journal article·2024-11

Microstructural regulation, work hardening and fracture behavior of Tip reinforced Mg‐xGd‐2Y‐3Zn (x=5, 7, 9 wt%) composites

Fang-fang Cao, Kun-kun Deng, Cui-ju Wang, Kai-bo Nie, Quan-xin Shi, Wang-gang Zhang, Chao Xu, Guo-Wei Zhang

Publisher page

Abstract

In this work, Ti p/Mg‐xGd‐2Y‐3Zn (x=5, 7, 9 wt%, Ti p/GWZx23) composites were fabricated using semi-solid stirring casting and hot extrusion. The Ti p/Mg laminar-like configuration was regulated by Gd content. The effect of Ti p/Mg laminar-like configuration on the microstructure, mechanical properties, work hardening and fracture behavior of Ti p/GWZx23 composites was thoroughly studied. The results revealed that the Ti p elongated along the extrusion direction (ED) after extrusion and formed Ti p/Mg laminar-like configuration with the Mg matrix. With the increase of Gd content, the hardness of the matrix increased, which was beneficial to the elongation of Ti p. The elongation of Ti p reduced its hardness value, released the stress and promoted the DRXed grain refinement. The refined grain enhanced the ability of grain boundaries to absorb dislocations and improved the recovery effect. Furthermore, the formation of Ti p/Mg laminar-like configuration induced back stress strengthening at the Ti p/Mg interface, enhancing the work hardening rate of the Ti p/GWZx23 composites. The Ti p/Mg laminar-like configuration changed the strain distribution and the strain was transferred from the Ti p sharp corner to the elongated Ti p, which was effectively alleviates stress concentration at the Ti p/Mg interface and inhibited crack propagation.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Understanding the enhanced ductility of Mg-Gd with Ca and Zn microalloying by slip trace analysis10.1016/j.jmst.2021.02.070 ↗
2. Origins of high ductility exhibited by an extruded magnesium alloy Mg-1.8Zn-0.2Ca: experiments and crystal plasticity modeling10.1016/j.jmst.2020.12.047 ↗
3. What is going on in magnesium alloys?10.1016/j.jmst.2017.07.019 ↗
4. Microstructure and damping properties of LPSO phase dominant Mg-Ni-Y and Mg-Zn-Ni-Y alloys10.1016/j.jma.2022.06.013 ↗
5. Enhancing tensile properties of extruded AZ31 rod by introducing gradient bimodal microstructure10.1016/S1003-6326(23)66362-9 ↗
6. Effect of volume fraction of 18R-LPSO phase on corrosion resistance of Mg−Zn−Y alloys10.1016/S1003-6326(22)66119-3 ↗
7. High strength TiCp/Mg-Zn-Ca magnesium matrix nanocomposites with improved formability at low temperature10.1016/j.jallcom.2019.04.028 ↗
8. High strength SiCp/AZ91 composite assisted by dynamic precipitated Mg17Al12 phase10.1016/j.jallcom.2017.10.164 ↗
9. Microstructure and mechanical properties of SiCp/MgZnCa composites fabricated by stir casting10.1016/j.msea.2011.11.040 ↗
10. Enhanced tensile properties and wear resistance of Tip/AZ31 composites prepared by hot-press sintering10.1016/j.jmrt.2024.01.175 ↗
11. Effect of Ti particles on the LPSO phase and mechanical properties of TiP/VW94 composites10.1016/j.jmrt.2023.06.172 ↗
12. Microstructures and mechanical properties of ultrafine-grained Ti/AZ31 magnesium matrix composite prepared by powder metallurgy10.1016/j.apt.2018.09.001 ↗
13. Mechanical properties of a Mg–10 (vol%)Ti composite10.1016/S0266-3538(03)00215-X ↗
14. Investigating the microstructure-property relationship in Mg matrix composites reinforced by particles of different sizes using experiments combined with finite element simulation
15. Influence of Ti particle sizes on microstructure and mechanical behaviors of AZ91-Ti composites under different loading paths10.1016/j.msea.2023.145723 ↗
16. Work hardening and softening behavior of Mg–Zn–Ca alloy influenced by deformable Ti particles10.1016/j.msea.2021.142336 ↗
17. A novel biomimetic approach to the design of high-performance ceramic–metal composites10.1098/rsif.2009.0331 ↗
18. Delaying premature local necking of high-strength Cu: a potential way to enhance plasticity10.1016/j.scriptamat.2010.08.049 ↗
19. Enhanced toughness and fatigue strength of cold roll bonded Cu/Cu laminated composites with mechanical contrast10.1016/j.scriptamat.2011.08.001 ↗
20. Effect of tip content on the work hardening and softening behavior of Mg–Zn–Ca alloy
21. The work hardening and softening behavior of spherical Tip/Mg-5Zn-0.3Ca composite
22. Effect of Y for enhanced age hardening response and mechanical properties of Mg–Gd–Y–Zr alloys10.1016/j.msea.2006.11.096 ↗
23. Superplasticity and microstructure in Mg–Gd–Y–Zr rolled sheet10.1016/j.jallcom.2009.06.113 ↗
24. Microstructure and strengthening mechanism of high strength Mg–10Gd–2Y–0.5Zr alloy10.1016/j.jallcom.2006.03.015 ↗
25. A new insight into LPSO transformation during multi-axial forging in Mg-Gd-Y-Zn-Zr alloy10.1016/j.matlet.2020.127625 ↗
26. Formation and stabilization of 18R long-period stacking order phase through friction stir processing of Mg-Gd-Y-Zn alloy10.1007/s11661-020-05989-6 ↗
27. On the microstructure and RE-texture evolution during hot tensile deformation of Mg-Gd-Y-Zn-Zr alloy10.1016/j.jmrt.2021.11.058 ↗
28. Strain dependency of dynamic recrystallization during thermomechanical processing of Mg-Gd-Y-Zn-Zr alloy10.1016/j.jmrt.2022.02.120 ↗
29. Strain induced transformation, dynamic recrystallization and texture evolution during hot compression of an extruded Mg-Gd-Y-Zn-Zr alloy10.1016/j.msea.2020.139021 ↗
30. Unraveling the effect of deformation-induced phase transformation on microstructure and micro-texture evolution of a multi-axially forged Mg-Gd-Y-Zn-Zr alloy containing the LPSO phase10.1016/j.jmrt.2021.09.035 ↗
31. Grain refinement of aluminum alloys: Part I. the nucleant and solute paradigms—a review of the literature10.1007/s11661-999-0098-5 ↗
32. The role of solute in grain refinement of magnesium10.1007/BF02830349 ↗
33. The role of solutes in grain refinement of hypoeutectic magnesium and aluminum alloys10.1016/j.jma.2022.01.013 ↗
34. The influence of Tip aspect ratio on the microstructure, mechanical properties, and work hardening behavior of the Tip/Mg-Gd-Y-Zn composites10.1016/j.msea.2023.145981 ↗
35. Dual influences of deformation-induced W precipitates on dynamic recrystallization and fracture mechanism of the hot-extruded Mg-Y-Zn alloys: an experimental and phase field study10.1016/j.ijplas.2023.103772 ↗
36. Analyses of AM50-Tip metal-metal composite microstructure10.1016/j.jallcom.2017.10.157 ↗
37. Formation of an abnormal texture in Mg-Gd-Y-Zn-Mn alloy and its effect on mechanical properties by altering extrusion parameters10.1016/j.msea.2021.142270 ↗
38. Review on titanium and titanium based alloys as biomaterials for orthopaedic applications10.1016/j.msec.2019.04.064 ↗
39. Microstructure and mechanical behavior of Mg-5Zn matrix influenced by particle deformation zone10.1016/j.jmst.2020.04.053 ↗
40. Deformation-induced dynamic precipitation of 14H-LPSO structure and its effect on dynamic recrystallization in hot-extruded Mg-Y-Zn alloys10.1016/j.ijplas.2023.103573 ↗
41. Texture analysis in hexagonal materials10.1016/S0254-0584(03)00168-8 ↗
42. Experimental determination and theoretical prediction of twin orientations in magnesium alloy AZ3110.1016/j.scriptamat.2004.01.013 ↗
43. Effect of sheet thickness on the microstructural evolution of an Mg AZ61 alloy during large strain hot rolling10.1016/j.scriptamat.2003.11.015 ↗
44. Effect of Nd on the microstructure and mechanical properties of Mg–3Zn-0.5Zr alloy10.1016/j.msea.2021.142562 ↗
45. Behavior of Mg–15Gd–5Y–0.5Zr alloy during solution heat treatment from 500 to 540°C10.1016/j.msea.2007.01.057 ↗
46. Effects of rare-earth elements Gd and Y on the solid solution strengthening of Mg alloys10.1016/j.jallcom.2009.02.131 ↗
47. Tailoring the mechanical properties of Mg–Zn magnesium alloy by calcium addition and hot extrusion process10.1016/j.msea.2020.138929 ↗
48. Strengthening mechanisms in magnesium alloys containing ternary I, W and LPSO phases10.1016/j.jmst.2017.12.005 ↗
49. Microstructure and mechanical properties of AZ91 alloy reinforced by carbon nanotubes coated with MgO10.1016/j.carbon.2015.10.018 ↗
50. Work hardening and softening behaviors of Mg-Zn-Gd-Ca alloy regulated by bimodal microstructure10.1016/j.jallcom.2022.168606 ↗
51. Effect of B4C on strength coefficient, cold deformation and work hardening exponent characteristics of Mg composites10.1016/j.jma.2020.09.010 ↗
52. Effect of I(Mg3YZn6)-, W(Mg3Y2Zn3)- and LPSO(Mg12ZnY)-phases on tensile work-hardening and fracture behaviors of rolled Mg–Y–Zn alloys10.1016/j.jmrt.2019.04.016 ↗
53. Review on superior strength and enhanced ductility of metallic nanomaterials10.1016/j.pmatsci.2018.02.002 ↗
54. The balance between work hardening and softening behaviors of Mg-xZn-1Gd-0.2Ca-0.1Zr alloys influenced by trace Zn addition10.1016/j.jallcom.2023.172379 ↗
55. Hierarchical microstructure enables high strength and good ductility in as-cast Fe27Ni35Cr18.25Al13.75Co2Ti2Mo2 high-entropy alloy10.1016/j.jmst.2023.08.054 ↗
56. Heterostructured materials10.1016/j.pmatsci.2022.101019 ↗
57. Deformation mechanisms in a novel multiscale hetero-structured Mg alloy with high strength-ductility synergy10.1016/j.ijplas.2023.103766 ↗
58. Microstructure evolution mechanism of micron particle reinforced magnesium matrix composite at room temperature10.1016/j.matchemphys.2012.04.010 ↗
59. A fracture model for hydride-induced embrittlement10.1016/0956-7151(95)00133-G ↗
60. Modeling the fracture toughness and tensile ductility of SiCp/Al metal matrix composites10.1016/j.msea.2007.05.075 ↗
61. The influences of multiscale-sized second-phase particles on ductility of aged aluminum alloys10.1007/s11661-004-0081-0 ↗