journal article·2023-05

Tailoring strength and ductility of Mg97Y2Zn1 alloy through the architecture of heterogeneous lamellar structure by large-ratio hot extrusion

Chao Sun, Huan Liu, Xiaoru Zhuo, Yuna Wu, Kai Yan, Jia Ju, Jinghua Jiang, Feng Xue, Jing Bai

Publisher page

Abstract

In this study, a heterogeneous lamellar structure is achieved in Mg 97Y 2Zn 1 alloy via large-ratio hot extrusion of the alloys in as-cast (CE) and as-annealed (AE) stages. The ultimate tensile strength (UTS) of CE and AE alloys is 426.5 and 471.4 MPa, and their fracture elongation (FE) is 8.1% and 1.0%, respectively. Mechanical properties of the CE and AE alloys exceed that of the majority of wrought Mg 97Y 2Zn 1 alloys due to the heterostructure induced strengthening. Both in the two extruded alloys, α-Mg layers and LPSO layers acting as soft and hard domains, respectively, constitute the heterogeneous lamellar structure. As a result of the narrower spacing of α-Mg and LPSO layers, more refined DRX grains and LPSO particles, and the increased volume fraction of LPSO phase, the strength of the AE alloy is higher than that of CE alloy. However, the AE alloy exhibits poor ductility owing to the easy aggregation of dislocations and stress at the interfaces of narrower layers. Based on discussion of the strengthening mechanisms, the preparation of Mg 97Y 2Zn 1 alloys with tailored mechanical properties of high UTS ranging from 420 to 480 MPa, and FE 1∼ 8%, could be realized via the combination of annealing (controlling the content of 14H phase) and large-ratio hot extrusion (promoting the formation of heterogeneous lamellar structure).
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Recent developments on corrosion behaviors of Mg alloys with stacking fault or long period stacking ordered structures10.1016/j.jma.2020.09.021 ↗
2. In-situ 14H-LPSO reinforced GW93 alloy prepared from the recycling of discard components by rapid-solidification plus hot press sintering technique
3. Developing super-hydrophobic and corrosion-resistant coating on magnesium-lithium alloy via one-step hydrothermal processing
4. Fragmentation of 18R LPSO phases through multi-pass equal channel angular pressing and its impact on rollability of Mg97Y2Zn1 (at%) alloy10.1016/j.jmrt.2020.10.067 ↗
5. Plasticity analysis by synchrotron radiation in a Mg97Y2Zn1 alloy with bimodal grain structure and containing LPSO phase10.1016/j.actamat.2015.04.048 ↗
6. α-Mg/LPSO (Long-Period Stacking Ordered) phase interfaces as obstacles against dislocation slip in as-cast Mg-Zn-Y alloys10.1016/j.ijplas.2022.103294 ↗
7. Mechanical properties and failure of ECAE processed Mg97Y2Zn1 at different strain rates10.1016/j.msea.2019.138094 ↗
8. A two-step dynamic recrystallization induced by LPSO phases and its impact on mechanical property of severe plastic deformation processed Mg97Y2Zn1 alloy10.1016/j.jallcom.2017.02.107 ↗
9. Fragmentation of long period stacking ordered (LPSO) phase and its impact on microstructure evolution of a Mg–Y–Zn alloy during multi-directional forging10.1016/j.msea.2020.139898 ↗
10. Exceptional mechanical properties of an Mg97Y2Zn1 alloy wire strengthened by dispersive LPSO particle clusters10.1016/j.matlet.2019.01.089 ↗
11. Microstructure and mechanical properties of ultrafine grained Mg97Y2Zn1 alloy processed by equal channel angular pressing10.1016/j.jallcom.2006.09.005 ↗
12. Microstructure and mechanical properties of Mg–RE–TM cast alloys containing long period stacking ordered phases: a review10.1007/s40195-018-0862-x ↗
13. Towards developing Mg alloys with simultaneously improved strength and corrosion resistance via RE alloying10.1016/j.jma.2020.08.016 ↗
14. Recent advances in LPSO-containing wrought magnesium alloys: relationships between processing, microstructure, and mechanical properties10.1007/s11837-019-03610-9 ↗
15. Growth and transformation mechanisms of 18R and 14H in Mg–Y–Zn alloys10.1016/j.actamat.2012.08.022 ↗
16. Comparative studies on evolution behaviors of 14H LPSO precipitates in as-cast and as-extruded Mg–Y–Zn alloys during annealing at 773K10.1016/j.matdes.2015.12.151 ↗
17. Coexistence of 14H and 18R-type long-period stacking ordered (LPSO) phases following a novel orientation relationship in a cast Mg-Al-RE-Zn alloy10.1016/j.jallcom.2018.07.053 ↗
18. Research advances in magnesium and magnesium alloys worldwide in 202010.1016/j.jma.2021.04.001 ↗
19. Fabrication of exceptionally high-strength Mg-4Sm-0.6Zn-0.4Zr alloy via low-temperature extrusion10.1016/j.msea.2021.142565 ↗
20. Achieving high strength-ductility synergy in a novel Mg–Bi–Sn–Mn alloy with bimodal microstructure by hot extrusion10.1016/j.msea.2022.142623 ↗
21. Optimization in strength-ductility of heterogeneous Mg-13Gd alloy via small extrusion ratio combined with pre-aging10.1016/j.msea.2021.142540 ↗
22. Heterogeneous materials: a new class of materials with unprecedented mechanical properties10.1080/21663831.2017.1343208 ↗
23. Heterostructured materials: superior properties from hetero-zone interaction10.1080/21663831.2020.1796836 ↗
24. A review on heterogeneous nanostructures: a strategy for superior mechanical properties in metals10.3390/met9050598 ↗
25. Effect of ECAP temperature on formation of triple heterogeneous microstructure and mechanical properties of Zn–1Cu alloy10.1016/j.msea.2021.141990 ↗
26. Effect of forced-air cooling on the microstructure and age-hardening response of extruded Mg-Gd-Y-Zn-Zr alloy full with LPSO lamella10.1016/j.jmst.2020.09.020 ↗
27. Improved strength in wrought Mg–Y–Ni alloys by adjusting the block-shaped LPSO phase and plate-shaped γ′ phase10.1016/j.msea.2021.142198 ↗
28. Effects of heat treatment before extrusion on dynamic recrystallization behavior, texture and mechanical properties of as-extruded Mg-Gd-Y-Zn-Zr alloy10.1016/j.msea.2021.142479 ↗
29. Preparation of ultra-high strength Mg-Gd-Y-Zn-Zr alloy by pre-ageing treatment prior to extrusion10.1016/j.jallcom.2021.162490 ↗
30. Microstructure and mechanical properties of ultrafine grained Mg97Y2Zn1 alloy processed by equal channel angular pressing10.1016/j.jallcom.2006.09.005 ↗
31. Microstructures and mechanical properties of Mg-2Y-xZn (x=1, 2, 3 at%) alloys10.1016/S1875-5372(14)60079-5 ↗
32. Effect of zirconium addition on microstructure and mechanical properties of Mg97Y2Zn1 alloy10.1016/S1003-6326(11)61244-2 ↗
33. Effect of multimodal microstructure evolution on mechanical properties of Mg–Zn–Y extruded alloy10.1016/j.actamat.2011.02.038 ↗
34. Mechanical properties and failure characteristics of cast and extruded Mg97Y2Zn1 alloys with LPSO phase10.1016/j.msea.2015.11.069 ↗
35. Optimization of strength by microstructural refinement of MgY2Zn1 alloy during extrusion and ECAP processing10.1016/j.msea.2014.07.012 ↗
36. Effect of rolling temperature on the microstructures and mechanical properties of Mg97Zn1Y2 magnesium alloy10.1007/s11665-009-9394-x ↗
37. Evading strength-corrosion tradeoff in Mg alloys via dense ultrafine twins10.1038/s41467-021-24939-3 ↗
38. Hydrogen storage behavior of Mg-based alloy catalyzed by carbon-cobalt composites10.1016/j.jma.2020.09.027 ↗
39. Deformation behavior of Mg-13Gd-4Y–2Zn-0.5Zr alloy on the basis of LPSO kinking, dynamic recrystallization and twinning during compression-torsion10.1016/j.matchar.2021.111215 ↗
40. A high strength and ductility Zn–Cu–Mg alloy achieved by bandlike distribution of ultra-fine CuZn5 and Mg2Zn11 particles10.1016/j.msea.2022.143584 ↗
41. Developing a low-alloyed fine-grained Mg alloy with high strength-ductility based on dislocation evolution and grain boundary segregation10.1016/j.scriptamat.2021.114414 ↗
42. Evolutions of CuZn5 and Mg2Zn11 phases during ECAP and their impact on mechanical properties of Zn-Cu-Mg alloys10.1016/j.jmrt.2022.11.095 ↗
43. Toward the development of Mg alloys with simultaneously improved strength and ductility by refining grain size via the deformation process10.1007/s12613-020-2190-1 ↗
44. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility10.1073/pnas.1517193112 ↗
45. Microstructure evolution during superplastic deformation process and its impact on superplastic behavior of a Mg-Gd-Y-Zn-Zr alloy10.1016/j.matchar.2021.110879 ↗
46. Ultrastrong nanotwinned pure nickel with extremely fine twin thickness10.1126/sciadv.abg5113 ↗
47. Tensile behavior and flow stress anisotropy of accumulative roll bonded Cu-Nb nanolaminates10.1063/1.4941043 ↗
48. Heterostructured materials10.1016/j.pmatsci.2022.101019 ↗
49. Ultrastrong Mg alloy via nano-spaced stacking faults10.1080/21663831.2013.765927 ↗
50. Improved workability for Mg-Y-Zn alloys via increased volume fraction of block LPSO phases10.1016/j.msea.2020.139934 ↗
51. Solute atom mediated Hall-Petch relations for magnesium binary alloys10.1016/j.scriptamat.2021.114451 ↗
52. Analysis of strain hardening behavior in a ductile Mg–Yb based alloy10.1016/j.msea.2021.141462 ↗
53. Ultrastrong low-carbon nanosteel produced by heterostructure and interstitial mediated warm rolling10.1126/sciadv.aba8169 ↗
54. A quantitative study on mechanical behavior of Mg alloys with bimodal texture components10.1016/j.actamat.2021.117013 ↗
55. Anisotropy investigation of an ECAP-processed Mg-Al-Ca-Mn alloy with synergistically enhanced mechanical properties and corrosion resistance10.1016/j.jallcom.2022.165046 ↗
56. Diffusion behaviour and mechanical properties of binary Mg–Gd system10.1016/j.intermet.2021.107171 ↗
57. Strengthening the Mg–Y–Zn alloy through the formation of nanoscale lamellar structures and nanograins10.1016/j.jallcom.2021.161148 ↗
58. New insights on the different corrosion mechanisms of Mg alloys with solute-enriched stacking faults or long period stacking ordered phase10.1016/j.corsci.2022.110163 ↗