performed after solution treatment at 505 °C, which destroyed the very fine Si-eutectic network in few minutes. Nevertheless, peak-aging at 175 °C was reached earlier in samples solution treated at 505 °C for 4 h rather than at 505 °C-0.5 h, ultimately reaching comparable hardness and tensile properties values. TEM analysis showed the distribution of Mg 2 Si precipitate and Si particles. The quality index shows that heat treatments fail to improve the quality of LPBF-manufactured AlSi7Mg compared to cast alloy under similar conditions. • Tall AlSi7Mg samples were additively manufactured on a substrate heated at 150 °C. • TEM inspections revealed sub-structures and more precipitate in bottom region. • New precipitation phenomena are induced by double aging at 175 °C. • Precipitate and secondary phases drive hardening and softening of the SHT alloy. • As-built and peak-aged alloy with networked structure shows the highest QI.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (86)

Show source-provided references
1. Thermal stability of aluminum alloys10.3390/ma13153441 ↗
2. Forced convection heat transfer in AlSi7Mg lattice structures fabricated by additive manufacturing10.1016/j.csite.2024.105006 ↗
3. Developing the additive manufacturing chain of AlSi7Mg with laser powder bed fusion and tailored heat treatments for railway spare parts10.1007/s11665-023-08912-3 ↗
4. Additive manufacturing of AlSi10Mg and Ti6Al4V lightweight alloys via laser powder bed fusion: a review of heat treatments effects10.3390/ma15062047 ↗
5. Microstructural analysis of the influences of platform preheating and post-build heat treatment on mechanical properties of laser powder bed fusion manufactured AlSi10Mg alloy10.1016/j.msea.2023.145486 ↗
6. The precipitation sequence in Al–Mg–Si alloys10.1016/S1359-6454(98)00059-7 ↗
7. Effect of heat treatment on the microstructure and anisotropy in mechanical properties of A357 alloy produced by selective laser melting10.1016/j.matdes.2018.05.026 ↗
8. Insight into the effect of different thermal treatment routes on the microstructure of AlSi7Mg produced by laser powder bed fusion10.1016/j.matchar.2021.110881 ↗
9. Crystal structure of the orthorhombic U2-Al4Mg4Si4 precipitate in the Al–Mg–Si alloy system and its relation to the β′ and β″ phases10.1016/j.msea.2004.09.019 ↗
10. Precipitation sequence of various kinds of metastable phases in Al-1.0mass% Mg2Si-0.4mass% Si alloy10.1023/A:1004769305736 ↗
11. Transmission electron microscopy study of the β′ phase (Al–Mg–Si alloys) and QC phase (Al–Cu–Mg–Si alloys): ordering mechanism and crystallographic structure10.1016/S1359-6454(00)00057-4 ↗
12. The crystal structure of the β″ phase in Al–Mg–Si alloys10.1016/S1359-6454(97)00493-X ↗
13. Influence on microstructure, strength and ductility of build platform temperature during laser powder bed fusion of AlSi10Mg10.1016/j.actamat.2020.10.001 ↗
14. In-situ residual stress reduction, martensitic decomposition and mechanical properties enhancement through high temperature powder bed pre-heating of Selective Laser Melted Ti6Al4V10.1016/j.msea.2017.04.033 ↗
15. Investigation on reducing distortion by preheating during manufacture of aluminum components using selective laser melting10.2351/1.4828755 ↗
16. Strengthening strategies for an Al alloy processed by in-situ alloying during laser powder bed fusion10.1016/j.matdes.2021.110247 ↗
17. Tuning the microstructure and mechanical properties of AlSi10Mg alloy via in-situ heat-treatments in laser powder bed fusion10.1016/j.msea.2023.145268 ↗
18. Unravelling the multi-scale structure–property relationship of laser powder bed fusion processed and heat-treated AlSi10Mg10.1038/s41598-021-85047-2 ↗
19. Effect of the distance from build platform and post-heat treatment of AlSi10Mg alloy manufactured by single- and multi-laser selective laser melting10.1007/s11665-021-05577-8 ↗
20. Production strategy for manufacturing large-scale AlSi10Mg components by laser powder bed fusion10.1007/s11837-020-04523-8 ↗
21. Change in mechanical properties of laser powder bed fused AlSi7Mg alloy during long-term exposure at warm operating temperatures10.3390/ma16247639 ↗
22. Aging profiles of AlSi7Mg0.6 and AlSi10Mg0.3 alloys manufactured via laser-powder bed fusion: direct aging versus T610.3390/ma15176126 ↗
23. The influence of processing parameters on aluminium alloy A357 manufactured by Selective Laser Melting10.1016/j.matdes.2016.07.009 ↗
24. Effect of build orientation and elevated temperature on microhardness and deformation of dynamically tested SLM processed AlSi12 alloy10.1016/j.matpr.2020.07.514 ↗
25. Effect of platform temperature and post-processing heat treatment on the fatigue life of additively manufactured AlSi7Mg alloy10.3390/met11050679 ↗
26. A comprehensive review on the effect of process parameters and post-process treatments on microstructure and mechanical properties of selective laser melting of AlSi10Mg10.1016/j.jmrt.2022.09.092 ↗
27. Effect of processing parameters on tensile properties and microstructure of selective laser melted AlSi10Mg alloy
28. A novel T6 rapid heat treatment for AlSi10Mg alloy produced by laser-based powder bed fusion: comparison with T5 and conventional T6 heat treatments10.1007/s11663-021-02365-6 ↗
29. Enhancement in mechanical properties of selectively laser-melted AlSi10Mg aluminum alloys by T6-like heat treatment10.1016/j.msea.2018.07.103 ↗
30. Effect of T6 heat treatment on the surface tribological and corrosion properties of AlSi10Mg samples produced by selective laser melting10.1016/j.matchar.2020.110769 ↗
31. Aging temperature effects on microstructure and mechanical properties for additively manufactured AlSi10Mg10.1080/02670836.2022.2164128 ↗
32. Achieving superior mechanical properties of selective laser melted AlSi10Mg via direct aging treatment10.1016/j.jmst.2021.07.059 ↗
33. Characterisation and prediction of mechanical properties in laser powder bed fusion-printed parts: a comparative analysis using machine learning10.1080/10667857.2024.2419228 ↗
34. Machine learning based fatigue life prediction with effects of additive manufacturing process parameters for printed SS 316L10.1016/j.ijfatigue.2020.105941 ↗
35. Mechanistic data-driven prediction of as-built mechanical properties in metal additive manufacturing10.1038/s41524-021-00555-z ↗
36. Machine-learning assisted laser powder bed fusion process optimization for AlSi10Mg: New microstructure description indices and fracture mechanisms10.1016/j.actamat.2020.10.010 ↗
37. Research progress and prospects of liquid–liquid triboelectric nanogenerators: mechanisms, applications, and future challenges10.1021/acsaelm.4c01729 ↗
38. Transfer learning to estimate lithium-ion battery state of health with electrochemical impedance spectroscopy10.1016/j.est.2025.115345 ↗
39. Effect of heat treatment on the microstructure and anisotropy in mechanical properties of A357 alloy produced by selective laser melting10.1016/j.matdes.2018.05.026 ↗
40. On microstructure and work hardening behavior of laser powder bed fused Al-Cu-Mg-Ag-TiB2 and AlSi10Mg alloys
41. Stress relaxation and the cellular structure-dependence of plastic deformation in additively manufactured AlSi10Mg alloys10.1016/j.ijplas.2019.12.003 ↗
42. Combined influence of traverse and rotation speeds in friction stir processing OF AlSi10Mg alloy produced by laser-powder bed fusion10.1016/j.matchemphys.2024.129585 ↗
43. Precipitation behavior of an Al7SiMg alloy processed by laser powder bed fusion during non-isothermal and isothermal heat treatments10.1016/j.mtla.2023.101751 ↗
44. Anomalous strengthening by supersaturated solid solutions of selectively laser melted Al–Si-based alloys
45. High-temperature tensile behavior of AlSi7Mg parts built by LPBF under high-productivity conditions10.1007/s40964-024-00590-4 ↗
46. Fracture toughness of AlSi10Mg alloy produced by LPBF: effects of orientation and heat treatment10.1007/s10704-024-00787-2 ↗
47. Evaluation of small-scale thin wall AlSi7Mg alloys LPBF coupons under extreme low cycle fatigue regime
48. Simultaneously enhanced strength and ductility of AlSi7Mg alloy fabricated by laser powder bed fusion with on-line static magnetic field
49. Effect of annealing twins, strain-recrystallization processing and δ-phase fraction on microtexture and evaluation of mechanical properties of nickel-based superalloy 71810.1016/j.msea.2023.145341 ↗
50. Effect of substrate plate heating on the microstructure and properties of selective laser melted Al-20Si-5Fe-3Cu-1Mg alloy10.3390/ma14020330 ↗
51. Comparative study of performance comparison of AlSi10Mg alloy prepared by selective laser melting and casting10.1016/j.jmst.2019.08.049 ↗
52. A novel method to 3D-print fine-grained AlSi10Mg alloy with isotropic properties via inoculation with LaB6 nanoparticles
53. Development of gradient microstructure in the lattice structure of AlSi10Mg alloy fabricated by selective laser melting10.1016/j.jmst.2019.06.015 ↗
54. Differences in microstructure and properties between selective laser melting and traditional manufacturing for fabrication of metal parts: a review10.1007/s11465-015-0341-2 ↗
55. Morphological development of sub-grain cellular/bands microstructures in selective laser melting10.3390/ma12081204 ↗
56. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
57. Intrinsic strain aging, Σ3 boundaries, and origins of cellular substructure in additively manufactured 316L
58. Origin of dislocation structures in an additively manufactured austenitic stainless steel 316L10.1016/j.actamat.2020.07.063 ↗
59. Evolution of the microstructure and mechanical properties of additively manufactured AlSi10Mg during room temperature holds and low temperature aging
60. Influence of Fe content on the microstructure and mechanical properties of Al-7Si-0.7Mg-2.8Fe alloy processed by laser powder bed fusion10.1016/j.msea.2024.146152 ↗
61. Assessing critical role of iron on microstructure and deformation behaviour of AlSi10Mg processed via laser powder bed fusion additive manufacturing10.1016/j.mtla.2024.102320 ↗
62. Microstructural consistency in the additive manufactured metallic materials: a study on the laser powder bed fusion of AlSi10Mg
63. Metallurgical analysis of laser powder bed-fused Al–Si–Mg alloys: main causes of premature failure10.1016/j.msea.2023.145402 ↗
64. Effect of heat treatment on SLM-fabricated TiN/AlSi10Mg composites: microstructural evolution and mechanical properties10.1016/j.jallcom.2020.156722 ↗
65. Spheroidization and coarsening of eutectic Si particles in Al-Si-based alloys10.1155/2021/6678280 ↗
66. Quantitative predictions of the trans-interface diffusion-controlled theory of particle coarsening10.1016/j.actamat.2010.04.018 ↗
67. Generalization of the Lifshitz–Slyozov–Wagner coarsening theory to non-dilute multi-component systems10.1016/j.actamat.2014.05.042 ↗
68. Influence of microstructure on fracture mechanisms of the heat-treated AlSi10Mg alloy produced by laser-based powder bed fusion10.3390/ma16052006 ↗
69. Influence of Si precipitates on fracture mechanisms of AlSi10Mg parts processed by Selective Laser Melting10.1016/j.actamat.2019.06.013 ↗
70. Considère · 1885 · 574
71. Age hardening of Al-7Si-0.5Mg alloy: role of Si size and distribution10.1016/j.jallcom.2022.167797 ↗
72. Recent development in aluminium alloys for the automotive industry10.1016/S0921-5093(99)00653-X ↗
73. On estimating high-cycle fatigue life of cast Al-Si-Mg-(Cu) alloys from tensile test results10.1016/j.msea.2017.01.106 ↗
74. Fine-tuning of mechanical properties of additively manufactured AlSi10Mg alloys by controlling the microstructural heterogeneity10.1016/j.jallcom.2023.170348 ↗
75. Revealing the strengthening contribution of stacking faults, dislocations and grain boundaries in severely deformed LPBF AlSi10Mg alloy
76. On the work-hardening behaviour of the additively manufactured Al-Si-Mg alloys: composite-like versus networked microstructure10.1016/j.mtla.2024.102282 ↗
77. Strength and strain hardening of a selective laser melted AlSi10Mg alloy10.1016/j.scriptamat.2017.07.025 ↗
78. Heat treatment of aluminium alloys produced by laser powder bed fusion: a review10.1016/j.matdes.2021.109651 ↗
79. Interpretation of tensile results by means of quality index and probable yield strength - application to AL-SI7 MG foundry alloys - France
80. Quality index charts of Al-Si-Mg semi solid alloys subjected to multiple temperatures aging treatments and different quenching media10.3390/ma12111834 ↗
81. The concept of quality index and its application for Al–Si cast alloys
82. Quality index of tensile properties on microporosity variation in A5052 aluminium alloy
83. High strength aerospace casting alloys: quality factor assessment10.1179/mst.1996.12.3.269 ↗
84. Work hardening of heat-treated AlSi10Mg alloy manufactured by selective laser melting: effects of layer thickness and hatch spacing10.3390/ma14174901 ↗
85. A357 alloy by LPBF for industry applications10.3390/ma13071488 ↗
86. Quality index for aluminum alloy castings