journal article·2024-12

Fracture toughness and fracture mechanism of Al-Mg-Si alloy sheet subjected to pre-cryorolling and subsequent bake hardening

Jianrui Xing, Gang Lei, Zhengyu Wang, Huijie Cui, Charlie Kong, Hailiang Yu

Publisher page

Abstract

The fracture toughness of AA6061 sheets subjected to pre-cryorolling and room-temperature pre-rolling with varying reductions (5 %, 10 %, 15 %, and 20 %) followed by bake hardening was investigated. In the direction parallel to the rolling direction (R-T), the unit crack initiation energy (UIE) of the pre-cryorolled samples after bake hardening exhibited an increase of 0.8–6 % compared to samples without pre-rolling. In contrast, the UIE of the room-temperature pre-rolled samples displayed a varying degree of decrease. This difference can be attributed to the smaller mean grain size in the pre-cryorolled samples compared to the room-temperature pre-rolled samples. Due to work hardening, the crack propagation resistance of the pre-rolled samples was diminished, as evidenced by a decrease in crack propagation energy (UPE) with increasing reduction. The variation trends of UIE and UPE in the direction perpendicular to the rolling direction (T-R) were similar to those observed in the R-T direction. The fracture mechanism of the samples during the tearing process involves a combination of intergranular and transgranular fractures. However, samples in the R-T direction exhibit higher resistance to crack propagation compared to those in the T-R direction, which is reflected in the larger UIE and UPE. The greater resistance in the R-T direction can be attributed to the significant elongation of grains prior to fracture, resulting in a higher degree of plastic deformation in the region near the crack. Additionally, the proportion of transgranular fracture along the crack propagation path is greater in the R-T direction.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and mechanical properties · Microstructure and Mechanical Properties of Steels · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Change in the structure and mechanical properties of Al–Mg–Si alloys caused by the addition of other elements: A comprehensive review10.1016/j.jmrt.2023.09.220 ↗
2. The combined effect of pre-aging and Mg/Si ratio on the natural aging and bake hardening in Al-Mg-Si-0.7Cu alloys10.1016/j.matchar.2024.113987 ↗
3. Hardness reversal in severely deformed automotive Al-Mg-Si alloys10.1016/j.jallcom.2024.173515 ↗
4. An investigation on damage tolerant design parameter of additively manufactured Al 2024: Fatigue crack growth rate and fracture toughness
5. The conflicts between strength and toughness10.1038/nmat3115 ↗
6. Synchronously enhancing the strength, toughness, and stress corrosion resistance of high-end aluminum alloys via interpretable machine learning10.1016/j.actamat.2024.119873 ↗
7. Making selective-laser-melted high-strength Al–Mg–Sc–Zr alloy tough via ultrafine and heterogeneous microstructure10.1016/j.scriptamat.2021.114052 ↗
8. Characterization and micromechanical modelling of microstructural heterogeneity effects on ductile fracture of 6xxx aluminium alloys10.1016/j.actamat.2015.10.008 ↗
9. A study on fracture toughness and strain rate sensitivity of severely deformed Al 6063 alloys processed by multiaxial forging and rolling at cryogenic temperature10.1016/j.msea.2017.01.035 ↗
10. On the influence of specimen size and geometry on the fracture toughness of tungsten heavy metal alloys10.1016/j.jnucmat.2022.154025 ↗
11. Mode I fracture toughness with fiber bridging of unidirectional composite laminates under cryogenic temperature10.1016/j.compscitech.2023.110386 ↗
12. Effect of notch depth ratio and specimen width on mode II fracture properties of ECC
13. Effect of support friction on pure mode I, II, and III fracture toughness of cement concrete tested with edge-notched disc bend specimen10.1016/j.tafmec.2023.104247 ↗
14. Three-dimensional numerical study of thickness effect on plastic CTOD and monotonic plastic zone in an aluminium CT specimen10.1016/j.tafmec.2023.104132 ↗
15. Analysis of dynamic fracture propagation in steel pipes using a shell-based constant-CTOA fracture model10.1016/j.ijpvp.2022.104677 ↗
16. Experimental evaluation of J-integral in elastic and elastic–plastic polymers by means of digital image correlation and higher-order eigenfields under mode-I10.1016/j.engfracmech.2023.109534 ↗
17. A strong fracture-resistant high-entropy alloy with nano-bridged honeycomb microstructure intrinsically toughened by 3D-printing10.1038/s41467-024-45178-2 ↗
18. Elastic-plastic fracture toughness of metastable, dual-phase, Fe49.5Mn30Co10Cr10C0.5, high entropy alloy (HEA)10.1016/j.matlet.2023.135094 ↗
19. Influence of microstructure and porosity on the fracture toughness of Al-Si-Mg alloy10.1016/j.jmrt.2019.11.055 ↗
20. Effect of composition on tensile properties and fracture toughness of Al–Zn–Mg alloy (A7N01S-T5) used in high speed trains10.1016/j.matdes.2015.11.107 ↗
21. Plane stress fracture toughness of cryorolled 6082 Al alloy10.1016/j.tafmec.2018.02.011 ↗
22. Effect of three-dimensional deformation at different temperatures on microstructure, strength, fracture toughness and corrosion resistance of 7A85 aluminum alloy10.1016/j.jallcom.2022.167200 ↗
23. 2013
24. Identification of fracture toughness parameters to understand the fracture resistance of advanced high strength sheet steels10.1016/j.engfracmech.2020.106949 ↗
25. Effect of minor Mn addition on microstructure and fracture toughness of Al-Zn-Mg-Zr alloy sheet
26. The effect of Ag on the tensile strength and fracture toughness of novel Al-Mg-Zn alloys10.1016/j.jallcom.2022.164640 ↗
27. Preparation of high-mechanical-property medium-entropy CrCoNi alloy by asymmetric cryorolling10.1016/S1003-6326(22)65893-X ↗
28. Edge-crack free and high mechanical properties of AA7075 sheets by using cryorolling and subsequent aging10.1016/j.jallcom.2022.167556 ↗
29. The microstructure evolution and strengthening mechanism of fine-grained Al–Mn alloy with nanoscale precipitates during cryorolling10.1016/j.msea.2024.146680 ↗
30. High strength and toughness of Ti–6Al–4V sheets via cryorolling and short-period annealing10.1016/j.msea.2022.143766 ↗
31. Achieving High Strength and Tensile Ductility in Pure Nickel by Cryorolling with Subsequent Low-Temperature Short-Time Annealing10.1016/j.eng.2023.01.019 ↗
32. Experimental and computational investigation of fracture toughness of cryo-rolling processed Al-6082 alloys10.1016/j.engfailanal.2024.108005 ↗
33. Effect of Room-Temperature Pre-rolling and Pre-cryorolling on Natural Aging and Bake Hardening Response of an Al–Mg–Si Alloy10.1007/s11661-023-07150-5 ↗
34. Effect of hot rolling finishing temperature and intermediate annealing on the microstructure, texture evolution, and comprehensive properties of Al-Mg-Si alloy10.1016/j.jallcom.2023.172525 ↗
35. Influence of asymmetric rolling on the microstructure, texture evolution and mechanical properties of Al–Mg–Si alloy10.1016/j.msea.2022.143154 ↗
36. Dislocation density-mediated creep ageing behavior of an Al-Cu-Li alloy10.1016/j.jmst.2023.08.011 ↗
37. Enhanced age-hardening of an Al–5Mg–2Zn–1Cu alloy by pre-aging combined with pre-straining10.1016/j.msea.2023.145410 ↗
38. Cluster evolution mechanisms during aging in Al–Mg–Si alloys10.1016/j.actamat.2015.09.027 ↗
39. Detailed atomistic insight into the β″ phase in Al–Mg–Si alloys10.1016/j.actamat.2014.01.052 ↗
40. Strength and biaxial formability of cryo-rolled 2024 aluminium subject to concurrent recovery and precipitation10.1016/j.actamat.2013.05.019 ↗
41. The role of intermetallic particles on mode I crack propagation mechanisms in metal plates10.1016/j.engfracmech.2021.107901 ↗
42. The effect of aging process on the microstructure and mechanical properties of a Cu–Be–Co–Ni alloy10.1016/j.matdes.2015.06.157 ↗
43. The influenced zones of stress intensity factor and plasticity at multi-crack tips10.1016/j.tafmec.2023.103978 ↗
44. Notch tip plastic zone determination by extending Irwin’s model10.1016/j.tafmec.2020.102643 ↗
45. Modulating fracture toughness through processing-mediated mesostructure in additively manufactured Al-12Si alloy10.1016/j.matdes.2022.110440 ↗
46. Void growth based inter-granular ductile fracture in strain gradient polycrystalline plasticity10.1016/j.ijplas.2021.103123 ↗
47. On the role of grain structure and crystal orientation in governing fatigue crack propagation behavior of Al-Cu-Li alloy10.1016/j.jallcom.2023.169317 ↗
48. Effects of grain structures on fatigue crack propagation behavior of an Al-Cu-Li alloy10.1016/j.ijfatigue.2023.107927 ↗
49. Effect of crystal orientation and texture on fatigue crack evolution in high strength steel welds10.1016/j.ijfatigue.2015.03.008 ↗
50. Schmid factor crack propagation and tracking crystallographic texture markers of microstructural condition in direct energy deposition additive manufacturing of Ti-6Al-4V
51. Effect of Microstructural Characteristics on Fracture Toughness in Direct Energy Deposited Novel Ti-6Al-4V-1Mo Alloy10.1007/s40195-023-01650-4 ↗
52. Fracture of ECAP-deformed iron and the role of extrinsic toughening mechanisms10.1016/j.actamat.2013.01.057 ↗