Refining Ti2AlC in the liquid region and improving the microstructure and mechanical properties of Ti-46Al-8 Nb-2.6 C alloy by adding Y
Source abstract
Abstract
To reveal the refinement mechanism of Ti 2AlC particle by in-situ Y 2O 3 in the liquid region and the improvement mechanisms of refined Ti 2AlC in solid-state phase transformation process, Ti-46Al-8 Nb-2.6 C- x Y alloys were prepared. Microstructures were observed by SEM, XRD and TEM, and the mechanical properties were examined. Calculated results indicated that the phase boundary energy of in-situ Y 2O 3 combined with TiC was low in the liquid region. TiC particle was formed initially, followed by Y 2O 3 particle. The Y 2O 3 particle moved to the surface of TiC particle to inhibit its growth, which left small-sized TiC nucleation substrate for the formation of Ti 2AlC. The orientation relationship was [ 2 ̅ 200 ] Ti 2 AlC / / [ 0 6 ̅ 6 ] Y 2 O 3 . A stepped atomic diffusion zone was formed in the interface of Y 2O 3 and Ti 2AlC to inhibit lateral and longitudinal growth of Ti 2AlC. As Y increased from 0.02 to 0.1 at%, the average aspect ratio of Ti 2AlC particles decreased from 7.7 to 3.4, the Ti 2AlC content with the aspect ratio of 1–5 increased from 13.7 to 91.3%. The lamellar colony size and lamellar spacing reduced from 47.5 to 26.0 µm and 0.74 to 0.58 µm, respectively. Both Y 2O 3 and refined Ti 2 AlC served as heterogeneous nucleation sites and inhibited the lateral thickening rate of γ lath. The Y-type YAl 2 phase was formed as Y content exceeded 0.1 at%. The compressive strength and Vickers hardness were improved from 1801 to 2201 MPa and 443.2 to 464.5 HV, respectively. However, the subsequent decrease in strength was caused by the embrittlement of grain boundary after the precipitation of YAl 2 phase. The significant refinement of Ti 2AlC and lamellar colony by in-situ Y 2O 3 and the precipitation strengthening of Ti 2AlC contributed to the mechanical properties.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Intermetallics and Advanced Alloy Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. A newly developed hot worked TiAl alloy for blades and structural components10.1016/S1359-6462(02)00158-6 ↗
2. Mechanical alloying: a critical review10.1080/21663831.2022.2075243 ↗
3. Fabrication of TiAl components by means of hot forging and machining10.1016/j.intermet.2004.12.012 ↗
4. The machining of γ-TiAI intermetallic alloys10.1016/S0007-8506(07)60059-6 ↗
5. Effect of Zr on microstructure and properties of TC4 alloy fabricated by laser additive manufacturing10.1016/j.jmrt.2023.05.137 ↗
6. Zhang · J. Alloy. Compd. · 2023 · 996
7. Efect of heat input on interfacial characterization of the butter joint of hot‑rolling CP‑Ti/Q235 bimetallic sheets by Laser+CMT10.1038/s41598-021-89343-9 ↗
8. Microstructural modulation of TiAl alloys for controlling ultra-precision machinability
9. Microstructure characterization and hot corrosion mechanism of as-cast and heat treated high Nb containing TiAl alloy10.1016/j.corsci.2021.109399 ↗
10. Effect of Al content and Nb addition on the strength and fault energy of TiAl alloys10.1016/S0921-5093(01)01663-X ↗
11. Investigation of welding crack in micro laser welded NiTiNb shape memory alloy and Ti6Al4V alloy dissimilar metals joints10.1016/j.optlastec.2016.12.028 ↗
12. Q. Wang. Tensile behavior, microstructural evolution, and deformation mechanisms of a high Nb-TiAl alloy additively manufactured by electron beam melting10.1016/j.matdes.2022.111503 ↗
13. Development of gamma titanium aluminide (γ-TiAl) alloys: a review10.1016/j.jallcom.2022.167262 ↗
14. Mechanical properties and microstructure evolution of Ti2AlC under compression in 25-1100 °C temperature range10.1016/j.actamat.2020.02.057 ↗
15. The effect of carbon addition on the high-temperature properties of β solidification TiAl alloys10.1016/j.jallcom.2018.09.397 ↗
16. Influence of nano-Y2O3 addition on microstructure and tensile properties of high-Al TiAl alloys10.1016/j.msea.2020.139803 ↗
17. Enhanced high temperature tensile and creep properties of a β-solidified γ-TiAl alloy with the hybrid addition of C and Y2O310.1016/j.intermet.2022.107698 ↗
18. J. Xie. Investigation on the in-situ reaction mechanism of Ti2AlC/TiAl composite prepared by spark plasma sintering10.1016/j.matchar.2022.112417 ↗
19. Achieving superior high-temperature strength and oxidation resistance of TiAl nanocomposite through in situ semicoherent MAX phase precipitation10.1021/acsami.1c21719 ↗
20. Y. Chen. Creep behavior and related phase precipitation of a creep-resistant Y2O3-bearing high Nb containing TiAl alloy10.1016/j.matchar.2023.112767 ↗
21. Microstructural refinement and improvement of mechanical properties and oxidation resistance in EPM TiAl-based intermetallics with yttrium addition10.1016/S1359-6454(02)00006-X ↗
22. H Fu. Role of graphite on microstructural evolution and mechanical properties of ternary TiAl alloy prepared by arc melting method10.1016/j.matdes.2018.06.048 ↗
23. An effective scheme to determine surface energy and its relation with adsorption energy10.1016/j.actamat.2021.116895 ↗
24. Summary of constitutional data on the aluminum-carbon-titanium system10.1007/BF02647559 ↗
25. Anti-phase boundary energy of β series precipitates in Mg-Y-Nd system10.1016/j.scriptamat.2020.11.004 ↗
26. Effect of nano Y2O3 addition on microstructure and room temperature tensile properties of Ti-48Al-2Cr-2Nb alloy10.1016/j.vacuum.2019.06.026 ↗
27. Significant enhancement in high-temperature tensile strength of trace nano-Y2O3-reinforced TiAl alloy prepared by selective electron beam melting10.1016/j.msea.2023.145086 ↗
28. Effects of V and B, Y additions on the microstructure and creep behaviour of high-Nb TiAl10.1016/j.jallcom.2018.03.055 ↗
29. A β-solidifying TiAl alloy reinforced with ultra-fine Y-rich precipitates10.1016/j.scriptamat.2020.10.010 ↗
30. Advances in phase relationship for high Nb-containing TiAl alloys10.1007/s12598-015-0658-3 ↗
31. Low temperature heat capacity of some rare earth aluminum Laves phase compounds: YAl2, LaAl2 and LuAl210.1016/0022-3697(72)90021-2 ↗
32. S. Liu. Ti-46Al-4Nb alloy refined and reinforced by in-situ TiC nanoparticles and TiB2
33. Thermal residual stress in metal matrix composite10.1016/0001-6160(87)90188-X ↗
34. Influence of interlayer temperature on microstructure and mechanical properties of TiAl alloys in wire and arc additive manufacturing10.1016/j.jmapro.2023.03.062 ↗
35. Investigation of the nucleation and growth behavior of Ti2AlC and Ti3AlC nano-precipitates in TiAl alloys10.1515/ntrev-2022-0510 ↗
36. Enhanced strength and ductility in Ti46Al4Nb1Mo alloys via boron addition10.1016/j.jmst.2021.06.037 ↗
37. The α2 to orthorhombic phase transformation facilitated high elastically mediated strain transfer ability in high Nb-TiAl alloys10.1016/j.matchar.2023.112924 ↗
38. Z. Wang. Balancing the strength and ductility of Ti2AlC/TiAl composite with a bioinspired micro-nano laminated architecture10.1016/j.matdes.2022.110851 ↗
39. Role of V in microstructure and strength enhancement of 4 vol% nano-TiB2/TiAl composites10.1016/j.msea.2022.144342 ↗
40. Superior strength-plasticity synergy in a heterogeneous lamellar Ti2AlC/TiAl composite with unique interfacial microstructure10.1016/j.jmst.2023.03.011 ↗
41. Effect of Sn addition on the mechanical properties and high-temperature oxidation resistance of intermetallic TiAl alloys by first principles study and experimental investigation10.1016/j.jmrt.2022.11.007 ↗
42. Individual and synergistic effects of Ta and Mn on optimizing the microstructures and mechanical properties of TiB reinforced high Nb-TiAl composites10.1016/j.jmrt.2023.01.004 ↗
43. Effect of LaB6 on the microstructure evolution and mechanical properties of Ti-45Al-8Nb alloy10.1016/j.jallcom.2022.168513 ↗
44. Improvement on high-temperature tensile strength and ductility of selective electron beam melting TiAl alloys via small-strain forging10.1016/j.msea.2023.145009 ↗
45. Defect elimination and microstructure improvement of laser powder bed fusion β-solidifying γ-TiAl alloys via circular beam oscillation technology10.1016/j.msea.2023.145019 ↗
46. Microstructure and mechanical properties of in-situ dual morphology Ti8C5/TiB2 reinforced TiAl composite10.1016/j.msea.2022.142918 ↗
47. Mechanical properties of high niobium TiAl alloys doped with Mo and C10.1016/j.matdes.2016.03.079 ↗
48. Effects of tailoring microstructure on short-term creep behavior of high Nb containing TiAl alloys under various stress levels10.1016/j.jmrt.2023.05.231 ↗
49. Microsegregation in high Nb containing TiAl alloy ingots beyond laboratory scale10.1016/j.intermet.2006.10.003 ↗
50. Microstructural evolution and mechanical properties of a high yttrium containing TiAl based alloy densified by spark plasma sintering10.1016/j.jallcom.2019.153264 ↗
51. Microstructural configuration and compressive deformation behavior of a TiAl composite reinforced by Mn and in situ Ti2AlC particles10.1016/j.msea.2021.141772 ↗
52. New insights into high-temperature deformation and phase transformation mechanisms of lamellar structures in high Nb-containing TiAl alloys10.1016/j.actamat.2020.01.021 ↗
53. On the influence of stoichiometry and purity on the deformation mechanisms in the intermetallic compound TiAl10.1016/0956-716X(90)90307-3 ↗
54. Dislocation mobility, ductility and anomalous strengthening of two-phase TiAl alloys: effects of oxygen and composition10.1016/0966-9795(95)00060-7 ↗
55. The microstructure evolution and properties of a Cu-Cr-Ag alloy during thermal-mechanical treatment10.1557/jmr.2017.17 ↗
56. Non-destructive pulsed field CuAg-solenoids10.1016/j.msea.2009.11.038 ↗
57. Dislocation self-interaction in TiAl: evolution of super-dislocation dipoles revealed by atomistic simulations10.1016/j.jmst.2020.03.091 ↗
58. evolution and mechanical behavior of ultrasonically synthesized Al6061-nano alumina composites10.1016/j.msea.2018.03.092 ↗
59. Compression properties and work-hardening behavior of Ti2AlC/TiAl composites fabricated by combustion synthesis and hot press consolidation in the Ti-Al-Nb-C system10.1016/j.matdes.2011.05.041 ↗
60. Effects of grain size on yield strength in TiAl10.1016/0956-716X(91)90106-B ↗
61. Effect of Y-modified TiB2 ceramic particles on the microstructure and mechanical properties of TIG welded joints of spray-formed 7055 aluminum alloy10.1016/j.jmrt.2022.08.077 ↗
62. Assessment of models used to predict the strength of discontinous silicon carbide reinforced aluminum alloys10.1016/0036-9748(87)90105-0 ↗
63. On the strength of discontinuous silicon carbide reinforced aluminum composites10.1016/0036-9748(86)90210-3 ↗