journal article·2023-02

Age hardening of Al-7Si-0.5Mg alloy: Role of Si size and distribution

Guowei Zhang, Zhaojie Wang, Changjun Xu, Hong Xu, Cong Wang

Publisher page

Abstract

The age-hardening behavior of the Al-7Si-0.5Mg alloy with different size and distribution of Si phase was investigated. The wedge-shaped mold was used to prepare specimens with different characteristics of Si. The specimen with fine and homogeneous Si showed accelerated age-hardening kinetics and higher peak hardness than the one with coarse and clustered Si due to the higher dislocation density resulted from the mismatch in the thermal contraction of Si and Al. The overlapping of the plastically-affected zone of the adjacent Si phase in the specimen with large and clustered Si led to a reduced volume fraction of the plastically-affected zone, lower dislocation density and lower age-hardening kinetics. The relationship between the radius of Si and the critical inter-particle spacing that minimize the interaction of adjacent Si to maximize the dislocation density and accelerate age-hardening kinetics was established.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Tension-compression mechanical behavior and corresponding microstructure evolution of cast A356-T6 aluminum alloy10.1016/j.msea.2021.141613 ↗
2. The effects of copper (Cu) or zinc (Zn) on fluidity of A357 alloy10.1016/j.matlet.2021.130733 ↗
3. Thermodynamic descriptions of ternary Al–Si–Sr system `orted by key experiments10.1016/j.calphad.2019.101732 ↗
4. Effects of strontium addition on the microstructure and corrosion behavior of A356 aluminum alloy10.1016/j.jallcom.2018.05.341 ↗
5. Efficient alloy design of Sr-modified A356 alloys driven by computational thermodynamics and machine learning10.1016/j.jmst.2021.09.061 ↗
6. 3D connectivity of eutectic Si as a key property defining strength of Al–Si alloys10.1016/j.commatsci.2016.04.019 ↗
7. Enhanced strength and ductility of A356 alloy due to composite effect of near-rapid solidification and thermo-mechanical treatment10.1016/j.msea.2019.03.039 ↗
8. Stress states in individual Si particles of a cast Al–Si alloy: micro-Raman analysis and microstructure based modeling10.1016/j.jallcom.2014.10.207 ↗
9. Modification mechanism and tensile property of Al-9Si-0.4Mg-0.1Cu alloy10.1016/j.matchar.2021.111693 ↗
10. Factors affecting eutectic Si modification in Al-Si hypoeutectic alloy with the addition of Na, Sr, Eu and Yb10.1016/j.matlet.2021.131206 ↗
11. Effects of duration of solution heat treatment on the evolution of 3D microstructure in AlSi7Cu3 alloy: a quantitative X-ray tomography study10.1016/j.matchar.2021.110919 ↗
12. Observation of morphology changes of fine eutectic Si phase in Al-10%Si cast alloy during heat treatment by synchrotron radiation nanotomography10.3390/ma11081308 ↗
13. Structures and formation mechanisms of dislocation-induced precipitates in relation to the age-hardening responses of Al-Mg-Si alloys10.1016/j.jmst.2019.11.001 ↗
14. Precipitation behavior and mechanical performances of A356.2 alloy treated by Al–Sr–La composite refinement-modification agent10.1016/j.jallcom.2019.153370 ↗
15. Decreased dislocation density as an origin for the quench sensitivity of the Al-Si-Mg alloys with high Si content10.1016/j.jallcom.2022.165011 ↗
16. Effect of as-cast microstructure heterogeneity on aging behavior of a high-pressure die-cast A380 alloy10.1016/j.matchar.2017.11.040 ↗
17. The effect of solution treatment and artificial aging on the work hardening characteristics of a cast Al–7%Si–0.6%Mg alloy10.1016/j.msea.2006.04.011 ↗
18. Correlation of solidification microstructure refining scale, Mg composition and heat treatment conditions with mechanical properties in Al-7Si-Mg cast aluminum alloys10.1016/j.msea.2016.12.051 ↗
19. Determination of Johnson-Cook parameters for cast aluminum alloys10.1115/1.4027793 ↗
20. Enhanced aging kinetic of Al3BC/6061 Al composites and its micro-mechanism10.1016/j.jallcom.2017.08.053 ↗
21. Effect of CNTs on precipitation hardening behavior of CNT/Al–Cu composites10.1016/j.carbon.2012.06.005 ↗
22. Study on thermal expansion of intermetallics in multicomponent Al–Si alloys by high temperature X-ray diffraction10.1016/j.intermet.2010.05.015 ↗
23. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
24. EBSD, XRD and SRS characterization of a casting Al-7wt%Si alloy processed by equal channel angular extrusion: dislocation density evaluation10.1016/j.matchar.2019.04.044 ↗
25. Measurement of dislocation density change during tensile deformation in coarse-grained aluminum by in-situ XRD technique with tester oscillation10.2320/matertrans.L-M2020861 ↗
26. Evaluation of dislocation density for 1100 aluminum with different grain size during tensile deformation by using In-situ X-ray diffraction technique10.2464/jilm.64.463 ↗
27. Characterization of nanostructures in a high pressure die cast Al-Si-Cu alloy10.1016/j.actamat.2021.117500 ↗
28. Three-dimensional characterization of ‘as-cast’ and solution-treated AlSi12(Sr) alloys by high-resolution FIB tomography10.1016/j.actamat.2007.03.004 ↗
29. Microstructure and mechanical properties of 45 vol% SiCp/7075Al composite10.1016/j.jmst.2015.01.012 ↗
30. Enhanced age-hardening behavior in Al–Cu alloys induced by in-situ synthesized TiC nanoparticles10.1016/j.jmst.2018.09.029 ↗