Hot deformation behaviour, dynamic recrystallization, and processing map development for additively manufactured AlSi9Cu3 alloy
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Metallurgy and Material Forming · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Processing of AlSi9Cu3 alloy by selective laser melting10.1080/00325899.2020.1792675 ↗
2. On the role of additive manufacturing, heat treatment and machining on the microstructural evolution and corrosion behaviour of AlSi9Cu3(Fe) alloy10.1016/j.matchar.2025.115089 ↗
3. Improving the processability and grain structures of additively manufactured Al-Fe-Cu-xZr alloy: experiment and high-fidelity simulation
4. Toughening the additively manufactured Al alloys via manipulating microstructural heterogeneity10.1016/j.jallcom.2023.169322 ↗
5. Achieving high strength in laser powder-bed fusion processed AlFeCuZr alloy via dual-nanoprecipitations and grain boundary segregation10.1016/j.jmst.2022.07.033 ↗
6. Electrochemical and passive behaviors of Ti-Fe-B alloy manufactured via casting, forging and additive manufacturing10.1016/j.matchar.2022.112530 ↗
7. Fe nanoparticles modified pure Ti alloy on microstructure evolution and fine crystallization mechanism fabricated by additive manufacturing10.1016/j.jmrt.2023.08.221 ↗
8. Enhanced mechanical properties and refined microstructure induced by micron Fe for additive manufactured Ti-Fe alloys10.1016/j.jallcom.2025.181144 ↗
9. Overcoming the strength-ductility trade-off in additively manufactured AlSi10Mg alloy by ECAP processing10.1016/j.jallcom.2022.165817 ↗
10. High temperature performance of additively manufactured Al 2024 alloy: Constitutive modelling, dynamic recrystallization evolution and kinetics10.1016/j.jmrt.2023.06.102 ↗
11. Crack-free high-strength AA-7075 fabricated by laser powder bed fusion with inoculations of metallic glass powders10.1016/j.msea.2023.145916 ↗
12. An investigation on damage tolerant design parameter of additively manufactured Al 2024: fatigue crack growth rate and fracture toughness
13. Optimization of hybrid manufacturing process combining forging and wire-arc additive manufactured Ti-6Al-4V through hot deformation characterization10.1016/j.jallcom.2021.162453 ↗
14. A study on hot-working as alternative post-processing method for titanium aluminides built by laser powder bed fusion and electron beam melting10.1016/j.jmatprotec.2020.117024 ↗
15. Severe plastic deformation as a processing tool for strengthening of additive manufactured alloys10.1016/j.jmapro.2021.05.070 ↗
16. Regression based novel constitutive analyses to predict high temperature flow behavior in super austenitic stainless steel10.1016/j.msea.2017.07.035 ↗
17. A critical review of experimental results and constitutive descriptions for metals and alloys in hot working10.1016/j.matdes.2010.11.048 ↗
18. Study on constitutive relationship of 6061 aluminum alloy based on Johnson-Cook model
19. Microstructural and constitutive relationship in process modeling of hot working: the case of a 60Mg-30Pb-9.2Al-0.8B magnesium alloy10.1016/j.jmrt.2023.09.212 ↗
20. Hot compressive deformation behaviour and constitutive equations of Mg–Pb–Al–1B–0.4Sc alloy10.1080/14786435.2021.1974113 ↗
21. A ductile fracture model considering stress state and Zener–Hollomon parameter for hot deformation of metallic materials10.1016/j.ijmecsci.2018.06.030 ↗
22. A comparative investigation on the capability of modified zerilli-armstrong and arrhenius-type constitutive models to describe flow behavior of BFe10-1-2 cupronickel alloy at elevated temperature10.1007/s11665-016-2005-8 ↗
23. Developed constitutive models, processing maps and microstructural evolution of Pb-Mg-10Al-0.5B alloy10.1016/j.matchar.2017.05.026 ↗
24. Modeling of hot deformation behavior and prediction of flow stress in a magnesium alloy using constitutive equation and artificial neural network (ANN) model10.1016/j.jma.2018.05.002 ↗
25. Flow characterization of magnesium alloy ZK61 during hot deformation with improved constitutive equations and using activation energy maps10.1016/j.ijmecsci.2020.106069 ↗
26. New hot workability prediction method under non-constant deformation conditions10.1016/j.ijmecsci.2024.109778 ↗
27. On the prediction of flow stress behavior of additively manufactured AlSi10Mg for high temperature applications
28. High temperature performance of additively manufactured Al 2024 alloy: constitutive modelling, dynamic recrystallization evolution and kinetics10.1016/j.jmrt.2023.06.102 ↗
29. Constitutive modeling, processing map establishment and microstructure analysis of spray deposited Al-Cu-Li alloy 219510.1016/j.jallcom.2018.11.289 ↗
30. Hot compression deformation behavior and microstructure evolution of Al-0.5Mg-0.4Si alloy10.1016/j.jallcom.2024.175282 ↗
31. Exploring hot deformation behavior of equimolar CoCrFeNi high-entropy alloy through constitutive equations and microstructure characterization10.1016/j.matchar.2023.113234 ↗
32. Exploring hot deformation behavior of the solutionized Cu–15Ni–8Sn alloy through constitutive equations and processing maps10.1016/j.jmrt.2024.01.225 ↗
33. Hot deformation behavior and processing maps for an Al-Mg-Si-Zr-Mn alloy
34. Singh IV, Kumar GSV. Flow stress modeling and microstructural evolution during hot compression of Al-4.8Mg-0.3Sc alloy produced by laser powder bed fusion10.1016/j.jallcom.2024.178011 ↗
35. Optimization of hot workability of an Al-Mg-Si alloy using processing maps10.1007/BF00349653 ↗
36. Constitutive equation and hot deformation behavior of homogenized Al-7.68Zn-2.12Mg-1.98Cu-0.12Zr alloy during compression at elevated temperature10.1016/j.msea.2014.04.055 ↗
37. Research on hot deformation behavior and microstructure characterization of the NiTi alloy fabricated by wire arc additive manufacturing10.1016/j.jmrt.2024.11.239 ↗
38. Effects of post-processing on the microstructural evolution and mechanical behaviour of an additively manufactured AlSi10Mg alloy10.1016/j.jmrt.2024.12.248 ↗
39. Control of microstructural characteristics and mechanical properties of AlSi12 alloy by processing conditions of laser powder bed fusion
40. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
41. Influence of working environment and built orientation on the tensile properties of selective laser melted AlSi10Mg alloy10.1016/j.msea.2019.01.103 ↗
42. Flow behaviors and microstructural evolutions of nickel-based ODS superalloys during hot deformation10.1016/j.jmst.2024.01.071 ↗
43. Additive manufacturing – A review of hot deformation behavior and constitutive modeling of flow stress10.1016/j.cossms.2022.100992 ↗
44. A physically-based constitutive model for hot deformation of Ti-10-2-3 alloy10.1016/j.jallcom.2016.11.208 ↗
45. Hot deformation behaviour of Swaged Zircaloy-4 at varying strain rate and its microstructural evolution10.1016/j.matchar.2024.113951 ↗
46. A modified Zerilli-Armstrong constitutive model to predict hot deformation behavior of 20CrMo alloy steel10.1016/j.matdes.2013.10.080 ↗
47. Dynamic recrystallization behavior and hot workability of AZ41M magnesium alloy during hot deformation10.1016/j.jallcom.2016.02.033 ↗
48. Microstructural evolution of Al-7.3Zn-2.2Mg-2Cu (Al7068) alloy in T6 condition during isothermal compression using 3-dimensional processing map10.1016/j.jallcom.2022.163690 ↗
49. Effect of thermomechanical processing on mechanical properties and the microstructure of binary Al-Ce alloy10.1016/j.msea.2024.147395 ↗
50. Hot compression behavior and dynamic recrystallization mechanisms of Ti-5Mo-5V-8Cr-3Al alloy10.1016/j.jallcom.2025.178727 ↗