journal article·2024-11

Microstructure of a novel Ni-Cr-W-Mo-V containing ductile iron and decomposition behavior of its eutectic carbides at elevated temperature

Chen Liu, Yuzhou Du, Xinyu Zhu, Ziyu Wang, Xin Wang, Chao Yang, Caiyin You, Bailing Jiang

Publisher page

Abstract

A ductile iron casting containing Ni, Cr, W, Mo, and V was produced in the present study, and the decomposition of eutectic carbides at elevated temperature was systematically investigated. The as-cast sample mainly contained blocky eutectic (Fe, Cr)-rich M 3C carbides, fishbone-shaped eutectic (W, Mo)-rich M 6C carbides, and polygonal primary (V, W)-rich MC carbides. The Cr-rich M 3C carbides were completely decomposed when exposing at 1050 ℃ for 7 h, during which carbon atoms mainly aggregated to form graphite because of the existence of Si and Ni. Part of the fishbone-shaped M 6C carbides decomposed at 1050 ℃, and their morphology gradually evolved into fine rod-shape, followed by granular and nearly spherical shape with increasing holding time. The polygonal (V, W)-rich MC carbides changed little attributing to their high thermal stability.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Metal Alloys Wear and Properties · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. The origin of graphite morphology in cast iron10.1016/j.actamat.2022.117660 ↗
2. Development of as-cast dual matrix structure (DMS) ductile iron10.1016/j.msea.2012.12.033 ↗
3. Revisiting the graphite nodule in ductile iron10.1016/j.scriptamat.2018.10.018 ↗
4. Nucleation and growth of graphite particles in ductile cast iron10.1016/j.jallcom.2018.10.136 ↗
5. Wear and friction behavior of austempered ductile iron as railway wheel material10.1016/j.matdes.2015.10.037 ↗
6. Tribological behaviour of ductile and austempered grey cast iron under dry environment
7. A steel-like unalloyed multiphase ductile iron10.1016/j.jmrt.2021.10.021 ↗
8. Wear mechanisms and wear resistance of austempered ductile iron in reciprocal sliding contact10.1016/j.wear.2022.204305 ↗
9. Tribological performance of austempered and tempered ductile iron10.1007/s11663-018-1338-0 ↗
10. Rolling contact fatigue resistance of carbidic austempered ductile iron (CADI)10.1016/j.wear.2018.11.005 ↗
11. Optimization of the rolling contact fatigue (RCF) performance of carbidic austempered ductile iron (CADI)10.1016/j.triboint.2019.106076 ↗
12. Wear behavior of CADI obtained at different austenitizing temperatures
13. Microstructure refinement of hypereutectic high Cr cast irons using hard carbide-forming elements for improved wear resistance10.1016/j.wear.2013.01.079 ↗
14. Development of high toughness in austempered type ductile cast iron and evaluation of its properties10.1007/BF02652541 ↗
15. Tribological behavior of austempered ductile iron (ADI) obtained at different austempering temperatures10.1016/j.wear.2020.203396 ↗
16. The bainite transformation and the carbide precipitation of 4.88% aluminium austempered ductile iron investigated using electron microscopy10.1016/j.jallcom.2008.06.131 ↗
17. The effect of quenching and partitioning heat treatment on the wear resistance of ductile cast iron10.1007/s11665-020-04871-1 ↗
18. Abrasive wear behavior of austempered ductile iron with niobium additions
19. Impact of heat treatment on mechanical and tribological behaviour of unalloyed and alloyed ductile iron10.1016/j.jmrt.2021.07.077 ↗
20. Experimental characterization of a Si-Mo-Cr ductile cast iron10.1016/j.matdes.2014.01.002 ↗
21. Effects of nickel contents on phase constituent and mechanical properties of ductile Iron
22. Development of a Ni-Cr-Mo-V alloyed ductile iron with high hardness
23. The effect of prior cold rolling on the carbide dissolution, precipitation and dry wear behaviors of M50 bearing steel10.1016/j.triboint.2018.12.031 ↗
24. Effects of vanadium addition on microstructure, mechanical properties and wear resistance of Ni-Hard4 white cast iron10.1016/j.matdes.2013.02.043 ↗
25. Effects of molybdenum addition on the microstructure and mechanical properties of Ni-Hard white cast iron10.1007/s12666-014-0504-6 ↗
26. Influence of microstructure on degradation of cast graphitic high-speed steel10.1016/j.wear.2023.204702 ↗
27. Electron microscopy of carbides in annealed 28 wt% Cr-1 wt% (Mo/W) cast irons10.1016/j.matchar.2023.112723 ↗
28. Transformation behavior of primary MC and M2C carbides in Cr4Mo4V steel10.1016/j.jallcom.2021.161755 ↗
29. Study on fragmentation and dissolution behavior of carbide in a hot-rolled hypereutectic high chromium cast iron10.1016/j.jallcom.2014.07.131 ↗
30. Refinement of primary carbides and improvement of wear resistance of hypereutectic high chromium cast iron after modification10.1016/j.jmrt.2023.04.176 ↗
31. Microstructure and mechanical properties of a Mo alloyed high chromium cast iron after different heat treatments10.1016/j.vacuum.2018.07.013 ↗
32. Carbides in M-50 high speed steel10.1007/BF02917552 ↗
33. Effects of graphite nodule count on mechanical properties and thermal conductivity of ductile iron
34. Solidification, processing and properties of ductile cast iron10.1179/026708310X12668415533649 ↗
35. Effects of niobium alloying on microstructure, toughness and wear resistance of austempered ductile iron10.1016/j.msea.2019.05.100 ↗
36. Influence of vanadium content and cooling rate on the characteristics of vanadium-alloyed spheroidal graphite cast irons10.1016/j.jallcom.2022.168017 ↗
37. Effect of austenitizing temperature and cooling rate on Ms temperature of Fe-Ni-Cr cast iron10.1016/j.jmrt.2023.07.208 ↗
38. Formation mechanism of MC and M2C primary carbides in as-cast M50 bearing steel10.1016/j.matchar.2021.111011 ↗
39. Effect of starting microstructure upon the nucleation sites and distribution of graphite particles during a graphitising anneal of an experimental medium-carbon machining steel10.1016/j.matchar.2015.05.014 ↗
40. Cementites decomposition of a pearlitic ductile cast iron during graphitization annealing heat treatment10.1016/S1006-706X(17)30124-3 ↗
41. Developing a graphitic white iron for abrasive wear application: thermal and wear properties10.1016/j.wear.2019.202967 ↗
42. Quantitative three-dimensional characterization of pearlite spheroidization10.1016/j.actamat.2010.05.023 ↗