In this paper, three different W/W-Cu joints (W/W-16Cu (joint 1), W/FeCoNiCrCu interlayer/W-16Cu (joint 2), and continuous graded W-Cu (pure W∼W-16 Cu)/W-52Cu (joint 3)), were prepared by tape casting and infiltration using W and graded W skeleton as substrates. Thermal shock tests at temperature of 800 °C-RT were conducted for the W/W-Cu joints. The microstructure and properties evolution, and damage behavior of the joints under thermal shock were studied by experiment combing with finite element modelling. The results show that, after thermal shock, a crack through the interface is found in joint 1. In joint 2, a main crack originates from the edge of the interface (the position of the maximum thermal stress) and extends inward, and some microcracks occur in the W side near the interface in joint 2. But there is no obvious crack in joint 3. Joint 2 has the highest initial shear strength of 287 MPa, and the joint 3 has the highest residual shear strength. After 150 thermal shocks, the shear strength of joint 3 decreases from 268 MPa to 185 MPa, and the strength loss rate is 30.97 %, while the loss rates of joint 1 and joint 2 are more than 70 %.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Fusion materials and technologies · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Engineering challenges and development of the ITER blanket system and divertor10.1016/j.fusengdes.2015.06.045 ↗
2. Design optimization of the ITER tungsten divertor vertical targets10.1016/j.fusengdes.2017.12.007 ↗
3. Overview of the present progress and activities on the CFETR10.1088/1741-4326/aa686a ↗
4. European DEMO divertor target: operational requirements and material-design interface10.1016/j.nme.2016.02.005 ↗
5. Characterization on the melting failure of CuCrZr cooling tube of W/Cu monoblocks during plasma operations in EAST
6. Status of technology R&D for the ITER tungsten divertor monoblock10.1016/j.jnucmat.2014.12.027 ↗
7. Evolution of mechanical performance with temperature of W/Cu and W/CuCrZr composites for fusion heat sink applications10.1016/j.msea.2017.12.054 ↗
8. W–Cu composites with submicron- and nanostructures: progress and challenges10.1038/s41427-019-0179-x ↗
9. High-strength vacuum diffusion bonding of Cu-plated, sandblasted W and CuCrZr alloy10.1016/j.jmrt.2021.11.069 ↗
10. Optimization of the chamfering structures for ITER-like W/Cu monoblocks to avoid the leading edge-induced melting in EAST10.1016/j.fusengdes.2020.111951 ↗
11. Fabrication of W-Cu functionally graded composites using high energy ball milling and spark plasma sintering for plasma facing components10.1016/j.apt.2020.07.015 ↗
12. Performance assessment of thick W/Cu graded interlayer for DEMO divertor target10.1016/j.fusengdes.2020.111610 ↗
13. Preparation of W–Cu functionally graded material coated with CVD–W for plasma-facing components10.1016/j.jnucmat.2013.01.326 ↗
14. Performance assessment of thick W/Cu graded interlayer for DEMO divertor target10.1016/j.fusengdes.2020.111610 ↗
15. Fabrication of W-Cu functionally graded composites using high energy ball milling and spark plasma sintering for plasma facing components10.1016/j.apt.2020.07.015 ↗
16. composite with an amorphous W–Fe coated copper foil through hot pressing method10.1016/j.matdes.2012.05.057 ↗
17. Vacuum diffusion bonding W to W-Cu composite: Interfacial microstructure and mechanical properties10.1016/j.vacuum.2019.03.060 ↗
18. Achieving high-strength W/W-10Cu joints by vacuum diffusion bonding with FeCoCu interlayer10.1016/j.fusengdes.2023.113553 ↗
19. Direct tape casting of Al2O3/AlN slurry for AlON transparent ceramic wafers via one-step reaction sintering10.1016/j.jeurceramsoc.2023.01.056 ↗
20. Tape casting coupled with isostatic pressing as an alternative fabrication method for microtubular solid oxide fuel cells10.1016/j.ijhydene.2022.01.053 ↗
21. Large-area anode-supported protonic ceramic fuel cells combining with multilayer-tape casting and hot-pressing lamination technology10.1016/j.jeurceramsoc.2022.09.057 ↗
22. Improved parallelism of graded W–Cu–SiC materials by adjusting the coefficient of thermal expansion10.1016/j.ceramint.2019.12.239 ↗
23. Fabrication of W/Cu FGM by aqueous tape casting
24. Thermal and mechanical properties of infiltrated W/CuCrZr composite materials for functionally graded heat sink application10.1016/j.jnucmat.2013.03.005 ↗
25. Continuous W Cu functional gradient material from pure W to W Cu layer prepared by a modified sedimentation method10.1016/j.net.2022.08.002 ↗
26. Theoretical analysis on the damages for tungsten plasma facing surface under superposition of steady-state and transient heat loads10.1016/j.fusengdes.2018.05.054 ↗
27. Numerical assessment of functionally graded tungsten/steel joints for divertor applications10.1016/j.fusengdes.2010.12.084 ↗
28. Optimization of W/Cu monoblock mock-up with FGM interlayer for CFETR devertor targets10.1016/j.fusengdes.2019.111262 ↗
29. Micromechanical modelling of functionally graded W-Cu materials for divertor plate components in a fusion reactor10.4028/www.scientific.net/MSF.308-311.603 ↗
30. The diffusion behaviors at the Cu-Al solid-liquid interface: a molecular dynamics study10.1016/j.rinp.2020.102998 ↗