Laser powder bed fusion of NbTi low-temperature superconductors
Source abstract
Abstract
This study investigates the superconducting properties of additive manufactured in-situ NbTi alloy using laser powder bed fusion. Laser parameters were optimised for a maximum microstructural density and lowest Nb segregation fraction. These characters have been achieved at the sample built with an energy density of 3.33 J/mm 2 , where it shows a density value of 6.12 g/cm 3 , undissolved Nb fraction of 0.05 %, and randomly distributed equiaxed grains with an average size of 10–20 μm. Post-processing of the as-fabricated (AF) sample was explored as a route to collapse residual porosity and dissolve residual segregated Nb particles using hot isostatic pressing (HIP) and heat treatment, respectively. HIPing resulted in a decrease of the undissolved Nb particle fraction to 0.035 %. Heat treatment at 1250 °C for 24 h, followed by aging at 400 °C for 2 h, was found to result in the complete dissolution of Nb particles and precipitation of the ɑ-Ti phase that works as pinning centres to increase the superconducting properties. The grain size increased in both post-processes to 400–500 μm. Electrical and magnetic properties were also measured for the AF, HIP and heat-treated samples. The thermal variation of electrical resistivity showed a critical temperature ( T c ) range of 9.8–9.0 K, 9.6–9.1 K and 9.9–8.8 K for the AF, HIP, and heat-treated samples, respectively, which were close to the values obtained from magnetic measurements. The critical current density ( J c ) was calculated using Bean’s model employing the magnetic hysteresis loops. The AF condition showed a negligible value of J c (5 × 10 −3 kA/mm 2 ), which improved to 0.28 kA/mm 2 and 2.65 kA/mm 2 for the HIPed, heat treated conditions, respectively (at 4.2 K, 5 T). Mechanical tensile testing was performed for the heat-treated sample to ensure both mechanical and superconducting properties would achieve the required performance, where achieves ultimate tensile strength value of 930 MPa, with 8 % elongation. • In-situ alloying approach is applicable to generate Nb 53 Ti 47 alloy using laser powder bed fusion. • Isotropic microstructure is achieved in the additive manufactured condition. • Heat treatment is essential to dissolve the segregated Nb particles. • Precipitation heat treatment provides superconductivity by generating ɑ-Ti phase.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Intermetallics and Advanced Alloy Properties · Rare-earth and actinide compounds
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. Improvements to the ITER magnets to extend the plasma operating window10.13182/FST09-A8987 ↗
2. Al-Nb (aluminum-niobium)
3. Microstructure, composition and critical current density of superconducting Nb3Sn wires10.1016/j.cryogenics.2008.05.005 ↗
4. D. Larbalestier, P. Lee, New developments in niobium titanium superconductors, in: Proceedings Particle Accelerator Conference, IEEE, 1995.
5. Superconductors in applications; some practical aspects10.1109/TASC.2009.2019287 ↗
6. Interaction of metallurgical treatment and flux pinning of NbTi superconductors10.1088/0953-2048/12/6/304 ↗
7. P.J. Lee, D.A. Superconductors, Abridged metallurgy of ductile alloy superconductors, 2013.
8. Cold work loss during heat treatment and extrusion of Nb-46.5 wt% Ti composites as measured by microhardness10.1109/77.233808 ↗
9. Development of high performance multifilamentary Nb-Ti-Ta superconductor for LHC insertion quadrupoles10.1109/77.784695 ↗
10. Investigation of the correlation between initial microstructure and critical current density of Nb-46.5 wt%Ti superconducting material10.3390/met11050777 ↗
11. A new approach to fabricate superconducting NbTi alloys10.1088/1361-6668/aa793d ↗
12. Superconducting materials: challenges and opportunities for large-scale applications10.1016/j.isci.2021.102541 ↗
13. New nanoscale artificial pinning centres for NbTi superconductors10.1016/j.matdes.2020.109285 ↗
14. A 3D printed superconducting aluminium microwave cavity10.1063/1.4958684 ↗
15. Laser powder bed fusion parameters to produce high-density Ti–53 %Nb alloy using irregularly shaped powder from hydride-dehydride (HDH) process10.1016/j.jmrt.2020.12.084 ↗
16. Advances in laser additive manufacturing of Ti-Nb alloys: from nanostructured powders to bulk objects10.3390/nano11051159 ↗
17. In situ fabrication of a titanium-niobium alloy with tailored microstructures, enhanced mechanical properties and biocompatibility by using selective laser melting
18. The effect of energy density and Nb content on the microstructure and mechanical properties of selective laser melted Ti-(10–30 wt%) Nb10.1007/s11665-021-06239-5 ↗
19. Role of laser powder bed fusion process parameters in crystallographic texture of additive manufactured Nb–48Ti alloy10.1016/j.jmrt.2021.06.054 ↗
20. Selective laser melting of Ti–35Nb composite from elemental powder mixture: microstructure, mechanical behavior and corrosion behavior10.1016/j.msea.2019.06.001 ↗
21. Low-cost and high-performance 3D printed YBCO superconductors10.1016/j.ceramint.2020.08.143 ↗
22. The use of very thin tfms in electromechanical devices10.1109/TASC.2019.2902187 ↗
23. The influence of particle shape, powder flowability, and powder layer density on part density in laser powder bed fusion10.3390/met11030418 ↗
24. Review on volumetric energy density: influence on morphology and mechanical properties of Ti6Al4V manufactured via laser powder bed fusion
25. Fabrication and superconducting properties of MgB2composite wiresby the PIT method10.1088/0953-2048/15/1/303 ↗
26. Fabricating CoCrFeMnNi high entropy alloy via selective laser melting in-situ alloying10.1016/j.jmst.2020.01.002 ↗
27. Superelastic behavior of Ti-Nb alloys obtained by the laser engineered net shaping (LENS) technique10.3390/ma13122827 ↗
28. An application of differential injection to fabricate functionally graded Ti-Nb alloys using DED-CLAD® process10.1016/j.jmatprotec.2019.01.018 ↗
29. Laser powder bed fusion (PBF-LB/M) process strategies for in-situ alloy formation with high-melting elements10.3390/met11020336 ↗
30. Shaped laser beam profiles for heat conduction welding of aluminium-copper alloys10.1016/j.optlaseng.2018.11.025 ↗
31. In-situ laser directed energy deposition of biomedical Ti-Nb and Ti-Zr-Nb alloys from elemental powders10.3390/met11081205 ↗
32. In situ synthesis of a binary Ti–10 at% Nb alloy by electron beam melting using a mixture of elemental niobium and titanium powders10.1016/j.jmatprotec.2020.116646 ↗
33. Influence of heat treatments on microstructure and mechanical properties of Ti(-)26Nb alloy elaborated in situ by laser additive manufacturing with Ti and Nb mixed powder.10.3390/ma12010061 ↗
34. Synthesis of titanium orthorhombic alloy using binder jetting additive manufacturing10.1016/j.matlet.2019.02.027 ↗
35. Systematic study of the microstructure, entropy change and adiabatic temperature change in optimized La–Fe–Si alloys10.1016/j.actamat.2011.02.033 ↗
36. Effects of recovery and recrystallization on microstructure and texture during annealing of a cold deformed superconducting Nb-50 (wt)%Ti alloy10.1016/j.jallcom.2021.161334 ↗
37. Diffusion of titanium and niobium in bcc Ti-Nb alloys10.1103/PhysRevB.19.4027 ↗
38. Bulk diffusion of niobium in single-crystal titanium dioxide10.1021/jp0678709 ↗
39. Thermal stability and latent heat of Nb–rich martensitic Ti-Nb alloys10.1016/j.jallcom.2016.12.108 ↗
40. Microstructural homogeneity and mechanical behavior of a selective laser melted Ti-35Nb alloy produced from an elemental powder mixture10.1016/j.jmst.2020.05.052 ↗
41. M. Boenisch, Structural properties, deformation behavior and thermal stability of martensitic Ti-Nb alloys, 2016.
42. Influence of cooling rate on ω phase precipitation and deformation mechanism of a novel metastable β titanium alloy10.1016/j.msea.2021.142151 ↗
43. Effects of oxygen on microstructure and mechanical properties of selective laser melted Ti–6Al–4V annealed at different temperatures10.1016/j.msea.2024.146170 ↗
44. Correlations between aging heat treatment, ω phase precipitation and mechanical properties of a cast Ti–Nb alloy10.1016/j.matdes.2010.11.012 ↗
45. Assessment of β stabilizers additions on microstructure and properties of as-cast β Ti–Nb based alloys10.1016/j.jmrt.2022.12.144 ↗
46. Influence of isothermal omega precipitation aging on deformation mechanisms and mechanical properties of a β-type Ti-Nb alloy10.1016/j.jallcom.2022.167309 ↗
47. Deformation behavior and fracture mechanism of laminated Ti/Ti-50 Nb alloy with diffusion layer10.1016/j.jallcom.2022.167754 ↗
48. Novel low modulus beta-type Ti–Nb alloys by gallium and copper minor additions for antibacterial implant applications10.1016/j.jmrt.2022.08.111 ↗
49. Effect of laser scanning speeds on microstructure, tribological and corrosion behavior of Ti-23Nb alloys produced by laser metal deposition10.1016/j.matchar.2023.112647 ↗
50. Microstructure and elastic deformation behavior of β-type Ti-29Nb-13Ta-4.6Zr with promising mechanical properties for stent applications10.1016/j.jmrt.2019.06.047 ↗
51. F. Lacy, Electrical Resistance of Superconductors, 2019.
52. Development of superconducting coaxial cables for cryogenic detectors
53. Simple method to measure the thermal conductivity of technical superconductors, e.g., NbTi10.1063/1.1135850 ↗
54. Anomalous phonon thermal resistivity in superconducting Ti55Nb45 alloys10.1016/0038-1098(77)90106-5 ↗
55. Speller · 2022
56. Evolution of morphological, crystal structure, and electrical properties of Ba-Pb-Bi-O superconducting materials
57. Niobium-titanium (Nb-Ti) superconducting joints for persistent-mode operation10.1038/s41598-019-50549-7 ↗
58. Fishtail shape in the magnetic hysteresis loop for superconductors: interplay between different pinning mechanisms10.1103/PhysRevB.55.3276 ↗
59. Oxygen-defect flux pinning, anomalous magnetization and intra-grain granularity in YBa2Cu307–δ10.1038/346332a0 ↗
60. Theory of collective flux creep10.1103/PhysRevLett.63.2303 ↗
61. ``Phase diagram'' of the vortex-solid phase in Y-Ba-Cu-O crystals: a crossover from single-vortex (1D) to collective (3D) pinning regimes10.1103/PhysRevLett.69.2280 ↗
62. Plastic vortex creep in YBa2Cu3O7-x crystals10.1103/PhysRevLett.77.1596 ↗
63. A possible mechanism for the peak effect in type II superconductors10.1080/14786436908217779 ↗
64. Nonlinear electrodynamics of randomly inhomogeneous superconductors10.1103/PhysRevLett.83.3037 ↗
65. Vortices in high-temperature superconductors10.1103/RevModPhys.66.1125 ↗