journal article·2018-04

Effect of growth rate on the microstructural transition and microhardness of directionally solidified Ni–11.8 wt% Si hypereutectic alloy

Lufeng Wei, Zhilong Zhao, Zhirong Hu, Kai Cui, Jianjun Gao, Yalong Liu, Lin Liu

Publisher page

Abstract

Abstract Ni–11.8 wt% Si hypereutectic alloys were directionally solidified under growth rates of 0.5–15 μm/s. The microstructures of Ni–11.8 wt% Si alloys were characterized by field-emission scanning electron microscopy–energy dispersive spectrometry, and the phase composition was identified by X-ray diffraction. The alloys exhibited three types of microstructures: rods, wavy lamellae, and straight lamellae. The alloys grown at 4–12 μm/s exhibited a completely lamellar structure that consisted of α-Ni and β-Ni3Si phases. During lamellar–rod transition, coarse lamellae first underwent zigzag instability to form wavy lamellae and then transformed into rods. An interface deflection parameter was defined based on the deviation of the interface shape from a flat interface and reached the maximum value under maximum lamellar spacing. Moreover, zigzag instability resulted in a macroscopically flat liquid-solid interface. Out of the three microstructures, the rod-like structure exhibited the highest microhardness, followed by straight lamellae and then wavy lamellae. The difference in microhardness was related to the volume fraction of α-Ni phase and microstructural type. The lamellar microstructure more effectively improved the microhardness of eutectic materials than the rod-like microstructure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Solidification and crystal growth phenomena · Intermetallics and Advanced Alloy Properties · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Formation of l12-structured Ni3Si10.1007/BF02657315 ↗
2. Microstructure evolution and mechanical properties of intermetallic Ni–xSi (x = 5, 10, 15, 20) alloys10.1016/j.jallcom.2012.02.165 ↗
3. Microstructural, mechanical, electrical and thermal characterization of arc-melted Ni–Si and Co–Si alloys10.1016/j.jnoncrysol.2010.06.005 ↗
4. Corrosion behaviour of vacuum induction-melted Ni-based alloy in sulphuric acid10.1016/j.corsci.2010.03.026 ↗
5. High-strength, high-temperature intermetallic compounds10.1007/BF01082105 ↗
6. Emerging applications of intermetallics10.1016/S0966-9795(00)00077-7 ↗
7. A review of directionally solidified intermetallic composites for high-temperature structural applications10.1023/B:JMSC.0000031479.32138.84 ↗
8. Intermediate-temperature mechanical properties of Ni–Si alloys: oxygen embrittlement and its remedies10.1016/S0966-9795(01)00134-0 ↗
9. Reactive powder metallurgy of Ni3Si-based alloys10.1016/0966-9795(95)97291-8 ↗
10. Effects of size reduction on the structure and magnetic properties of core-shell Ni3Si/silica nanoparticles prepared by electrochemical synthesis10.1016/j.jallcom.2013.09.035 ↗
11. Electrochemical production of a magnetic Ni3Si template in lamellar Ni–Si eutectic alloy10.1149/2.0831712jes ↗
12. Low temperature embrittlement of Ni3(Si, Ti) alloys10.1016/0966-9795(95)00050-X ↗
13. Effect of the growth parameters on the Ni–Ni3Si eutectic microstructure
14. Growth and solid/solid transformation in a Ni–Si eutectic alloy10.1016/j.jallcom.2005.03.039 ↗
15. Effect of Solidification Rate on microstructure and solid/liquid interface morphology of Ni–11.5 wt% Si eutectic alloy10.1016/j.jmst.2013.09.025 ↗
16. Wetting and interfacial behavior of Ni–Si alloy on different substrates10.1007/s10853-009-3858-0 ↗
17. Wetting and bonding of Ni–Si alloys on silicon carbide10.1016/S1359-6454(98)00374-7 ↗
18. Microstructure and mechanical behavior of in situ Ni–Ni3Si composite10.1016/j.jallcom.2006.06.019 ↗
19. Microstructure and properties of Ni–Ni3Si composites by directional solidification10.1016/j.physb.2012.05.026 ↗
20. Tensile and fatigue behaviour of Ni–Ni3Si eutectic in situ composites10.1080/02670836.2015.1110883 ↗
21. Microstructural evolution during powder metallurgical processing of a Ni3Si-based intermetallic alloy10.1016/S1044-5803(96)00099-X ↗
22. Microstructures and mechanical properties of directionally solidified Ni–25%Si full lamellar in situ composites10.1016/j.msea.2016.07.064 ↗
23. The formation of full lamellar structures from Ni–25at% Si melts10.1016/j.jallcom.2016.02.144 ↗
24. Directional solidification and microstructures of near-eutectic Cr–Cr3Si alloys10.1016/S1359-6454(03)00447-6 ↗
25. Microstructure and property of directionally solidified Ni–Si hypereutectic alloy10.1007/s00339-016-9702-x ↗
26. Nucleation-controlled microstructures and anomalous eutectic formation in undercooled Co–Sn and Ni–Si eutectic melts10.1007/s11661-003-0199-5 ↗
27. Multiple micro-channels Ni3Si template fabricated by selective dissolution of Ni–Ni3Si eutectic10.1016/j.matlet.2016.10.041 ↗
28. Eutectic spacing selection in Al–Cu system10.1179/mst.1994.10.4.312 ↗
29. Microstructure development in the directionally solidified Al–4.0 wt% Cu alloy system10.1016/S1468-6996(01)00062-6 ↗
30. The microstructure parameters and microhardness of directionally solidified Sn–Ag–Cu eutectic alloy10.1016/j.jallcom.2009.06.067 ↗
31. Microstructure evolution and room temperature fracture toughness of as-cast and directionally solidified novel NiAl–Cr(Fe) alloy10.1016/j.intermet.2016.12.021 ↗
32. Dependency of microhardness on solidification processing parameters and microstructure characteristics in the directionally solidified Ti–46Al–0.5W–0.5Si alloy10.1016/j.jallcom.2010.05.095 ↗
33. Research on lamellar structure and microhardness in directionally solidified ternary Sn–40.5Pb–2.6Sb eutectic alloy10.1016/j.jallcom.2009.12.086 ↗
34. Effect of sample diameter on the primary dendrite spacing of directionally solidified Al–4wt% Cu alloy10.1016/S1003-6326(08)60220-4 ↗
35. Directional solidification of large superalloy castings with radiation and liquid-metal cooling: a comparative assessment10.1007/s11661-004-0066-z ↗
36. Microstructure and mechanical properties of NiAl-based hypereutectic alloy obtained by liquid metal cooling and zone melted liquid metal cooling directional solidification techniques10.1557/jmr.2016.61 ↗
37. Dynamic effects in the lamellar–rod eutectic transition10.1016/j.actamat.2011.01.050 ↗
38. Morphological instabilities of lamellar eutectics10.1007/BF02648952 ↗
39. Eutectic growth in three dimensions10.1007/s11661-007-9163-0 ↗
40. Stability of lamellar eutectic growth10.1016/j.actamat.2007.11.037 ↗
41. Experimental evidence for a zigzag bifurcation in bulk lamellar eutectic growth10.1103/PhysRevLett.93.175701 ↗
42. Eutectic and peritectic solidification patterns10.1016/j.cossms.2015.10.002 ↗
43. Materials microhardness “finger prints”10.1016/j.msea.2006.12.115 ↗