Mechanical and magnetic properties of phase separated Cu50Fe50 (at%) alloys synthesized by mechanical alloying and spark plasma sintering
Source abstract
Abstract
A bulk Cu 50Fe 50 (at%) alloy was prepared by mechanical alloying (MA) of elemental Cu and Fe powders for 20 h, followed by the spark plasma sintering (SPS). All the powder and bulk samples were characterized using X-ray diffraction (XRD) and scanning electron microscopy (SEM). The mechanical and magnetic properties of the bulk samples were also evaluated. From 1 h to about 10 h of milling, the formation of nanocrystalline Cu-rich face-centered cubic solid solution (FCC γ phase) and Fe-rich body-centered cubic solid solution (BCC α phase) was observed. Above 10 h of milling, the γ and α phases merged to form a single-phase face-centered cubic (γ S ) solid solution till 20 h. Subsequently, the 20 h MA powder was consolidated using spark plasma sintering (SPS) at three different temperatures: 519 ℃ (0.5 T m), 677 ℃(0.6 T m), and 835 ℃ (0.7 T m), where T m is the average melting point of the alloy (1310 ℃). In all three samples, the metastable γ S phase decomposed into the nanocrystalline Cu-rich γ and Fe-rich α phases during SPS. Notably, the 0.7 T m sample exhibited a better balance between strength and ductility by demonstrating a compressive yield strength of 886 MPa and an ultimate compressive strength of 1166 MPa with a ductility of 15%. The high strength and ductility are attributed to a bimodal grain size distribution, i.e., a few microns thick and continuous Cu-rich γ grain boundary phase and an intragranular nanocrystalline mixture of γ and α phases. In addition to its excellent mechanical properties, the 0.7 T m sample displayed favorable soft ferromagnetic characteristics exhibiting a saturation magnetization (M s ) of 66 emu/g and a coercivity (H c) of 16 Oe.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. T.B. Massalski (Editor-in-Chief), Binary Alloy Phase Diagrams Vol.1, American Society for Metals, Metals Park, OH, USA (1986).
2. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element10.2320/matertrans.46.2817 ↗
3. Evolution kinetics of microgravity facilitated spherical macro segregation within immiscible alloys10.1016/j.jallcom.2018.06.022 ↗
4. Novel insight into evolution mechanism of second liquid-liquid phase separation in metastable immiscible Cu-Fe alloy10.1016/j.matdes.2018.06.044 ↗
5. FexCu1-x Alloys for Permanent Magnets
6. Influences on distribution of solute atoms in Cu-8Fe alloy solidification process under rotating magnetic field10.1007/s12540-018-0133-4 ↗
7. Production of the 70% Cu–30% Fe alloy by SHS metallurgy and electrometallurgy: comparative analysis of microstructures10.3103/S1067821220010137 ↗
8. Microstructure and properties of Cu-10 wt% Fe alloy produced by double melt mixed casting and multi-stage thermomechanical treatment10.1016/j.jallcom.2019.153323 ↗
9. Homogeneous Cu–Fe supersaturated solid solutions prepared by severe plastic deformation10.1080/14786430903313682 ↗
10. The formation of supersaturated solid solutions in Fe–Cu alloys deformed by high-pressure torsion10.1016/j.actamat.2011.10.044 ↗
11. On the supersaturated solution in the Fe-Cu binary system induced by high energy ball milling10.1007/BF00701439 ↗
12. Mechanical alloying and milling10.1016/S0079-6425(99)00010-9 ↗
13. Mechanical alloying of immiscible elements: experimental results on Ag-Cu and Co-Cu10.1080/01418639708241131 ↗
14. Nanosized mechanocomposites and solid solution in immiscible metal systems10.1023/B:JMSC.0000039258.56606.55 ↗
15. Mechanical alloying of the immiscible Cu-60wt% Cr alloy: phase transitions, microstructure, and thermodynamic characteristics
16. Structural study of nanocrystalline solid solution of Cu–Mo obtained by mechanical alloying10.1016/j.msea.2012.03.105 ↗
17. Characterization of the metastable Cu-Fe nanoparticles prepared by the mechanical alloying route
18. Mechanically driven alloying of immiscible elements10.1103/PhysRevLett.68.2235 ↗
19. Mechanical alloying of immiscible elements: Ag-Fe contrasted with Cu-Fe10.1103/PhysRevB.55.5542 ↗
20. Mechanical alloying in the Fe–Cu system10.1016/S0921-5093(97)00522-4 ↗
21. Two-phase coexistence region in mechanically alloyed Cu–Fe: an X-ray absorption near-edge structure study10.1016/S1359-6454(99)00111-1 ↗
22. Influence of milling temperature on the mechanical alloying and magnetic properties of Cu-Co and Cu-Fe systems
23. Mechanical alloying of Fe-Cu alloys from As-received and premilled elemental powder mixtures10.4028/www.scientific.net/KEM.230-232.631 ↗
24. Alloys created between immiscible elements10.1016/j.pmatsci.2004.07.001 ↗
25. Mechanochemical reactions in nanocrystalline Cu–Fe system induced by mechanical alloying in air atmosphere10.1016/j.powtec.2012.03.016 ↗
26. Thermal and magnetic properties of mechanically alloyed fcc Cu-Fe supersaturated solid solutions10.2320/matertrans.MRA2007189 ↗
27. Fe clustering in fcc Cu-Fe alloys prepared by mechanical alloying10.1023/A:1006507806258 ↗
28. Processing of Cu-Fe and Cu-Fe-SiC nanocomposites by mechanical alloying10.1016/j.apt.2017.04.023 ↗
29. Mössbauer investigations of mechanical alloying in the Fe-Cu system10.1063/1.110329 ↗
30. Thermal stability and grain growth behavior of mechanically alloyed nanocrystalline Fe-Cu alloys10.1063/1.353890 ↗
31. A study of Cu50Fe50 produced by mechanical alloying and its thermal treatment10.1063/1.357354 ↗
32. Processing and microhardness of bulk Cu-Fe nanocomposites10.1016/0965-9773(96)00003-7 ↗
33. A Study of the consumption of iron during the mechanical alloying of the Cu-Fe immiscible system10.4028/www.scientific.net/MSF.179-181.249 ↗
34. Mechanically driven alloying and grain size changes in nanocrystalline Fe-Cu powders10.1063/1.353055 ↗
35. The microstructure and mechanical properties of Fe–Cu materials fabricated by pressure-less-shaping of nanocrystalline powders10.1007/s10853-007-1892-3 ↗
36. Fe–Cu nanocomposites by high pressure consolidation of powders prepared by electric explosion of wires10.1002/adem.201701024 ↗
37. Microstructure and strength of Cu-Fe in situ composites after very high drawing strains10.1016/1359-6454(95)00212-X ↗
38. Metastable transition-metal system bulk alloys prepared by MA and shock compression10.4028/www.scientific.net/MSF.539-543.1937 ↗
39. Spark Plasma Sintering: Process Fundamentals
40. Structural and magnetic properties of metastable fcc Cu-Fe alloys10.1103/PhysRevB.54.441 ↗
41. adapted by R. Balasubramaniam
42. Suryanarayana · 1998
43. Cullity · 1956
44. P. Shingu (Ed), Mechanical Alloying, Proceedings of the 1st International Symposium on Mechanical Alloying, Kyoto, Japan, May 1991 (Materials Science Forum), Trans Tech Publishers, 1992.10.4028/b-XNw5fh ↗
45. Magneto-volume effects in Fe–Cu solid solutions10.1016/j.jmmm.2005.10.073 ↗
46. Is there a hexagonal-close-packed (hcp)→ face-centered-cubic (fcc) allotropic transformation in mechanically milled Group IV(B) elements?10.1557/jmr.2009.0423 ↗
47. Spinodal decomposition and precipitation in Cu–Cr nanocomposite10.1016/j.jallcom.2013.11.019 ↗
48. Thermodynamic and magnetic properties of metastable FexCu100−x solid solutions formed by mechanical alloying10.1063/1.354837 ↗
49. Mechanical properties of nanocrystalline materials10.1016/j.pmatsci.2005.08.003 ↗
50. Fabrication of Fe-Cu composites from electroexplosive bimetallic nanoparticles by spark plasma sintering10.1016/j.vacuum.2019.108980 ↗
51. The properties of foams and lattices10.1098/rsta.2005.1678 ↗
52. Oxygen-mediated deformation and grain refinement in Cu-Fe nanocrystalline alloys10.1016/j.actamat.2018.12.040 ↗
53. Microstructure and properties of Cu–Fe deformation processed in-situ composite10.1016/j.vacuum.2019.05.030 ↗
54. Effects of annealing temperature and layer thickness on hardening behavior in cross accumulative roll bonded Cu/Fe nanolamellar composite10.1016/j.jallcom.2020.154312 ↗
55. Hierarchical microstructures and deformation behavior of laser direct-metal-deposited Cu–Fe alloys10.1016/j.msea.2020.140659 ↗
56. Magnetic phase-transition dependence on nano-to-micron grain-size microstructural changes of mechanically alloyed and sintered Ni 0.6 Zn 0.4 Fe2O410.1007/s10948-013-2453-4 ↗
57. Investigation on solid solubility and physical properties of Cu–Fe/CNT nano-composite prepared via mechanical alloying route10.1016/j.powtec.2014.08.010 ↗