Abstract
Abstract Innovative methods for producing soft magnetic materials, such as inductor cores, are highly sought to achieve desirable microstructures, pursuant to excellent magnetic, mechanical and chemical properties. Here, silicone resin and nano-sized LBSCA glass (NG), prepared by a sol-gel method, were introduced to a nanocrystalline FeSiBNbCu ferromagnetic phase to produce soft magnetic composites (SMCs) by applying liquid-phase sintering-related spark plasma sintering (SPS). This novel strategy contributed to form a dense and uniform double-percolating microstructure in the SMCs with the co-doping of 1.0 wt % silicone resin (SR) and 0.6 wt % NG, which not only remarkably improved magnetic flux density (∼1.39 T), effectively permeability (∼237.0 at 1 kHz) and Vickers hardness (∼7.1 GPa), but also lowered coercivity (∼7.9 A/m) and core loss (∼120 W/m3 at 20 mT and 1 kHz, ∼2774.6 kW/m3 at 60 mT and 50 kHz). A group of additives have been designed and doped into the SMC and systematically studied to compare and understand the behaviors behind these outstanding results. The evolution of phase components and microstructure of the SMCs with different additives has been revealed and correlated with their performances.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Electromagnetic wave absorption materials · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
2. Soft magnetic materials for a sustainable and electrified world10.1126/science.aao0195 ↗
3. Soft magnetic composite materials (SMCs)10.1016/j.jmatprotec.2007.02.034 ↗
4. Interplay of domain walls and magnetization rotation on dynamic magnetization process in iron/polymer-matrix soft magnetic composites10.1016/j.jmmm.2016.11.084 ↗
5. Submicrometer laminated Fe/SiO2 soft magnetic composites-an effective route to materials for high-frequency applications10.1002/adma.200401096 ↗
6. Enhanced soft magnetic properties of Fe-based amorphous powder cores by longitude magnetic field annealing10.1016/j.jallcom.2017.02.202 ↗
7. Improved permeability of Fe based amorphous magnetic powder cores by adding permalloy10.1016/j.jmmm.2017.04.082 ↗
8. Multimillimetre-large superlattices of air-stable iron–cobalt nanoparticles10.1038/nmat1480 ↗
9. Fabrication and growth mechanism of iron oxide insulation matrix for Fe soft magnetic composites with high permeability and low core loss10.1016/j.jallcom.2017.03.229 ↗
10. Oxidation fabrication and enhanced soft magnetic properties for core-shell FeCo/CoFe2O4 micro-nano composites10.1016/j.matdes.2017.02.073 ↗
11. Structure and magnetic properties of FeSiAl-based soft magnetic composite with AlN and Al2O3 insulating layer prepared by selective nitridation and oxidation10.1016/j.jmmm.2012.03.026 ↗
12. Exfoliated BN shell-based high-frequency magnetic core-shell materials10.1039/C7NR03801A ↗
13. Correlating the microstructure, growth mechanism and magnetic properties of FeSiAl soft magnetic composites fabricated via HNO3 oxidation10.1016/j.actamat.2018.01.001 ↗
14. Interplay of crystallization, stress relaxation and magnetic properties for FeCuNbSiB soft magnetic composites10.1016/j.jallcom.2016.02.239 ↗
15. The effects of field annealing on the magnetic properties of FeSiB amorphous powder cores10.1016/j.materresbull.2017.04.030 ↗
16. Bulk nanogranular composite of magnetic metal and insulating oxide matrix10.1016/j.scriptamat.2015.10.013 ↗
17. Regulation and control of insulated layers for intergranular insulated Fe/SiO2 soft magnetic composites10.1007/s10853-017-0941-9 ↗
18. Structure and magnetic properties of ZrO2-coated Fe powders and Fe/ZrO2 soft magnetic composites10.1016/j.apt.2017.04.029 ↗
19. Investigation on sol-gel Al2O3 and hybrid phosphate-alumina insulation coatings for FeSiAl soft magnetic composites10.1007/s10853-015-9189-4 ↗
20. Low loss Sendust powder cores comprised of particles coated by sodium salt insulting layer10.1063/1.4917337 ↗
21. Mechanically strong nanocrystalline Fe-Si-B-P-Cu soft magnetic powder cores utilizing magnetic metallic glass as a binder10.1063/1.4944766 ↗
22. Synthesis and magnetic properties of core-shell structured finemet/NiZn ferrite soft nanocomposites by co-precipitation10.1016/j.jallcom.2016.08.102 ↗
23. Iron-based soft magnetic composites with Mn–Zn ferrite nanoparticles coating obtained by sol–gel method10.1016/j.jmmm.2012.06.042 ↗
24. Effect of iron particle size and volume fraction on the magnetic properties of Fe/silicate glass soft magnetic composites10.1016/j.jmmm.2014.09.019 ↗
25. SiO2 nanoparticles enhanced silicone resin as the matrix for Fe soft magnetic composites with improved magnetic, mechanical and thermal properties10.1016/j.jallcom.2017.12.322 ↗
26. Incorporation of the Fe3O4 and SiO2 nanoparticles in epoxy-modified silicone resin as the coating for soft magnetic composites with enhanced performance10.1016/j.jmmm.2017.12.005 ↗
27. Amorphous and nanocrystalline materials for applications as soft magnets10.1016/S0079-6425(99)00002-X ↗
28. Modern soft magnets: amorphous and nanocrystalline materials10.1016/j.actamat.2012.10.040 ↗
29. New Fe-based soft magnetic alloys composed of ultrafine grain structure10.1063/1.342149 ↗
30. On the formation of nanocrystals in the soft magnetic alloy Fe73.5Nb3Cu1Si13.5B910.1016/S1359-6454(97)00436-9 ↗
31. Enhanced ferromagnetic properties of low temperature sintering LiZnTi ferrites with Li2O-B2O3-SiO2-CaO-Al2O3 glass addition10.1016/j.jallcom.2014.09.138 ↗
32. Characterization and properties of new silicone-containing epoxy resin10.1016/S0032-3861(99)00790-9 ↗
33. Graphene nanoplatelets as novel additive to enhance coercivity of hot-deformed magnets by tuning microstructures10.1002/admi.201800288 ↗
34. Fe-Si/ZrO2 composites with core-shell structure and excellent magnetic properties prepared by mechanical milling and spark plasma sintering10.1016/j.jallcom.2017.05.114 ↗
35. Enhanced thermoelectric performance of solution-derived bismuth telluride based nanocomposites via liquid-phase sintering10.1016/j.nanoen.2016.10.056 ↗
36. Dense dislocation arrays embedded in grain boundaries for high-performance bulk thermoelectrics10.1126/science.aaa4166 ↗
37. Crystallization behaviour of amorphous Fe73.5Cu1Nb3Si13.5B910.1088/0953-8984/4/50/017 ↗
38. Fabrication of FINEMET bulk alloy from amorphous powders by spark plasma sintering10.1016/j.powtec.2015.11.060 ↗
39. Kinetics of the amorphous-to-nanocrystalline transformation in Fe73.5Cu1Nb3Si13.5B910.1063/1.354581 ↗
40. Synthesis and characterization of a series of smectic liquid crystalline elastomers10.1002/app.21767 ↗
41. Nafion/organically modified silicate hybrids membrane for vanadium redox flow battery10.1016/j.jpowsour.2008.12.040 ↗
42. Analysis of XPS spectra of Fe2+ and Fe3+ ions in oxide materials10.1016/j.apsusc.2007.09.063 ↗
43. Templating organic semiconductors via self-Assembly of polymer colloids10.1126/science.1081334 ↗
44. Enhanced initial permeability and dielectric constant in a double-percolating Ni0.3Zn0.7Fe1.95O4-Ni-Polymer composite10.1002/adfm.200500045 ↗
45. Magnetic assembly of transparent and conducting graphene-based functional composites10.1038/ncomms12078 ↗
46. Review: liquid phase sintering10.1007/s10853-008-3008-0 ↗
47. Effect of NiZn ferrite nanoparticles upon the structure and magnetic and gyromagnetic properties of low-temperature processed LiZnTi ferrites10.1021/jp512608z ↗
48. Evolution from amorphous to nanocrystalline and corresponding magnetic properties of Fe-Si-B-Cu-Nb alloys by melt spinning and spark plasma sintering10.1016/j.mseb.2014.04.005 ↗