journal article·2023-10

Effects of Sn addition on the improved hydrogen intrusion and emission behaviors in 1.5-GPa-grade Al-Si-coated hot press forming steels

Selim Kim, Alireza Zargaran, Sunghak Lee, Nack J. Kim, Sang-Heon Kim, Seok Su Sohn

Publisher page

Abstract

High-strength hot press forming (HPF) steel sheets are coated mostly by Al-Si to prevent the decarburization or oxidation of sheet surfaces, but become vulnerable to hydrogen embrittlement (HE) as H atoms supplied from moisture in a furnace penetrate through the molten coating into the steel substrate during the HPF process. In this study, 0.1-wt% of Sn was added to a 1.5-GPa-grade reference HPF steel (referred to as 0.1Sn and Ref steels), and their coating microstructures including Sn-enriched zone and Kirkendall and surface voids were examined after laboratory-scale HPF simulation tests. The content of diffusible H atoms immediately after the HPF simulation at 900 °C was 0.111 wt.ppm in the Ref sheet, decreased slowly as the elapsed time increased, and remained to be 0.030 wt.ppm even after 17 days. In the 0.1Sn sheet, it was about half of that of the Ref sheet (0.061 wt.ppm), and decreased rapidly to nil after 3 days. These results indicated that the 0.1Sn steel showed excellent H-intrusion and emission behavior, which would favorably work for better resistance to HE, by optimally controlling the multi-mechanisms of enrichment of Sn solutes and population of coating voids. The presence of Sn-enriched zone and voids played an important role in blocking the H intrusion to the substrate and in accelerating the H emission to the coating surface, respectively.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Microstructural features and mechanical properties of 22MnB5 hot stamping steel in different heat treatment conditions10.1016/j.jmrt.2020.07.043 ↗
2. Effect of plastic hot deformation on the hardness and continuous cooling transformations of 22MnB5 microalloyed boron steel10.1007/s11661-009-9790-8 ↗
3. A review on the laser welding of coated 22MnB5 press-hardened steel and its impact on the production of tailor-welded blanks10.1080/13621718.2020.1742472 ↗
4. Microstructural characteristics and mechanical properties of the Al-Si coating on press hardened 22MnB5 steel10.1016/j.jallcom.2020.156349 ↗
5. Corrosion behavior of Al-Si-Mg coated hot-press-forming steel10.1016/j.corsci.2021.109339 ↗
6. Phase transformation temperatures and Fe enrichment of a 22MnB5 Zn-Fe coated steel under hot stamping conditions10.1016/j.jmrt.2019.11.003 ↗
7. Hydrogen embrittlement of Zn-, Zn–Ni-, and Cd-coated high strength steel10.1007/s10800-013-0529-2 ↗
8. Corrosion-induced hydrogen embrittlement in aluminum alloy 202410.1016/j.corsci.2005.05.015 ↗
9. Improvement in hot dip galvanized coating microstructure and properties by pre-metallic deposition on steel surface: a comprehensive review10.1016/j.surfcoat.2022.128972 ↗
10. Effect of Zn-coating process on liquid metal embrittlement of TRIP steel10.1007/s12540-022-01214-8 ↗
11. Effect of V/Mo ratio on the evolution of carbide precipitates and hydrogen embrittlement of tempered martensitic steel10.1016/j.corsci.2020.108929 ↗
12. Effects of titanium content on hydrogen embrittlement susceptibility of hot-stamped boron steels10.1016/j.jallcom.2017.12.004 ↗
13. Effects of solid solution and grain-boundary segregation of Mo on hydrogen embrittlement in 32MnB5 hot-stamping steels10.1016/j.actamat.2021.116661 ↗
14. Alleviation of hydrogen embrittlement to delay effective hydrogen diffusion against MA constituent formation due to Mo solutes for 420 MPa grade offshore steels
15. Coating degradation in hot press forming10.2355/isijinternational.50.561 ↗
16. Oxidation enhanced and concentration dependent diffusions of dopants in silicon10.1063/1.332776 ↗
17. On the role of self-interstitials in impurity diffusion in silicon10.1063/1.327540 ↗
18. First-principles study of the self-interstitial diffusion mechanism in silicon10.1088/0953-8984/10/5/009 ↗
19. Study on hydrogen embrittlement and reversibility of hot-stamped aluminized 22MnB5 steel10.1016/j.msea.2022.143411 ↗
20. Investigation of mechanical tests for hydrogen embrittlement in automotive PHS steels10.3390/met9090934 ↗
21. The characteristics of Al-Si coating on steel 22MnB5 depending on the heat treatment10.14311/AP.2019.59.0352 ↗
22. Phase transformation and carbon profile at the interface between Al-Si coating and steel substrate in a press-hardened steel
23. Phase formation at the interface between a boron alloyed steel substrate and an Al-rich coating10.1016/j.surfcoat.2013.03.045 ↗
24. Diffusivity of Al and Fe near the diffusion bonding interface of Fe3Al with low carbon steel10.1007/BF02711175 ↗
25. Effect of Al-Si coating on weldability of press-hardened steels10.1007/s11665-020-04555-w ↗
26. Suppression of coating layer crack by diffusion heat treatment in Al-Si coated HPF steels10.1007/s12540-021-01161-w ↗
27. Hydrogen diffusivity in Fe-40 at% Al alloy10.30970/cma1.0043 ↗
28. Characterization of low-symmetry structures from phase equilibrium of Fe-Al system-microstructures and mechanical properties10.3390/ma8030914 ↗
29. A review on welding of dissimilar metals in car body manufacturing
30. 3D Fe-rich phases evolution and its effects on the fracture behavior of Al-7.0Si-1.2Fe alloys by Mn neutralization10.1007/s40195-021-01299-x ↗
31. Hydrogen trapping in alloys studied by thermal desorption spectrometry10.1016/j.jallcom.2018.03.066 ↗
32. Critical assessment of the evaluation of thermal desorption spectroscopy data for duplex stainless steels: a combined experimental and numerical approach10.1016/j.actamat.2019.12.055 ↗
33. Hydrogen trapping characteristics and mechanical degradation in a duplex stainless steel10.1007/s12540-022-01212-w ↗
34. Hydrogen solubility and diffusion in austenitic stainless steels studied with thermal desorption spectroscopy10.1002/srin.201000227 ↗
35. Hydrogen absorption and desorption behavior on aluminum-coated hot-stamped boron steel during hot press forming and automotive manufacturing processes10.3390/ma14216730 ↗
36. Effects of Al-Si coating and Zn coating on the hydrogen uptake and embrittlement of ultra-high strength press-hardened steel10.1016/j.surfcoat.2019.06.047 ↗
37. Prevention of hydrogen embrittlement in steels10.2355/isijinternational.ISIJINT-2015-430 ↗
38. Hydrogen embrittlement in different materials: a review10.1016/j.ijhydene.2018.09.201 ↗
39. Influence of Al-Si coating on microstructure and mechanical properties of fiber laser welded and then press-hardened 22MnB5 steel10.1016/j.msea.2020.139918 ↗
40. Electrochemical behaviour of 22MnB5 steel coated with hot-dip Al-Si before and after hot-stamping process investigated by means of scanning Kelvin probe microscopy10.1016/j.corsci.2020.108811 ↗
41. State-of-the-knowledge on coating systems for hot stamped parts10.1002/srin.201100292 ↗
42. An environmental effect as the major cause for room-temperature embrittlement in FeAl10.1016/0036-9748(89)90263-9 ↗
43. Thermodynamic evaluation of Fe-Sn phase diagram10.1016/S0364-5916(96)00021-1 ↗
44. Effects of Al-Si coating structures on bendability and resistance to hydrogen embrittlement in 1.5-GPa-grade hot-press-forming steel10.1016/j.actamat.2021.117561 ↗
45. Influence of microstructure constituents on the hydrogen-induced mechanical degradation in ultra-high strength sheet steels10.1007/s12540-021-00968-x ↗
46. Influence of microstructure on the mechanical properties and hydrogen embrittlement characteristics of 1800 MPa grade hot-stamped 22MnB5 steel10.1007/s10853-018-3175-6 ↗
47. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
48. Structural and magnetic properties of nanocrystalline stannic substituted cobalt ferrite10.1016/j.jmmm.2012.04.010 ↗
49. Interaction between interstitial hydrogen and substitutional solute atoms in solid solutions of niobium-base ternary alloys10.1016/0022-3697(75)90013-X ↗
50. Chemical heterogeneity enhances hydrogen resistance in high-strength steels10.1038/s41563-021-01050-y ↗