journal article·2025-06

Temperature-dependent mechanical behaviors of laser powder bed fused WE43 alloy with heterogeneous grain structure: Deformation and fracture mechanisms

Chen Ji, Liang Zhu, Bangzhao Yin, Shengwen Bai, Lawrence E. Murr, Peng Wen, Bin Jiang, Fusheng Pan, Kun Li

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Metal and Thin Film Mechanics · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. Effect of multiple thermal cycles on the microstructure evolution of GA151K alloy fabricated by laser-directed energy deposition
2. Distinguished roles of static aging and strain aging in the microstructure and creep resistance of Mg-4Y-3.5Nd alloy10.1016/j.jmst.2023.07.080 ↗
3. Achieving outstanding heat-resistant Mg-Gd-Y-Zn-Mn alloy via introducing RE/Zn segregation on α-Mn nanoparticles10.1016/j.scriptamat.2023.115672 ↗
4. Research advances of magnesium and magnesium alloys worldwide in 202110.1016/j.jma.2022.04.001 ↗
5. Additive manufacturing of biodegradable metals: current research status and future perspectives10.1016/j.actbio.2019.04.046 ↗
6. The effects and utility of homogenization and thermodynamic modeling on microstructure and mechanical properties of SS316/IN718 functionally graded materials fabricated by laser-based directed energy deposition10.1016/j.jmatprotec.2023.118084 ↗
7. Laser additive manufacturing of biodegradable magnesium alloy WE43: a detailed microstructure analysis10.1016/j.actbio.2019.05.056 ↗
8. Microstructure and mechanical behavior of an additive manufactured (AM) WE43-Mg alloy
9. Microstructure evolution and mechanical properties of a high-strength Mg-10Gd-3Y-1Zn-0.4Zr alloy fabricated by laser powder bed fusion
10. A detailed microstructural and corrosion analysis of magnesium alloy WE43 manufactured by selective laser melting
11. High-temperature oxidation behavior and mechanism of Inconel 625 super-alloy fabricated by selective laser melting10.1016/j.optlastec.2020.106509 ↗
12. Defects as a root cause of fatigue weakening of additively manufactured AlSi10Mg components10.1016/j.tafmec.2020.102611 ↗
13. Laser shock peening and its effects and modeling on fatigue performance of additive manufactured metallic materials10.1016/j.tafmec.2024.104281 ↗
14. Investigation on the fracture behaviour of wire arc additive manufactured rotor steel weldments after heat treatment10.1016/j.tafmec.2022.103342 ↗
15. Microstructure and properties of a high temperature Al–Ce–Mn alloy produced by additive manufacturing10.1016/j.actamat.2020.07.014 ↗
16. Strength-plasticity transition mechanism after the solution treatment of GH3230 superalloy fabricated via laser powder bed fusion10.1016/j.msea.2023.145124 ↗
17. In-situ SEM investigation on fatigue behaviors of additive manufactured Al-Si10-Mg alloy at elevated temperature10.1016/j.engfracmech.2019.03.040 ↗
18. Anisotropic response in mechanical behavior of additively manufactured Al–Mn-Sc alloys by in-situ EBSD tensile tests10.1016/j.msea.2022.144155 ↗
19. Elevated temperature tensile behaviour of 5183 aluminium alloy made by electrospark deposition additive manufacturing10.1016/j.msea.2023.144746 ↗
20. Influence of friction stir processing and aging heat treatment on microstructure and mechanical properties of selective laser melted Mg-Gd-Zr alloy
21. Additive manufacturing of dense WE43 Mg alloy by laser powder bed fusion
22. Tensile creep mechanisms of laser powder bed fused WE43 alloy with heterogeneous microstructure: evolution in dislocations and precipitates10.1016/j.jmst.2025.02.063 ↗
23. Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Mg-11Gd-2Zn-0.4Zr alloy10.1016/j.msea.2021.142139 ↗
24. Microstructure and mechanical properties of WE43 magnesium alloy fabricated by direct-chill casting10.1016/j.msea.2016.11.009 ↗
25. Development of grain size/ texture graded microstructures through friction stir processing and subsequent cold compression of a rare earth bearing magnesium alloy10.1016/j.msea.2021.141190 ↗
26. Enhancing the strength and ductility in accumulative back extruded WE43 magnesium alloy through achieving bimodal grain size distribution and texture weakening10.1016/j.msea.2017.04.098 ↗
27. Micro and macro texture evolution during multiaxial forging of a WE43 magnesium alloy10.1016/j.jallcom.2017.12.181 ↗
28. Influence of layer thickness on formation quality, microstructure, mechanical properties, and corrosion resistance of WE43 magnesium alloy fabricated by laser powder bed fusion
29. Selective laser melting of magnesium alloys: Necessity, formability, performance, optimization and applications10.1016/j.jmst.2022.12.053 ↗
30. Effect of deformation temperature on the slip activity in pure Mg and AZX21110.1016/j.jmrt.2022.06.050 ↗
31. Precipitation and Hardening in Magnesium Alloys10.1007/s11661-012-1217-2 ↗
32. The origin of high-density dislocations in additively manufactured metals10.1080/21663831.2020.1751739 ↗
33. Effect of initial temper on the creep behavior of precipitation–hardened WE43 alloy10.1016/j.msea.2017.02.081 ↗
34. Microstructure and mechanical properties of a peak-aged Mg-5Y-2.5Nd-1.5Gd-0.5Zr casting alloy10.1016/j.jallcom.2017.09.063 ↗
35. Microstructure and elevated temperature mechanical and creep properties of Mg–4Y–3Nd–0.5Zr alloy in the product form of a large structural casting10.1016/j.matdes.2014.03.062 ↗
36. Effect of process modes on microstructure and mechanical properties of CMT wire arc additive manufactured WE43 magnesium alloy10.1016/j.jmrt.2023.10.063 ↗
37. Achieving fully equiaxed grain microstructure and isotropic mechanical properties in wire arc additive-manufactured Mg-Y-Nd-Zr alloys10.1016/j.jallcom.2023.171041 ↗
38. The influence of the LPSO on the deformation mechanisms and tensile properties at elevated temperatures of the Mg-Gd-Zn-Mn alloys10.1016/j.jmrt.2023.02.154 ↗
39. A review of dynamic recrystallization phenomena in metallic materials10.1016/j.matdes.2016.09.012 ↗
40. Construction of an Arrhenius constitutive model for Mg-Y-Nd-Zr-Gd rare earth magnesium alloy based on the Zener-Hollomon parameter and objective evaluation of its accuracy in the twinning-rich intervals
41. A new die-cast magnesium alloy for applications at higher elevated temperatures of 200–300 °C10.1016/j.jma.2020.09.012 ↗
42. Effect of temperature on the transition in deformation modes in Mg single crystals10.1016/j.actamat.2019.08.014 ↗
43. Dynamic recrystallization and twinning behavior of magnesium alloy during hot tension10.1016/j.jmrt.2023.05.056 ↗
44. On the interaction of precipitates and tensile twins in magnesium alloys10.1016/j.actamat.2019.07.046 ↗
45. In-situ analysis of the tensile deformation modes and anisotropy of extruded Mg-10Gd-3Y-0.5Zr (wt%) at elevated temperatures10.1016/j.ijplas.2016.06.001 ↗
46. Cyclic deformation behavior of a rare-earth containing extruded magnesium alloy: effect of heat treatment10.1007/s11661-014-2687-1 ↗
47. Deformation mechanism of high ductility Mg-Gd-Mn alloy during tensile process
48. Advancement of microstructural evolution and deformation mechanisms in AA6082 aluminum alloy under elevated-temperature tensile loading10.1016/j.ijplas.2024.103969 ↗
49. Deformation mechanisms in a novel multiscale hetero-structured Mg alloy with high strength-ductility synergy10.1016/j.ijplas.2023.103766 ↗
50. Clarifying the deformation modes and strengthening mechanisms of Mg-11Gd-5Y-2Zn-0.7Zr with outstanding high-temperature mechanical properties10.1016/j.msea.2023.144638 ↗
51. Microstructure and texture evolution of Mg-14Gd-0.5Zr alloy during rolling and annealing under different temperatures10.1007/s40195-022-01447-x ↗
52. High temperature mechanical properties and strain hardening mechanism of directionally solidified Mg-Gd-Y alloy10.1016/j.msea.2021.142337 ↗
53. Deformation behaviors and the related high-temperature mechanical properties of Mg-11Gd-5Y-2Zn-0.7Zr via regulating extrusion temperatures10.1016/j.jmrt.2023.07.213 ↗
54. Texture analysis of the effect of non-basal slip systems on the dynamic recrystallization of the Mg alloy AZ3110.1016/j.matchar.2012.10.002 ↗
55. Unveiling strength-plasticity synergic mechanism of AZ91 alloy during multi-DOF forming10.1016/j.jmst.2024.02.004 ↗
56. Effect of long-period ordered stacking on twinning behavior and mechanical properties of Mg-Al-Y alloy during uniaxial hot compression10.1016/j.jmst.2022.09.041 ↗
57. Activation of non-basal slip in multicomponent Mg alloys10.1016/j.jma.2021.03.007 ↗
58. Effects of temperature on critical resolved shear stresses of slip and twining in Mg single crystal via experimental and crystal plasticity modeling10.1016/j.jma.2023.04.007 ↗
59. Fatigue and dynamic aging behavior of a high strength Al-5024 alloy fabricated by laser powder bed fusion additive manufacturing10.1016/j.actamat.2021.117312 ↗
60. On the excellent strength-ductility synergy of wire-arc directed energy deposited Mg-Gd-Y-Zn-Zr alloy via manipulating precipitates
61. Dynamic recrystallization based ductile fracture modeling in hot working of metallic materials10.1016/j.ijplas.2017.04.002 ↗
62. Microstructural evolution and strengthening mechanism of Mg-Y-RE-Zr alloy fabricated by quasi-directed energy deposition
63. Dynamic precipitation and deformation behaviors of a bimodal-grained WE43 alloy with enhanced mechanical properties10.1016/j.ijplas.2023.103682 ↗
64. Coarsening- and creep resistance of precipitation-strengthened Al–Mg–Zr alloys processed by selective laser melting10.1016/j.actamat.2020.02.008 ↗
65. Perspective on hetero-deformation induced (HDI) hardening and back stress10.1080/21663831.2019.1616331 ↗