Microstructural evolution of near-β Ti-6Zr-5Fe alloy fabricated by selective laser melting before and after solution treatment
Source abstract
Abstract
Abstract The homogeneity of microstructure and microhardness in different parts of as-fabricated selective laser melting (SLM) and as-solutionized Ti-6Zr-5Fe alloy is presented in this paper. The results show that the as-fabricated SLM alloy has a bigger β phase and finer α phase size in the top part than that in the bottom part due to the reheating treatment during SLM process. However, as-solutionized Ti-6Zr-5Fe alloy mainly consists of β phase in the top part, and the bottom part is mainly comprised of β and α phase in the grain boundary. Apart from the change of phase composition, the β phase size in bottom part is smaller than that in the top part, due to the precipitation of α phase at the grain boundary in the bottom part. The fine α phase in the top part of as-fabricated SLM Ti-6Zr-5Fe alloy results in that the top part has a higher microhardness (518 HV) than the bottom part (394 HV). While, the microhardness becomes almost the same in the top part (482 HV) and bottom part (475 HV) after solid solution treatment. The dissolution of fine α phase in the top part and solution strengthening of Fe and Zr element in the bottom part after solution treatment improve the uniformity of microhardness. This research provides an approach for obtaining the gradient microstructure or gradient property for near-β Ti alloy samples by governing the parameters of SLM technology and solution treatment.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Mechanical properties and microstructural evolution of TA15 Ti alloy processed by selective laser melting before and after annealing10.1016/j.msea.2019.138742 ↗
2. Improved mechanical properties of the new Ti-15Ta-xZr alloys fabricated by selective laser melting for biomedical application10.1016/j.jallcom.2016.07.002 ↗
3. Microstructural homogeneity and mechanical behavior of a selective laser melted Ti-35Nb alloy produced from an elemental powder mixture10.1016/j.jmst.2020.05.052 ↗
4. On the role of laser in situ re-melting into pore elimination of Ti-6Al-4V components fabricated by selective laser melting10.1016/j.jallcom.2020.156866 ↗
5. Effects of selective laser melting build orientations on the microstructure and tensile performance of Ti-6Al-4V alloy10.1016/j.msea.2020.139001 ↗
6. Enhanced corrosion resistance of Ti-5 wt% TiN composite compared to commercial pure Ti produced by selective laser melting in HCl solution10.1016/j.jallcom.2019.153422 ↗
7. Selective laser melting of low modulus Ti-Mo alloy: α/β heterogeneous conchoidal structure10.1016/j.matlet.2020.127544 ↗
8. A novel approach to in-situ fabricate Ti-6Al-4V alloy with graded microstructure and property by selective laser melting10.1016/j.matlet.2017.12.098 ↗
9. Gradient in microstructure and mechanical property of selective laser melted AlSi10Mg10.1016/j.jallcom.2017.11.020 ↗
10. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
11. Characterization of a laser-fabricated hypereutectic Al-Sc alloy bar10.1016/j.scriptamat.2014.05.021 ↗
12. Manufacture by selective laser melting and mechanical behavior of a biomedical Ti–24Nb–4Zr–8Sn alloy10.1016/j.scriptamat.2011.03.024 ↗
13. Selective laser melting of Ti–35Nb composite from elemental powder mixture: Microstructure, mechanical behavior and corrosion behavior10.1016/j.msea.2019.06.001 ↗
14. Transformation-induced plasticity and high strength in beta titanium alloy manufactured by selective laser melting10.1016/j.mtla.2019.100299 ↗
15. Mechanical behavior and phase transformation of β-type Ti-35Nb-2Ta-3Zr alloy fabricated by 3D-Printing10.1016/j.jallcom.2019.03.138 ↗
16. Effect of heat treatment variations on the microstructure evolution and mechanical properties in a β metastable Ti alloy10.1016/j.jallcom.2016.05.225 ↗
17. Microstructural tailoring and mechanical properties of a multi-alloyed near β titanium alloy Ti-5321 with various heat treatment10.1016/j.msea.2017.11.029 ↗
18. Selective laser melting of near-α titanium alloy Ti-6Al-2Zr-1Mo-1V: parameter optimization, heat treatment and mechanical performance10.1016/j.jmst.2020.05.004 ↗
19. Study on selective laser melting and heat treatment of Ti-6Al-4V alloy10.1016/j.rinp.2018.07.008 ↗
20. Effect of heat treatment on microstructure and mechanical properties of the selective laser melting processed Ti-5Al-2.5Sn α titanium alloy10.1016/j.msea.2017.10.061 ↗
21. Microstructure and mechanical performance tailoring of Ti-13Nb-13Zr alloy fabricated by selective laser melting after post heat treatment10.1016/j.jallcom.2018.10.030 ↗
22. Effects of direct aging on near-alpha Ti-6Al-2Sn-4Zr-2Mo (Ti-6242) titanium alloy fabricated by selective laser melting (SLM)10.1016/j.msea.2020.139533 ↗
23. Microstructure and properties of a novel ternary Ti–6Zr–xFe alloy for biomedical applications10.1016/j.jallcom.2020.157119 ↗
24. Microstructure, defects and mechanical behavior of beta-type titanium porous structures manufactured by electron beam melting and selective laser melting10.1016/j.actamat.2016.04.029 ↗