Source abstract
Abstract
A new Ti64-Fe-Co alloy was studied via a laser-material-deposition method. Associated with high growth restriction factors, β-eutectoid (Fe, Co) alloying minimizes anisotropy (due to the prior columnar β-grain growth) in the laseradditive -manufacturing (AM) built Ti-parts along with enhanced properties. Fe alloying for Ti64 via laser-AM results in superior strengthening with reduced ductility, where a good combination of strength and elongation properties can be achieved for a Ti-Fe-Co system. However, studies on Ti-Fe-Co-based systems via laser processing are limited. Co possesses a similar electronic property as Fe and the Ti-Fe system accompanies further solute addition. The effect of Co alloying the Ti64-Fe system was investigated in this study via a pre-placed laser-material-deposition method. A Ti64–5Fe-5Co alloy was formulated referring to CALPHAD simulations, along with a Ti64–10Fe composition. The new Ti-alloys were fabricated via both the laser-material-deposition and conventional vacuum arc melting routes, and the characteristics of the fabricated samples were examined. XRD analysis shows the evolution of the β-Ti phase with Fe and Co alloying, which agrees with the thermodynamic phase simulation results. The corresponding SEM micrographs depicted a β-phase dominant matrix with α-dendrites, and the solidification path was discussed. Considerable grain refinement was obtained for the laser-deposited alloys compared to the arc-melted ones, with an improved hardness value twice that of the commercial Ti64. A reduced stiffness for the laser-deposited Ti64–5Fe-5Co was observed from the load-vs-displacement characteristics, indicating matrix softening with Co alloying, which might benefit the elongation properties. The studied Ti-alloy shows a 30 % improvement in the dry-sliding wear characteristic with reduced fretting and abrasion compared to the commercial Ti64. The studied Ti-alloys were located in the theoretical d-electron space and new (Bo) ̅-(Md) ̅ vectors were introduced. Further studies on this would help in extending the applicability of laser-AM-built Ti-components.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (78)
Show source-provided references
1. C. Veiga, J.P. Davim, A.J.R. Loureiro, PROPERTIES AND APPLICATIONS OF TITANIUM ALLOYS: A BRIEF REVIEW, n.d. 〈https://www.researchgate.net/publication/283863116〉.
2. Excellent dynamic mechanical properties of a newly developed titanium alloy with bimodal structure10.1016/j.jallcom.2023.170980 ↗
3. Titanium alloy production technology, market prospects and industry development10.1016/j.matdes.2010.09.011 ↗
4. A critical review of microstructure and mechanical properties of laser welded similar and dissimilar titanium alloy joints
5. Advances in investment casting of Ti–6Al–4V alloy: a review10.1179/136404605225023225 ↗
6. Gibson · 2015
7. The rise of 3-D printing: The advantages of additive manufacturing over traditional manufacturing10.1016/j.bushor.2017.05.011 ↗
8. The Additive Manufacturing (AM) of titanium alloys10.1016/j.mprp.2016.12.062 ↗
9. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
10. Additive manufacturing of titanium alloy for aircraft components10.1016/j.procir.2015.08.061 ↗
11. Fatigue of Ti6Al4V structural health monitoring systems produced by selective laser melting10.3390/ma9020106 ↗
12. Fabrication of large Ti–6Al–4V structures by direct laser deposition10.1016/j.jallcom.2014.12.234 ↗
13. Material properties of Ti6Al4V parts produced by laser metal deposition10.1016/j.phpro.2012.10.056 ↗
14. G. Welsch, R. Boyer, E. W. (Eds.), Materials properties handbook: titanium alloys., ASM International, 1993.
15. Martensite formation and decomposition during traditional and AM processing of two-phase titanium alloys—an overview10.3390/met11030481 ↗
16. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
17. Review of mechanical properties of Ti-6Al-4V made by laser-based additive manufacturing using powder feedstock10.1007/s11837-015-1759-z ↗
18. A review of metastable beta titanium alloys10.3390/met8070506 ↗
19. On the design of new β-metastable titanium alloys with improved work hardening rate thanks to simultaneous TRIP and TWIP effects10.1016/j.scriptamat.2012.01.049 ↗
20. A β-titanium alloy with extra high strain-hardening rate: Design and mechanical properties10.1016/j.scriptamat.2015.11.020 ↗
21. State of the art in beta titanium alloys for airframe applications10.1007/s11837-015-1442-4 ↗
22. Precipitation reactions in age-hardenable alloys during laser additive manufacturing10.1007/s11837-015-1764-2 ↗
23. Microstructural heterogeneity and anisotropy control of additive manufactured Ti-6Al-4V alloy for aircraft components10.1007/s11837-023-05756-z ↗
24. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
25. Anisotropic properties of directed energy deposition (DED)-processed Ti–6Al–4V10.1016/j.jmapro.2016.06.020 ↗
26. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
27. Microstructural control during direct laser deposition of a β-titanium alloy10.1016/j.matdes.2015.05.031 ↗
28. Microstructural evolution during post-heat treatment and its effect on the mechanical properties of directed energy deposited near β titanium alloy10.1016/j.jallcom.2022.168001 ↗
29. A study of microstructural factors governing strength and ductility of titanium alloys fabricated by powder bed fusion additive manufacturing10.1016/j.jallcom.2023.170094 ↗
30. Use of alloying to effect an equiaxed microstructure in additive manufacturing and subsequent heat treatment of high-strength titanium alloys10.1007/s11661-021-06475-3 ↗
31. Beryllium as a grain refiner in titanium alloys10.1016/j.jallcom.2009.03.016 ↗
32. Microstructures and grain refinement of additive-manufactured Ti-xW alloys10.1007/s11661-017-4117-7 ↗
33. The contribution of constitutional supercooling to nucleation and grain formation10.1007/s11661-015-2960-y ↗
34. The influence of iron in minimizing the microstructural anisotropy of Ti-6Al-4V produced by laser powder-bed fusion10.1007/s11661-020-05692-6 ↗
35. Effects of Cr and Fe addition on microstructure and tensile properties of Ti–6Al–4V prepared by direct energy deposition10.1007/s12540-018-0148-x ↗
36. Microstructural response of β-stabilized Ti–6Al–4V manufactured by direct energy deposition10.1016/j.jallcom.2019.152021 ↗
37. Microstructural engineering of a dual-phase Ti-Al-V-Fe alloy via in situ alloying during laser powder bed fusion
38. A review on alloy design, biological response, and strengthening of β-titanium alloys as biomaterials10.1016/j.msec.2020.111661 ↗
39. Beta titanium alloys processed by laser powder bed fusion: a review10.1007/s11665-021-05800-6 ↗
40. Effect of Fe content on microstructures and properties of Ti6Al4V alloy with combinatorial approach10.1016/S1003-6326(18)64815-0 ↗
41. Effect of cooling process on the α phase formation and mechanical properties of sintered Ti–Fe alloys10.1016/j.msea.2011.02.092 ↗
42. High-strength binary Ti–Fe bulk alloys with enhanced ductility10.1557/JMR.2004.0462 ↗
43. Investigation of Ti–Fe–Co bulk alloys with high strength and enhanced ductility10.1016/j.actamat.2005.01.012 ↗
44. Deformation behavior of high strength metastable hypereutectic Ti–Fe–Co alloys10.1016/j.intermet.2006.05.006 ↗
45. Microstructural evolution in novel suction cast multicomponent Ti-Fe-Co alloys10.1007/s11661-014-2675-5 ↗
46. Phase evolution and mechanical properties of suction cast Ti–Fe–Co ternary alloys10.1007/s12666-017-1174-y ↗
47. Direct laser cladding of Co on Ti–6Al–4V with a compositionally graded interface10.1016/j.jmatprotec.2008.05.017 ↗
48. Friction and wear properties of titanium10.1016/0043-1648(58)90428-9 ↗
49. Dry sliding wear behaviour of titanium (Grade 5) alloy by using response surface methodology10.1155/2013/272106 ↗
50. Functionally graded Co–Cr–Mo coating on Ti–6Al–4V alloy structures10.1016/j.actbio.2007.10.005 ↗
51. Additive manufacturing of titanium-base alloys with equiaxed microstructures using powder blends
52. Development of an additively manufactured metastable beta titanium alloy with a fully equiaxed grain structure and ultrahigh yield strength
53. In situ absorption synchrotron measurements, predictive modeling, microstructural analysis, and scanning probe measurements of laser melted Ti-6Al-4V single tracks for additive manufacturing applications10.1016/j.jallcom.2021.163494 ↗
54. Investigation of IR pyrometer-captured thermal signatures and their role on microstructural evolution and properties of Inconel 625 tracks in DED-based additive manufacturing10.1016/j.surfcoat.2022.128818 ↗
55. Achieving grain refinement and ultrahigh yield strength in laser aided additive manufacturing of Ti−6Al−4V alloy by trace Ni addition10.1080/17452759.2021.1949091 ↗
56. A Scheil–Gulliver model dedicated to the solidification of steel10.1016/j.calphad.2015.01.002 ↗
57. Experimental validation of Scheil–Gulliver simulations for gradient path planning in additively manufactured functionally graded materials
58. Mechanisms of Ti3 Al precipitation in hcp α-Ti10.1016/j.actamat.2021.116811 ↗
59. Beta Titanium Alloys and Their Role in the Titanium Industry10.1007/BF03220742 ↗
60. Electronic Structure and Magnetic Properties of the TiFexCo1-X System
61. Decomposition of the α-phase in titanium-rich Ti-Al alloys10.1007/BF02644528 ↗
62. An investigation of the ordered DO19 phase formation in the Ti-Al system10.1007/BF01106520 ↗
63. Formation of Widmanstätten Alpha Structure in a Ti–6Al–4V Alloy10.2320/matertrans1989.35.238 ↗
64. High-temperature oxidation of titanium10.1016/0022-5088(67)90017-3 ↗
65. Phase modulation of Ti3O/R-TiO2 nanocomposites for the self-powered photoelectrochemical sensing of tetracycline10.1021/acsanm.3c04849 ↗
66. Direct reduction of synthetic rutile using the FFC process to produce low-cost novel titanium alloys10.1007/s10853-015-9718-1 ↗
67. G.R.B. and E.W.C. Welsch, Materials properties handbook: titanium alloys, ASM international, 1993.
68. Chemical reactions at surfaces: titanium oxidation10.1016/S0257-8972(99)00420-X ↗
69. Titanium and Titanium Alloy Castings
70. A review on wear-resistant coating with high hardness and high toughness on the surface of titanium alloy10.1016/j.jallcom.2021.160645 ↗
71. Dry sliding wear behavior of laser clad TiVCrAlSi high entropy alloy coatings on Ti–6Al–4V substrate10.1016/j.matdes.2012.04.049 ↗
72. A review on wear-resistant coating with high hardness and high toughness on the surface of titanium alloy10.1016/j.jallcom.2021.160645 ↗
73. General approach to phase stability and elastic properties of β-type Ti-alloys using electronic parameters10.1016/j.scriptamat.2006.04.022 ↗
74. Design of a new multi-element beta titanium alloy based on d-electron method10.1007/978-3-319-72526-0_36 ↗
75. Molecular orbital approach to alloy design10.1007/978-0-387-34565-9_8 ↗
76. The molecular orbital approach to titanium alloy design
77. D. Kuroda, M. Niinomi, M. Morinaga, Y. Kato, T. Yashiro, Design and mechanical properties of new i type titanium alloys for implant materials, 1998.10.1016/S0921-5093(97)00808-3 ↗
78. Design and tensile properties of a bcc Ti-rich high-entropy alloy with transformation-induced plasticity10.1080/21663831.2016.1221861 ↗