Effects of Co on the microstructure evolution and mechanical properties of Ti-4Al-6Cr-5Mo-8 Nb alloy by ultrasonic vacuum melting
Source abstract
Abstract
An investigation was conducted into the impact of low cobalt content on the microstructure and mechanical properties of titanium alloys. Ti-4Al-6Cr-5Mo-8 Nb- xCo ( x = 0, 2, 3, 4, and 5) alloys were prepared by ultrasonic-assisted melting and casting. The changes in microstructure, mechanical properties, and the strengthening and toughening mechanisms were researched. Results show that, when the cobalt content increases from 0 to 5 wt%, the as-cast structure is all β phase. The lattice parameter of the β phase decreases from 0.3663 to 0.3114 nm, a 15% decrease. The size of primary β grains decreases from 676.8 to 310.7 μm, a 54% decrease. When the cobalt content exceeds 3 wt%, the segregation energy of cobalt increases and grain boundary segregation occurs. Grain refinement is due to constitutional supercooling caused by the β-stable element cobalt, as well as the solute drag caused by the differences in intragranular and grain boundary compositions. In addition, the size mismatch between cobalt and titanium atoms leads to lattice distortion. As the cobalt content increases from 0 to 3 wt%, the tensile strength increases from 918.1 to 1147.8 MPa, a 25% increase, while the fracture toughness increases from 51.7 to 59.7 MPa·m 1/2 , a 15% increase. At 5 wt% cobalt, the tensile strength and fracture toughness diminished to 247.5 MPa and 14.8 MPa·m 1/2 , respectively. The decrease in lattice parameters mainly lead to an increase in strength. The secondary crack leads to an increase in toughness. The decline in strength and toughness results from cobalt segregating at grain boundaries, leading to embrittlement.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Properties and applications of titanium alloys: a brief review
2. Assessment of the effects of Si addition to a new TiMoZrTa system10.3390/ma14247610 ↗
3. Titanium alloys for aerospace applications10.1002/adem.200310095 ↗
4. Opportunities and issues in the application of titanium alloys for aerospace components10.3390/met10060705 ↗
5. A review on high-strength titanium alloys: microstructure, strengthening, and properties10.1002/adem.201801359 ↗
6. High-strength titanium alloys for aerospace engineering applications: a review on melting-forging process10.1016/j.msea.2022.143260 ↗
7. Structure and properties of titanium-25 niobium-x iron alloys
8. Structure and mechanical properties of as-cast Ti–5Nb–xFe alloys10.1016/j.matchar.2010.05.003 ↗
9. Forming mechanism of growth twins and microstructure evolution on improvement of strength and toughness properties by β-eutectoid element in Ti-7Mo-4Al-4Zr-3Nb-2Cr-xFe alloys10.1016/j.jallcom.2023.169507 ↗
10. Influence of Fe and Ni on creep of near α-Ti alloy IMI83410.1016/j.msea.2005.03.027 ↗
11. Titanium and titanium alloy applications in medicine10.1504/IJNBM.2007.016517 ↗
12. Titanium alloys for biomedical applications10.1016/j.msec.2005.08.032 ↗
13. Effects of Fe, Co and Ni elements on the ductility of TiAl alloy10.1016/j.jallcom.2014.07.199 ↗
14. The interdependence of microstructure, strength and fracture toughness in a novel β titanium alloy Ti-5Al-4Zr-8Mo-7V10.1016/j.msea.2020.139248 ↗
15. Recent development of effect mechanism of alloying elements in titanium alloy design10.1016/S1875-5372(14)60082-5 ↗
16. Investigation of Ti–Fe–Co bulk alloys with high strength and enhanced ductility10.1016/j.actamat.2005.01.012 ↗
17. High strength beta titanium alloys: New design approach10.1016/j.msea.2015.01.073 ↗
18. Beta fleck and segregation in titanium alloy ingots10.1515/HTMP.2006.25.5-6.337 ↗
19. Effects of ultrasonic introduced by L-shaped ceramic sonotrodes on microstructure and macro-segregation of 15t AA2219 aluminum alloy ingot10.3390/ma12193162 ↗
20. A novel method for grain refinement and microstructure modification in TiAl alloy by ultrasonic vibration10.1016/j.msea.2015.12.001 ↗
21. Effects of ultrasonic vibration on the microstructure and mechanical properties of high alloying TiAl
22. The interdependence of microstructure, strength and fracture toughness in a novel β titanium alloy Ti-5Al-4Zr-8Mo-7V10.1016/j.msea.2020.139248 ↗
23. Effect of various Ca content on microstructure and fracture toughness of extruded Mg-2Zn alloys10.1016/j.jallcom.2017.11.276 ↗
24. X-ray diffraction and the Bragg equation10.1021/ed074p129 ↗
25. First-principles analysis of the grain boundary segregation of transition metal alloying elements in γ Fe10.1016/j.commatsci.2021.111050 ↗
26. Effects of alloying elements on cohesion and brittleness of grain boundary of iron10.1016/j.matchemphys.2021.125291 ↗
27. Surface energies of elemental crystals10.1038/sdata.2016.80 ↗
28. Grain boundary properties of elemental metals10.1016/j.actamat.2019.12.030 ↗
29. Effects and mechanisms of grain refinement in aluminum alloys.10.1007/BF02708630 ↗
30. Beryllium as a grain refiner in titanium alloys10.1016/j.jallcom.2009.03.016 ↗
31. Solvent and solute diffusion in bcc Ti-Co and Ti-Mn alloys.10.1080/14786437508229632 ↗
32. Effect of solute on the growth rate and the constitutional undercooling ahead of the advancing interface during solidification of an alloy and the implications for nucleation10.1557/jmr.2006.0302 ↗
33. Surface characterization and diffusion model of pack borided TB2 titanium alloy10.1016/j.ceramint.2018.07.060 ↗
34. An analytical model for constitutional supercooling-driven grain formation and grain size prediction10.1016/j.actamat.2010.01.052 ↗
35. Migration of solidification grain boundaries and prediction10.1038/s41467-022-33482-8 ↗
36. Solute drag, solute trapping and diffusional dissipation of Gibbs energy10.1016/S1359-6454(99)00336-5 ↗
37. The interrelated effect of initial melt undercooling, solute trapping and solute drag on the grain growth mechanism of as-solidified Ni-B alloys10.1016/j.jallcom.2014.05.064 ↗
38. Effect of atomic size mismatch and chemical complexity on the local lattice distortion of BCC solid solution alloys
39. A statistical theory of solid solution hardening10.1002/pssb.19700410221 ↗
40. Multi-component solid solution hardening: Part 1 Proposed model10.1007/BF00540987 ↗
41. Solid solution strengthening theories of high-entropy alloys10.1016/j.matchar.2019.02.034 ↗
42. Solid solution strengthening in concentrated Mg-Al alloys10.1016/S1471-5317(01)00008-6 ↗
43. Solid Solution Hardening of Copper Crystals10.1007/BF00552938 ↗
44. Multiplicity of dislocation pathways in a refractory multiprincipal element alloy10.1126/science.aba3722 ↗
45. Substitutional solution hardening of magnesium single crystals10.1080/14786437208229311 ↗
46. Solid solution strengthening behaviors in binary Mg-Y single phase alloys10.1016/j.jallcom.2008.04.049 ↗
47. Microstructural effects on the mechanical behavior of B-modified Ti–6Al–4V alloys10.1016/j.actamat.2007.05.009 ↗
48. Precipitation behavior of silicide and synergetic strengthening mechanisms in TiB-reinforced high-temperature titanium matrix composites during multi-directional forging10.1016/j.jallcom.2021.159051 ↗
49. The effects of microstructure evolution on the fracture toughness of BT-25 titanium alloy during isothermal forging and subsequent heat treatment10.1016/j.msea.2018.12.062 ↗
50. Microstructure and mechanical properties of in-situ synthesized TiB whiskers reinforced titanium matrix composites by high-velocity compaction10.1016/j.powtec.2014.07.048 ↗
51. Investigation of Ti–Fe–Co bulk alloys with high strength and enhanced ductility10.1016/j.actamat.2005.01.012 ↗
52. Simultaneously enhanced strength and ductility of titanium via multimodal grain structure10.1016/j.scriptamat.2010.07.010 ↗
53. Effect of annealing temperature on mechanical properties of TC21 titanium alloy with multilevel lamellar microstructure10.1016/j.msea.2023.144788 ↗
54. Effect of Mn addition on microstructural changes and mechanical properties of Ti–5Al–2.5 Fe alloys10.1007/s12540-018-0115-6 ↗
55. Effects of niobium addition on the microstructure and mechanical properties of laser-welded joints of NiTiNb and Ti6Al4V alloys10.1016/j.jallcom.2017.11.307 ↗
56. Effects of β-stabilizer elements on microstructure formation and mechanical properties of titanium alloys10.1016/j.jallcom.2021.160085 ↗
57. Hot and cold rolling of a novel near-α titanium alloy: Mechanical properties and underlying deformation mechanism10.1016/j.msea.2022.144543 ↗