Micro- and nano-mechanical approach to fracture toughness determination of borided layer produced on Nimonic 80A-alloy
Source abstract
Abstract
Borided layer produced on Nimonic 80A-alloy by plasma paste boriding ensure the high hardness and wear resistance. However, the high hardness and Young’s modulus of this layer contribute to its susceptibility to cracking. The fracture toughness was investigated using two approaches: micro-mechanical (crack-length-based method) and nano-mechanical (crack-energy-based method). In the case of the crack-length-based method, there was a strong correlation between the length of cracks produced from the corners of Vickers indent and the applied load. In order to characterize the susceptibility to cracking without loading, the K C0 coefficient was determined from the plot representing K C vs. indentation load. This parameter ranged from 1.5324 MPa·m 1/2 to 3.6880 MPa·m 1/2, depending on the applied model (Palmqvist, Casellas, Shetty, Niihara, Lankford and Laugier). The use of the crack-energy-based method resulted in a higher (even three times) fracture toughness compared to the crack-length-based method. It was found, that the K C values determined by Berkovich nanoindentation represents the absolute fracture toughness independent of the applied load and not related to crack formation.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Surface Treatment and Residual Stress
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Nickel-based superalloys for advanced turbine engines: chemistry, microstructure, and properties10.2514/1.18239 ↗
2. Effect of temperature on mechanical properties and type of fracture of superalloys Nimonic 80A
3. Oxidation assisted recrystallization and cracking at grain boundaries in Nimonic 80 A during elevated temperature service10.1016/j.corsci.2022.110452 ↗
4. The effects of chemical composition of Nimonic 80A-alloy on the microstructure and properties of gas-borided layer10.1016/j.surfcoat.2015.06.031 ↗
5. Growth kinetics and some mechanical properties of plasma paste borided layers produced on Nimonic 80A-alloy10.3390/ma14185146 ↗
6. The importance of plasma paste boriding parameters for thickness, nanomechanical properties, residual stress distribution and fracture toughness of layers produced on Nimonic 80A-alloy10.1016/j.engfracmech.2022.108842 ↗
7. Microstructure and property investigation of paste boronized pure nickel and Nimonic 90 superalloy10.1016/j.matchemphys.2008.11.055 ↗
8. corrosion behavior of hard boride layer produced on Nimonic 80A-alloy by gas boriding10.1007/s12666-017-1113-y ↗
9. The importance of phase composition for corrosion resistance of borided layers produced on nickel alloys10.3390/ma13225131 ↗
10. Characteristics, high temperature wear and oxidation behavior of boride layer grown on Nimonic 80A Ni-based superalloy10.1016/j.surfcoat.2021.126906 ↗
11. The importance of phase composition for corrosion resistance and thermal oxidation behavior of gas-borided layer produced on nickel alloy10.1515/corrrev-2020-0081 ↗
12. Silicon-boronising of Nimonic 90 superalloy10.1016/j.surfcoat.2005.03.030 ↗
13. Single-crystal growth and properties of CrB, Cr3B4, Cr2B3 and CrB2 from high-temperature aluminum solutions10.1016/0022-0248(95)00890-X ↗
14. Annealing effects on the structure and mechanical properties of r.f.-sputtered Cr−B hard thin films10.1016/S0040-6090(99)00741-5 ↗
15. Evaluation of halide-activated pack boriding of Inconel 72210.1007/s11661-999-0059-z ↗
16. Boriding of nickel in a fluidized bed reactor10.1016/S0025-5408(02)00672-4 ↗
17. Fracture toughness of hard ceramic phases produced on Nimonic 80A-alloy by gas boriding10.1016/j.ceramint.2015.10.119 ↗
18. Nanomechanical properties and fracture toughness of hard ceramic layer produced by gas boriding of Inconel 600 alloy10.1016/S1003-6326(20)65224-4 ↗
19. Evaluation by indentation of fracture toughness of ceramic materials10.1007/BF00544209 ↗
20. Evaluation of Kic of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗
21. An improved Vickers indentation fracture toughness model to assess the quality of thermally sprayed coatings10.1016/j.engfracmech.2014.07.015 ↗
22. Determination of fracture toughness of brittle materials by indentation10.1016/S0894-9166(15)30010-0 ↗
23. Fracture toughness evaluation using Palmqvist crack models on AISI 1045 borided steels10.1016/j.msea.2007.11.082 ↗
24. Vickers Indentation Fracture (VIF) modeling to analyze multi-cracking toughness of titania, alumina and zirconia plasma sprayed coatings10.1016/j.msea.2009.08.058 ↗
25. Fracture toughness of boride formed on low-alloy steels10.1016/S0257-8972(97)00466-0 ↗
26. Improved fracture toughness of boride coating developed with a diffusion annealing process10.1016/j.surfcoat.2013.05.050 ↗
27. The crack-initiation threshold in ceramic materials subject to elastic/plastic indentation10.1007/BF00569288 ↗
28. Fracture mechanisms of thin amorphous carbon films in nanoindentation10.1016/S1359-6454(97)00143-2 ↗
29. On the fracture toughness of bulk metallic glasses under Berkovich nanoindentation10.1016/j.jnoncrysol.2017.11.008 ↗
30. An instrumented indentation technique for estimating fracture toughness of ductile materials: a critical indentation energy model based on continuum damage mechanics10.1016/j.actamat.2005.10.033 ↗
31. The influence of chemical composition of Ni-based alloys on microstructure and mechanical properties of plasma paste borided layers10.1016/j.surfcoat.2019.03.042 ↗
32. Growth kinetics and some mechanical properties of two-phase boride layers produced on commercially pure titanium during plasma paste boriding10.1016/j.tsf.2017.02.033 ↗
33. The relationship between thin film fragmentation and buckle formation: Synchrotron-based in situ studies and two-dimensional stress analysis10.1016/j.actamat.2008.11.023 ↗
34. Size- and phase-dependent mechanical properties of ultrathin Si films on polyimide substrates10.1016/j.actamat.2016.03.028 ↗
35. Scaling relationships in conical indentation of elastic-perfectly plastic solids10.1016/S0020-7683(97)00349-1 ↗
36. A normalized damage variable for ductile metals based on toughness performance10.1016/j.msea.2010.09.076 ↗
37. A continuum damage model for composite laminates: Part I - Constitutive model10.1016/j.mechmat.2007.03.005 ↗
38. Assessment of the toughness of thin coatings using nanoindentation under displacement control10.1016/j.tsf.2005.08.176 ↗
39. Identification of the continuum damage parameter: An experimental challenge in modeling damage evolution10.1016/j.actamat.2012.03.017 ↗
40. A method to determine the toughness of brittle materials, especially hard metals
41. The work for the formation of a crack as a measure of hard metals
42. Microstructural coarsening of zirconia-toughened alumina composites10.1111/j.1551-2916.2005.00374.x ↗
43. Analysis of indentation crack as a wedge-loaded half-penny crack10.1111/j.1151-2916.1985.tb15288.x ↗
44. Indentation fracture of WC-Co cermets10.1007/BF00555296 ↗
45. Indentation microfracture in the Palmqvist crack regime: implications for fracture toughness evaluation by the indentation method10.1007/BF00721938 ↗
46. New formula for indentation toughness in ceramics10.1007/BF01729352 ↗
47. An improved technique for determining hardness and elastic 1modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
48. Review of fracture toughness (G, K, J, CTOD, CTOA) testing and standardization10.1016/j.engfracmech.2012.02.001 ↗
49. Analysis of stresses and strains near the end of a crack traversing a plate10.1115/1.4011547 ↗
50. A path independent integral and the approximate analysis of strain concentration by notches and cracks10.1115/1.3601206 ↗
51. Application of fracture mechanics at and beyond general yielding, British
52. Statistical analysis of Vickers indentation fracture toughness of Y-TZP ceramics10.21278/TOF.41201 ↗
53. Cohesive interface simulations of indentation cracking as a fracture toughness measurement method for brittle materials10.1016/j.actamat.2012.07.011 ↗
54. On the Vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗