Effect of annealing on the corrosion-fatigue strength and hot salt corrosion resistance of fine-grained titanium near-α alloy Ti-5Al-2V obtained using Rotary Swaging
Source abstract
Abstract
The corrosion-fatigue strength in 3% aqueous NaCl solution and the resistance against hot salt corrosion (HSC) of the fine-grained near-a alloy Ti-5Al-2V (Russian analog of Grade 9 titanium alloy with increased aluminum content) has been studied. The properties of the Ti-5Al-2V alloy in the coarse-grained state, in the fine-grained after cold Rotary Swaging (RS), in partly recrystallized state, and in fully recrystallized one have been investigated. The mechanical properties of the alloy were characterized using compression tests and microhardness measurements. The effects of RS and of the annealing temperature and time on the character of corrosion destruction of the surface and on the composition of the products of the HSC were studied. RS was shown to result in an increase in the depth of the intergranular corrosion defects while the recrystallization annealing promotes the increasing of the corrosion resistance of the Ti-5Al-2V titanium alloy. The parameters of the Basquin equation for the corrosion-fatigue curves for the near-a Ti-5Al-2V alloy in the coarse-grained state, in the severely strained one, and after recrystallization annealing were determined for the first time. An effect of nonmonotonous dependencies of the slopes of the corrosion-fatigue curves for the strained near-a Ti-5Al-2V alloy on the recrystallization annealing temperature has been observed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. I.V. Gorynin, B.B. Chechulin, Titan in Mechanical Engineering, Mashinostroenie, Moscow, Russia, 1990. (In Russian).
2. Marine titanium alloys: Present and future10.1134/S2075113315060106 ↗
3. Titanium alloys for marine application10.1016/S0921-5093(98)01180-0 ↗
4. Understanding the “blue spot”: Sodium chloride hot salt stress-corrosion cracking in titanium-6246 during fatigue testing at low pressure10.1016/j.engfailanal.2015.06.008 ↗
5. Effect of streaming water vapor on the corrosion behavior of Ti60 alloy under solid NaCl deposit in water vapor at 600 °C10.1016/j.corsci.2019.108177 ↗
6. Chevrot, T. Pressure Effects on the Holt-Salt Stress-Corrosion Cracking of Titanium Alloys. Ph.D. Thesis, Cranfield University, Bedford, UK, 1994.
7. The mechanisms of hot salt stress corrosion cracking in titanium alloy Ti-6Al-2Sn-4Zr-6Mo10.1016/j.corsci.2018.02.025 ↗
8. Hot-salt-stress-corrosion cracking of titanium alloys10.1016/0010-938X(78)90015-X ↗
9. Hot salt stress corrosion cracking of titanium alloys: An improved model for the mechanism10.5006/0010-9312-33.7.252 ↗
10. Hot-salt stress-corrosion of titanium: A review of the problem and methods for improving the resistance of titanium10.1007/BF03355696 ↗
11. AgCl-induced hot salt stress corrosion cracking in a titanium alloy10.1016/j.corsci.2021.109497 ↗
12. Effect of salt corrosion on the endurance strength of pseudoalfa-titanium alloys10.1007/BF00715257 ↗
13. Thermodynamic analysis of the chemical mechanism for the hot-salt corrosion of titanium alloys10.1007/BF00716248 ↗
14. The stress-corrosion cracking susceptibility of near-α titanium alloy IMI 834 in presence of hot salt10.1016/j.corsci.2014.01.013 ↗
15. Environmentally assisted fatigue crack nucleation in Ti-6Al-2Sn-4Zr-6Mo10.1016/j.corsci.2015.03.013 ↗
16. The effect of NaCl-induced corrosion on Ti60’s hot salt stress corrosion cracking10.1016/j.corsci.2023.111677 ↗
17. Effect of NaCl-rich environment on internal corrosion for Ti60 alloy at 600 °C
18. The influence of alloying on the tendency of titanium alloys towards salt corrosion10.1007/BF00722899 ↗
19. Effect of aluminium on the susceptibility of titanium to corrosion by salt10.1007/BF00721765 ↗
20. Degradation mechanism of Ti-6Al-2Sn-4Zr-2Mo-Si alloy exposed to sold NaCl deposit at high temperature10.1016/j.corsci.2020.108611 ↗
21. Salt corrosion of titanium alloys10.1007/BF00652203 ↗
22. Hot salt corrosion behavior of Ti-6Al-4V alloy treated with different surface deformation strengthening processes10.1016/j.matchemphys.2023.128410 ↗
23. Effect of the ultrasonic surface rolling process and plasma electrolytic oxidation on the hot salt corrosion fatigue behavior of TC11 alloy10.1016/j.ijfatigue.2022.107443 ↗
24. Hot corrosion behavior of TC11 titanium alloy treated by laser shock processing10.1016/j.apsusc.2013.07.017 ↗
25. Effect of abrasive water jet peening of NaCl-induced hot corrosion behavior of Ti-6Al-4V10.1016/j.vacuum.2023.111872 ↗
26. Hot corrosion behaviour of Ti-6Al-4V modified by ultrasonic shot peening10.1016/j.matdes.2016.07.133 ↗
27. Hot salt stress corrosion resistance of Ti 6246 alloy10.1016/S0010-938X(98)00028-6 ↗
28. NaCl induced corrosion of Ti-6Al-4V alloy at high temperature10.1016/j.corsci.2016.04.016 ↗
29. Hot salt stress corrosion cracking behavior of Ti-6242S alloy10.1007/s11661-015-3155-2 ↗
30. Effect of pre-hot salt corrosion on hot salt corrosion fatigue behavior of the TC11 titanium alloy at 500 °C10.1016/j.ijfatigue.2022.107055 ↗
31. Effect of hot corrosion on cycle deformation and fracture behavior of Ti-6Al-4V alloy under salt coating10.1016/j.corsci.2023.111545 ↗
32. Effect of long term exposure and hydrogen effects on HSSCC behavior of titanium alloy IMI 83410.1016/j.matdes.2015.08.002 ↗
33. A cracking oxygen story: A new view of stress corrosion cracking in titanium alloys10.1016/j.actamat.2022.117687 ↗
34. Hot corrosion resistance of TB8 titanium alloy after ECAP and heat treatment10.1007/s11595-023-2840-z ↗
35. Study of mechanical properties and corrosive resistance of ultrafine-grained α-titanium alloy Ti-5Al-2V10.1016/j.jallcom.2017.06.220 ↗
36. Effect of severe plastic deformation realized by rotary swaging on the mechanical properties and corrosion resistance of near-α-titanium alloy Ti-2.5Al-2.6Zr10.1016/j.jallcom.2019.01.268 ↗
37. Corrosion fatigue crack initiation in ultrafine-grained near-α titanium alloy PT7M prepared by Rotary Swaging10.1016/j.jallcom.2019.03.146 ↗
38. Principles of equal-channel angular pressing as a processing tool for grain refinement10.1016/j.pmatsci.2006.02.003 ↗
39. Cyclic behavior of ultrafine-grain titanium produced by severe plastic deformation10.1016/S0921-5093(01)01262-X ↗
40. Strength and ductility-related properties of ultrafine grained two-phase titanium alloy produced by warm multiaxial forging10.1016/j.msea.2011.12.102 ↗
41. Enhanced corrosion behavior of ultrafine-grained pure titanium in simulated high-temperature seawater10.1016/j.jmrt.2022.05.032 ↗
42. Corrosion behavior of pure titanium processed by rotary-die ECAP10.1016/j.jmrt.2021.09.047 ↗
43. Stress corrosion cracking of ultrafine-grained Ti-2Fe-0.1B alloying after equal channel angular pressing10.3390/met13071316 ↗
44. Superplastic deformation behavior of Ti-4Al-2V alloy governed by its structure and precipitation phase evolution10.1016/j.msea.2018.06.094 ↗
45. Superplastic deformation behavior of ultra-fine-grained Ti-1V–4Al-3Mo alloy: constitutive modeling and processing map10.1088/2053-1591/ab31f9 ↗
46. Influence of low-temperature annealing time on the evolution of the structure and mechanical properties of a titanium Ti-Al-V alloy in the submicrocrystalline state10.1134/S0031918X15030114 ↗
47. Spark Plasma Sintering for high-speed diffusion bonding of the ultrafine-grained near-α Ti-5Al-2V alloy with high strength and corrosion resistance for nuclear engineering10.1007/s10853-019-03926-6 ↗
48. Corrosion resistance of the weld joints from the ultrafine-grained near-α titanium alloys Ti-5Al-2V obtained by Spark Plasma Sintering10.3390/met13040766 ↗
49. A review of mechanical properties and microstructure of ultrafine grained metals and alloys processed by rotary swaging10.1016/j.jallcom.2021.163122 ↗
50. Nano-gradient materials prepared by rotary swaging10.3390/nano11092223 ↗
51. Structural-phase state and mechanical properties of β titanium alloy produced by rotary swaging with subsequent aging10.1016/j.jallcom.2022.167973 ↗
52. Structural phenomena introduced by Rotary Swaging: A review10.3390/ma17020466 ↗
53. Irradiation behavior of Ti-4Al-2V (ПТ-3В) alloy for ITER
54. Effect of σ-phase on the strength, stress relaxation behavior, and corrosion resistance of an ultrafine-grained austenitic steel AISI 32110.3390/met13010045 ↗
55. The exponential law of endurance tests
56. Hot-salt corrosion of alloys PT-7M, 42XHM, Inconel 690 and Incoloy 80010.18572/2619-0141-2019-1-23-31 ↗
57. Structure, phase composition and mechanical properties of hot-extruded Ti-3Al-2.5V pipe after vacuum annealing10.1007/s11015-019-00885-w ↗
58. Evolution of texture and tensile properties of cold-rotary swaged Ti-6Al-4V alloy seamless tubing after annealing at different temperatures10.1016/j.msea.2022.143003 ↗
59. J.A. Fellows, Fractography and Atlas of Fractographs, Metals Handbook, Metals Park, Ohio: Am. Soc. Met., 1974.
60. Segal · 2010
61. A theoretical model of grain boundary self-diffusion in metals with phase transitions (case study into titanium and zirconium)10.1016/j.physb.2018.01.069 ↗
62. Lütjering · 2007
63. Investigation of the processes of fatigue and corrosion-fatigue destruction of pseudo-α titanium alloy10.1134/S2075113322020290 ↗
64. Research progress on the corrosion behavior of titanium alloys10.1515/corrrev-2022-0031 ↗