Deformation and fracture behaviors of Ti6Al4V alloy fabricated by laser powder bed fusion under combined tension and shear loading
Source abstract
Abstract
The present work aims to study the deformation and failure behavior of laser powder bed fusion (LPBF) manufactured Ti6Al4V alloy. Uniaxial tension, pure shear, combined tension and shear specimens in horizontally, inclined and vertically (0°, 45° and 90°) building directions have been tested and observed by digital image correlation (DIC) technique. Significant anisotropy in ultimate strength, strain hardening and maximum elongation were observed. The failure mechanisms of 0°, 45° and 90° built LPBF Ti6Al4V alloy under different stress states are revealed by fractographical analyses. As the stress triaxiality increases from 0 to 0.33, distortion and shearing of micro voids induce the failure of shear specimen whilst void nucleation, growth and coalescence is the dominant failure mechanism of LPBF Ti6Al4V alloy under tension. The inherent defects significantly affect shear and tensile performance, large interlaminar shear deformation appears in horizontally built shear specimen, the tensile loading is prone to open the defects of vertically built uniaxial tensile sample due to the building direction. It can help to better understand the failure mechanism and improve the quality of LPBF Ti6Al4V in practical applications.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Review on titanium and titanium based alloys as biomaterials for orthopaedic applications10.1016/j.msec.2019.04.064 ↗
2. A constitutive model for a rate and temperature-dependent, plastically anisotropic titanium alloy10.1016/j.ijplas.2020.102777 ↗
3. A quantitative analysis of the transition of fracture mechanisms of Ti6Al4V over a wide range of stress triaxiality and strain rate10.1016/j.engfracmech.2020.107020 ↗
4. Microstructure evolution during hot-packed rolling and mechanical properties anisotropy of as-rolled network-structured TiBw/TA15 composites10.1016/j.msea.2022.143518 ↗
5. Data-driven fatigue life prediction in additive manufactured titanium alloy: a damage mechanics based machine learning framework10.1016/j.engfracmech.2021.107850 ↗
6. Fracture and fatigue in additively manufactured metals10.1016/j.actamat.2021.117240 ↗
7. Additive manufactuing of structural materials10.1016/j.mser.2020.100596 ↗
8. Processing parameters in laser powder bed fusion metal additive manufacturing10.1016/j.matdes.2020.108762 ↗
9. Design of titanium alloys by additive manufacturing: a critical review
10. Microstructural evolution and cryogenic and ambient temperature deformation behavior of the near-α titanium alloy TA15 fabricated by laser powder bed fusion10.1016/j.jallcom.2024.175075 ↗
11. Fatigue of laser powder-bed fusion additive manufactured Ti-6Al-4V in presence of process-induced porosity defects10.1016/j.engfracmech.2021.108140 ↗
12. Defects-dictated tensile properties of selective laser melted Ti-6Al-4V10.1016/j.matdes.2018.08.004 ↗
13. Alloys-by-design: a low-modulus titanium alloy for additively manufactured biomedical implants10.1016/j.actamat.2022.117749 ↗
14. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti-6Al-4V10.1016/j.msea.2014.07.086 ↗
15. The influence of building direction on the fatigue crack propagation behavior of Ti6Al4V alloy produced by selective laser melting10.1016/j.msea.2019.138409 ↗
16. Sample building orientation effect on porosity and mechanical properties in Selective Laser Melting of Ti6Al4V titanium alloy10.1016/j.msea.2021.142306 ↗
17. Interrupted fatigue testing with periodic tomography to monitor porosity defects in wire + arc additive manufactured Ti-6Al-4V
18. Study of pore defect and mechanical properties in selective laser melted Ti6Al4V alloy based on X-ray computed tomography10.1016/j.msea.2020.139981 ↗
19. An experimental and numerical study for the damage characterization of a Ti-6AL-4V titanium alloy10.1016/j.ijmecsci.2015.01.005 ↗
20. Influence of stress triaxiality on the failure behavior of Ti-6Al-4V alloy under a broad range of strain rates10.1016/j.tafmec.2018.07.008 ↗
21. Mechanical characterization of the AlSi9Cu3 cast alloy under distinct stress states and thermal conditions10.1016/j.engfracmech.2019.106499 ↗
22. Fracture of an anisotropic rare-earth-containing magnesium alloy (ZEK100) at different stress states and strain rates: experiments and modeling10.1016/j.ijplas.2019.07.011 ↗
23. Experiments on stress-triaxiality dependence of material behavior of aluminum alloys10.1016/j.mechmat.2009.11.012 ↗
24. Optimized butterfly specimen for the fracture testing of sheet materials under combined normal and shear loading10.1016/j.engfracmech.2011.08.008 ↗
25. Compact forced simple-shear sample for studying shear localization in materials10.1016/j.actamat.2015.09.051 ↗
26. Novel technique for static and dynamic shear testing of Ti6Al4V sheet10.1007/s11340-011-9541-9 ↗
27. Failure behavior of laser metal deposited additive manufacturing Ti-6Al-4V: effects of stress state and initial defects10.1089/3dp.2021.0101 ↗
28. A grooved in-plane torsion test for the investigation of shear fracture in sheet materials10.1016/j.ijsolstr.2015.03.032 ↗
29. Calibration of ductile fracture criteria at negative stress triaxiality10.1016/j.ijmecsci.2016.02.001 ↗
30. Ductile fracture locus of Ti-6Al-4V titanium alloy10.1016/j.ijmecsci.2011.10.003 ↗
31. Experimental study on pure titanium subjected to different combined tension and torsion deformation processes10.1016/j.msea.2016.10.106 ↗
32. Calibration of ductile fracture criterion from shear to equibiaxial tension using hydraulic bulge test10.1016/j.jmatprotec.2020.116589 ↗
33. Effects of the stress state on plastic deformation and ductile failure: experiment and numerical simulation using a newly designed tension-shear specimen10.1111/ffe.13084 ↗
34. Structural response of metal sheets under combined shear and tension10.1016/j.istruc.2020.05.006 ↗
35. Dynamic large strain characterization of tantalum using shear-compression and shear-tension testing10.1016/j.mechmat.2017.06.003 ↗
36. An investigation of ductile fracture behavior of Ti6Al4V alloy fabricated by selective laser melting
37. Deformation and failure mechanisms of Ti-6Al-4V as built by selective laser melting10.1016/j.msea.2019.138456 ↗
38. Comparison study on microstructure and mechanical properties of Ti-6Al-4V alloys fabricated by powder-based selective-laser-melting and sintering methods10.1016/j.matchar.2020.110358 ↗
39. Selective laser melting of Ti6Al4V alloy: process parameters, defects and post-treatments10.1016/j.jmapro.2021.01.009 ↗
40. Effects of thickness and orientation on the small scale fracture behaviour of additively manufactured Ti-6Al-4V10.1016/j.matchar.2018.04.003 ↗
41. Effects of defects and microstructures on tensile properties of selective laser melted Ti6Al4V alloys fabricated in the optimal process zone10.1016/j.msea.2021.142294 ↗
42. Anisotropic plasticity and fracture of alpha titanium sheets from cryogenic to warm temperatures10.1016/j.ijplas.2022.103348 ↗
43. High-temperature anisotropic behaviors and microstructure evolution mechanisms of a near-α Ti-alloy sheet10.1016/j.msea.2021.141560 ↗
44. X-ray CT analysis of the influence of process on defect in Ti-6Al-4V parts produced with Selective Laser Melting technology10.1007/s00170-019-04347-0 ↗
45. On the texture and mechanical property anisotropy of Ti6Al4V alloy fabricated by powder-bed based laser additive manufacturing10.1016/j.vacuum.2020.109732 ↗
46. Unraveling the inherent anisotropic properties of in situ alloyed copper-modified titanium alloys produced by laser powder bed fusion10.1016/j.jallcom.2023.171323 ↗