Exploring the multi-scale evolution mechanism of the ultra-high-temperature mechanical behaviour of carbon/carbon composites

Lichao Song, Songhe Meng, Ying Zhang, Fan Yang, Weihua Xie

Publisher page

Abstract

The microstructure and mechanical properties of Carbon/Carbon (C/C) composites were investigated after ultra-high-temperature heat treatment (HTT) in the range of 30 – 2950 °C. The evolutionary mechanisms of the mechanical behaviour were explained at three scales: graphene sheets, carbon fibre (CF) monofilaments and the C/C composites. The results displayed that the tensile strength of CF monofilaments decreases monotonically as the HTT increases, while C/C composites present a tendency to decrease and then increase, demonstrating that CF/matrix interfacial properties play a decisive role in the tensile properties. Obvious microstructure change of C/C composites after HTT at 2700 °C was observed, meanwhile the high temperature tensile strength (measured at 2000 °C and 2500 °C) for the composites treated at temperature beyond 2600 °C was higher than that of room temperature. The high-temperature mechanical properties of C/C composites were regulated by the competing mechanisms of the graphite crystallite structure and the skin-core structure of CF monofilament, the CF/matrix interfacial strength and the porosity of C/C composites.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Fiber-reinforced polymer composites · Thermal properties of materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Effects of high-temperature annealing on the microstructures and mechanical properties of C/C-ZrC-SiC composites prepared by precursor infiltration and pyrolysis10.1016/j.matdes.2015.10.140 ↗
2. Microstructure and properties of C/C–ZrC composites prepared by hydrothermal deposition combined with carbothermal reduction10.1016/j.jallcom.2018.01.148 ↗
3. Ablation and mechanical behaviour of C/C composites under an oxyacetylene flame and tensile loading environment10.1016/j.jeurceramsoc.2024.03.051 ↗
4. Effects of high-temperature annealing on the microstructure and properties of C/SiC–ZrC composites10.1016/j.ceramint.2015.12.039 ↗
5. Preparation and characterization of three-dimensional carbon fiber reinforced zirconium carbide composite by precursor infiltration and pyrolysis process10.1016/j.ceramint.2011.02.024 ↗
6. Comparative study on tensile fracture behavior of monofilament and bundle C/C composites10.1016/j.compositesa.2005.12.015 ↗
7. Strain rate effect on mechanical properties of 3D needle-punched C/C composites at different temperatures10.1016/j.compositesb.2018.10.044 ↗
8. Strengths of C/C composites under tensile, shear, and compressive loading: role of interfacial shear strength10.1016/j.compscitech.2005.07.012 ↗
9. Effects of thermal and thermomechanical induced mechanical changes of C/C composites10.1016/j.carbon.2010.04.040 ↗
10. Microstructure and elastic properties of individual components of C/C composites10.1016/j.carbon.2009.07.057 ↗
11. The role of CNT in improving the mechanical strength retention rate of C/C composites during heat treatment10.1016/j.compositesb.2020.107856 ↗
12. Compressive experimental method and properties of C/C composites under ultra-high temperature environment10.1016/j.jeurceramsoc.2022.05.008 ↗
13. Effect of high-temperature heat treatment on the microstructure and mechanical behavior of PIP-based C/C-SiC composites with SiC filler10.1016/j.jeurceramsoc.2021.08.032 ↗
14. Improved mechanical properties and fracture mechanism of C/C composites with salt treatment monitored by synchrotron-based in-situ tensile XRD10.1016/j.compositesb.2020.108274 ↗
15. Study of microstructure evolution and mechanical behaviour changes of PAN-based carbon fibers after high-temperature heat treatment (up to 2950 °C)10.1016/j.jiec.2023.04.041 ↗
16. Mechanical properties in compression of CVI-densified porous carbon/carbon composite10.1016/S0266-3538(98)00059-1 ↗
17. Effect of pyrocarbon content in C/C preforms on microstructure and mechanical properties of the C/C–SiC composites10.1016/j.msea.2008.11.026 ↗
18. Effects of high-temperature heat treatment on the mechanical properties of unidirectional carbon fiber reinforced geopolymer composites10.1016/j.ceramint.2010.02.012 ↗
19. Effects of moisture on tensile stress rupture behavior of a SiC/SiC composite at elevated temperatures10.1016/j.compscitech.2007.03.005 ↗
20. Improved microstructure and high temperature mechanical properties of C/C–SiC composites by introduction of ZrC nanoparticles10.1016/j.ceramint.2019.12.034 ↗
21. The effect of carbon fabric treatment on delamination of 2D-C/C composites10.1016/j.compscitech.2006.03.025 ↗
22. High-temperature mechanical properties and microstructure of C/C-ZrC-SiC-ZrB composites prepared by a joint process of precursor infiltration and pyrolysis and slurry infiltration10.1016/j.jallcom.2019.151953 ↗
23. Microstructure difference between core and skin of T700 carbon fibers in heat-treated carbon/carbon composites10.1016/j.carbon.2011.02.025 ↗
24. A comparison of the effect of graphitization on microstructures and properties of polyacrylonitrile and mesophase pitch-based carbon fibers10.1016/j.carbon.2012.05.024 ↗
25. High-temperature mechanical properties of carbon and composite carbon-carbon materials10.1134/S2075113315050044 ↗
26. Stretching deformation mechanism of polyacrylonitrile-based carbon fiber structure at high temperatures10.1007/s12221-018-7988-3 ↗
27. Characterization and modeling of tensile properties of continuous fiber reinforced C/C-SiC composite at high temperatures10.1016/j.jeurceramsoc.2020.09.043 ↗
28. Influence of heat treatment on physical–chemical properties of PAN-based carbon fiber10.1016/j.ceramint.2005.02.014 ↗
29. Mechanical, surface and interfacial characterisation of pitch and PAN-based carbon fibres10.1016/S0008-6223(99)00266-3 ↗
30. Surface characteristics of fluorine-modified PAN-based carbon fibers10.1016/S0008-6223(02)00384-6 ↗
31. Mechanical, microstructure and surface characterizations of carbon fibers prepared from cellulose after liquefying and curing10.3390/ma7010075 ↗
32. Mechanical behaviour of carbon fibre reinforced TaC/SiC and ZrC/SiC composites up to 2100°C10.1016/j.jeurceramsoc.2018.11.017 ↗
33. Flexural strength and wear resistance of C/C–SiC brake materials improved by introducing SiC ceramics into carbon fiber bundles10.1016/j.ceramint.2021.05.124 ↗
34. Mechanical properties and microstructure evolution of 3D Cf/SiBCN composites at elevated temperatures10.1111/jace.15704 ↗
35. Mechanical properties of a carbon fiber reinforced self-healing multilayered matrix composite at elevated temperatures10.1016/j.msea.2011.01.009 ↗
36. Experimental study of high-temperature tensile mechanical properties of 3D needled C/C–SiC composites10.1016/j.msea.2015.12.010 ↗
37. Compressive strength of three-dimensionally reinforced carbon/carbon composite10.1016/j.carbon.2004.09.026 ↗
38. Effects of high-temperature annealing on the microstructure and properties of C/SiC–ZrB2 composites10.1016/j.matdes.2013.06.073 ↗
39. High residual mechanical properties at elevated temperatures of carbon fiber/acetylene-functional benzoxazine composite10.1016/j.compositesa.2018.05.021 ↗