journal article·2022-12

A new β-Ti alloy with good tensile properties by the mixed microstructure characteristics of α phase

Huijin Jin, Shaobin Shi, Jianjun Li, Xianxian Wang, Chenxi Yang

Publisher page

Abstract

In this study, the mechanical properties, microstructural characteristics and deformation behavior of a novel high-strength metastable β alloy Ti-6.5Cr-4.5Sn-4.5Mo (wt %) were investigated. By obtaining α phase mixed microstructure with different size, morphology and orientation combinations in β matrix, a good combination of tensile strength σ b~1305 MPa and total elongation ɛ f~13.4 % was achieved. The microstructural characteristics of α phase consisting of discontinuous thin grain boundary α phase (α GB), lamellar α colonies and acicular α s precipitates were obtained by the solution treatment above β transus for a short time plus subsequent aging treatment after the heavy cold rolling. Detailed TEM analysis shows that it is difficult to deform for acicular α s precipitates due to their fine-scale, leading to a large number of α/β interfaces acting as dislocation barriers, which may ultimately result in an improvement on strength of the alloy. Compared with α s, the α GB and lamellar α colonies are soft, which could produce the large enough deformation and allow dislocations to generate and accumulate within them, so that it is beneficial to improve the mechanical properties of the alloy. Stress-relaxation experiments show that the sample with a uniform and finer distribution of α precipitate has a larger value of mobile dislocation ρ m/ρ m0 after relaxation, implying that most of the mobile dislocations remains in the sample, which results in the ultrahigh strength meanwhile accepted ductility in the specimen.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. A review on heat treatment efficiency in metastable β titanium alloys: the role of treatment process and parameters10.1016/j.jmrt.2020.10.088 ↗
2. Deformation behavior and microstructure evolution of titanium alloys with lamellar microstructure in hot working process: a review10.1016/j.jmst.2019.07.052 ↗
3. Design of uniform nano α precipitates in a pre-deformed β-Ti alloy with high mechanical performance10.1016/j.jmrt.2018.06.006 ↗
4. Correlation between alpha phase morphology and tensile properties of a new beta titanium alloy10.1016/j.matdes.2017.02.043 ↗
5. Tuning the scale of α precipitates in β-titanium alloys for achieving high strength10.1016/j.scriptamat.2018.05.040 ↗
6. Improvement of ductility in Ti-5Al-5Mo-5V–3Cr alloy by network-like precipitation of blocky α phase10.1016/j.msea.2018.03.025 ↗
7. Study on the relationship between microstructure and mechanical property in a metastable β titanium alloy10.1016/j.jallcom.2014.12.100 ↗
8. Effect of microstructure on tensile properties of Ti-5Al-5Mo-5V–3Cr-1Zr alloy10.1016/j.jallcom.2016.09.233 ↗
9. A novel high-strength β-Ti alloy with hierarchical distribution of α-phase: the superior combination of strength and ductility10.1016/j.matdes.2019.107640 ↗
10. Microstructural tailoring and mechanical properties of a multi-alloyed near β titanium alloy Ti-5321 with various heat treatment10.1016/j.msea.2017.11.029 ↗
11. Phase precipitation behavior during isothermal deformation in β-quenched near beta titanium alloy Ti-733310.1016/j.jallcom.2016.02.102 ↗
12. Effect of cold rolling and heat-treatment on the microstructure and mechanical properties of β-titanium Ti-25Nb-25Zr alloy10.1016/j.msea.2018.09.002 ↗
13. Development of α-phase morphologies during low temperature isothermal heat treatment of a Ti–5Al–5Mo–5V–3Cr alloy10.1016/j.msea.2010.09.061 ↗
14. Effects of cold pre-deformation on aging behavior and mechanical properties of Ti-1300 alloy10.1016/j.jallcom.2014.09.064 ↗
15. Microstructural evolution, mechanical properties and fracture toughness of near β titanium alloy during different solution plus aging heat treatments10.1016/j.jallcom.2019.07.134 ↗
16. Processing-microstructure-yield strength correlation in a near β Ti alloy, Ti–5Al–5Mo–5V–3Cr10.1016/j.msea.2014.04.113 ↗
17. Correlation between alpha phase morphology and tensile properties of a new beta titanium alloy10.1016/j.matdes.2017.02.043 ↗
18. Microstructure development in a thermomechanically processed Ti- 15V–3Cr-3Sn-3A1 alloy10.1016/0921-5093(96)10236-7 ↗
19. Role of defects on microstructure development of beta titanium alloys10.1007/BF03028215 ↗
20. Effect of solution treatment and aging on microstructure and tensile properties of high strength β titanium alloy Ti–5Al–5V–5Mo–3Cr10.1016/j.matdes.2014.04.015 ↗
21. Effect of heat treatment variations on the microstructure evolution and mechanical properties in a β metastable Ti alloy10.1016/j.jallcom.2016.05.225 ↗
22. Quick reference guide for β titanium alloys in the 00s10.1361/105994905X75646 ↗
23. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
24. W. Gerhard, R.R. Boyer, E.W. Collings, Materials Properties Handbook: Titanium Alloys, 1994.
25. A comparative study of the mechanical properties of high-strength β-titanium alloys10.1016/j.jallcom.2007.03.070 ↗
26. Properties of TIMETAL 555 (Ti-5Al-5Mo-5V–3Cr-0.6Fe)10.1361/105994905X75628 ↗
27. Influence of solution treatment on microstructure and mechanical properties of a near β titanium alloy Ti-733310.1016/j.matdes.2015.06.015 ↗
28. Influence of phase transformation kinetics on the formation of α in a β-quenched Ti–5Al–5Mo–5V–3Cr–1Zr alloy10.1016/j.actamat.2015.05.008 ↗
29. Influence of transformation temperature on microtexture formation associated with α precipitation at β grain boundaries in a β metastable titanium alloy10.1016/j.actamat.2013.03.007 ↗
30. Correlation between alpha phase morphology and tensile properties of a new beta titanium alloy10.1016/j.matdes.2017.02.043 ↗
31. A review on heat treatment efficiency in metastable β titanium alloys: the role of treatment process and parameters10.1016/j.jmrt.2020.10.088 ↗
32. Tensile brittleness and ductility improvement in a novel metastable β titanium alloy with lamella structure10.1016/j.jallcom.2020.154311 ↗
33. Influence of strain-rate sensitivity on necking under uniaxial tension10.1016/0001-6160(77)90168-7 ↗
34. Theory of tensile test10.1016/0001-6160(67)90211-8 ↗
35. T. Zhu, J. Li, A. Samanta, H.G. Kim, S. Suresh, Interfacial plasticity governs strain rate sensitivity and ductility in nanostructured metals, Proc. Natl. Acad. Sci. 104(207), pp. 3031–3036.10.1073/pnas.0611097104 ↗
36. Toward a quantitative understanding of mechanical behavior of nanocrystalline metals10.1016/j.actamat.2007.01.038 ↗
37. Mechanical properties of nanocrystalline materials, Progr
38. E. Orowan, Proceedings of the physical society, Proc. Phys. Soc. 52(1940) 8.10.1088/0959-5309/52/1/303 ↗
39. Stress relaxation and the structure size-dependence of plastic deformation in nanotwinned copper10.1016/j.actamat.2009.07.018 ↗
40. Activation volume and density of mobile dislocations in plastically deforming nanocrystalline Ni
41. Design of high strength and wear-resistance ß-Ti alloy via oxygen-charging
42. Deformation behavior and microstructure evolution of titanium alloys with lamellar microstructure in hot working process: a review10.1016/j.jmst.2019.07.052 ↗
43. Hierarchical 3D nanolayered duplex-phase Zr with high strength, strain hardening and ductility
44. In situ TEM study of dislocation slip in a metastable β titanium alloy10.1016/j.scriptamat.2011.11.036 ↗