Effects of Mg content on microstructure, mechanical properties and fracture behavior of wrought Al–8Si–(<0.01–1.32)Mg alloy sheets in T6 temper
Source abstract
Abstract
In this paper, the effects of the Mg content on the microstructure, mechanical properties and fracture behavior of wrought Al–8Si–(<0.01–1.32)Mg (mass fraction, %) alloy sheets in T6 temper were systematically studied by OM, SEM/EDS, EBSD, LSCM, DSC, TEM and tensile tests. The results show that the size of Si particles decreased slightly with the increase of Mg content, and the recrystallized grain size of experimental alloy sheets was refined from about 16 µm to about 11 µm. The size of β" phases did not change obviously, but its volume fraction increased gradually and then became stable. When Mg content was 1.32%, there were many associated aggregation areas of Mg 2 Si particles and Si particles in alloy sheet. In addition, the strength of experimental alloy sheets showed an initial increase followed by a slight decrease as the Mg content increased, while the elongation gradually decreased. The finite element model accurately predicted the yield strength of Al–8Si–(<0.01–1.32)Mg alloy sheets in T6 temper, and the model was able to quantify the contribution of various strengthening mechanisms to the yield strength of the alloy sheets. The predicted results were in good agreement with the actual measured results. The tensile fracture mode of Al–8Si alloy sheet was ductile fracture. When Mg content was greater than 0.51%, the fracture pattern of the sheets comprised a combination of ductile and brittle fractures. With the increase of Mg content, the number of dimples in experimental alloy sheets increased slightly, the depth gradually became shallow and the size slightly decreased. Meanwhile, most secondary cracks on the surface of the Al–8Si alloy sheets after tensile fracture bypassed the Si particles and a few sheared the Si particles. With the Mg content gradually increasing to 0.78%, the number of Si particles sheared by secondary cracks gradually increased. However, When Mg content was 1.32%, the intergranular fracture phenomenon of Al–8Si–1.32Mg in T6 temper was weakened or even disappeared. There were multiple particles embedded in the same dimples in the tensile fracture. The particles in the associated aggregation areas were more easily broken.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Metal Forming Simulation Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Characterization of nanostructures in a high pressure die cast Al–Si–Cu alloy10.1016/j.actamat.2021.117500 ↗
2. Microstructure and strength analysis of eutectic Al–Si alloy in-situ manufactured using selective laser melting from elemental powder mixture10.1016/j.jallcom.2016.08.249 ↗
3. Evolution of microstructure and mechanical properties in a hypoeutectic Al–Si–Mg alloy processed by accumulative back extrusion10.1016/j.msea.2015.10.066 ↗
4. Microstructure, tensile properties and fracture behavior of high temperature Al–Si–Mg–Cu cast alloys10.1016/j.msea.2013.03.084 ↗
5. Interactions between Fe-rich intermetallics and Mg–Si phase in Al–7Si–xMg alloys10.1016/j.jallcom.2019.01.352 ↗
6. Characterization of externally solidified crystals in a high-pressure die-cast AlSi10MnMg alloy and their effect on porosities and mechanical properties
7. Microscopic strength of silicon particles in an aluminium–silicon alloy10.1016/j.actamat.2015.12.006 ↗
8. Precipitation hardening in Al–Mg–Si alloys with and without excess Si10.1016/S0921-5093(01)01247-3 ↗
9. Precipitation sequence of a SiC particle reinforced Al–Mg–Si alloy composite10.1007/s11665-016-2370-3 ↗
10. The effect of Mg and Si content on the microstructure, texture and bendability of Al–Mg–Si alloys10.1016/j.msea.2021.141199 ↗
11. Multiple precipitation pathways in an Al–7Si–0.6 Mg alloy fabricated by selective laser melting10.1016/j.scriptamat.2018.09.045 ↗
12. Nano-scale characterisation of sheared beta" precipitates in a deformed Al–Mg–Si alloy10.1038/s41598-019-53772-4 ↗
13. Precipitation phenomena in ultrafine grained Al–Mg–Si alloy with heterogeneous microstructure10.1016/j.actamat.2015.10.030 ↗
14. Shearing and rotation of beta'' and beta' precipitates in an Al-Mg-Si alloy under tensile deformation: In-situ and ex-situ studies
15. Hardening response and precipitation behavior of Al–7%Si–0.3%Mg alloy in a pre-aging process10.1016/j.msea.2012.10.041 ↗
16. Effect of Mg level on the microstructure and mechanical properties of die-cast Al–Si–Cu alloys10.1016/j.msea.2015.07.008 ↗
17. The effects of Mg addition on the microstructure and mechanical properties of thixoformed Al–5%Si–Cu alloys10.1016/j.jallcom.2014.09.152 ↗
18. The effect of Mg on the structure and properties of Type 319 aluminum casting alloys10.1016/j.actamat.2008.11.021 ↗
19. Effect of Mg content on age-hardening response, tensile properties, and microstructures of a T5-treated thixo-cast hypoeutectic Al–Si alloy10.1016/j.msea.2020.140089 ↗
20. Damage by eutectic particle cracking in aluminum casting alloys A356/35710.1007/s11661-003-0190-1 ↗
21. Effect of chemical compositions on tensile behaviors of high pressure die-casting alloys Al–10Si–yCu–xMn–zFe
22. The effect of scandium addition on microstructure and mechanical properties of Al–Si–Mg alloy: a multi-refinement modifier10.1016/j.matchar.2015.10.030 ↗
23. Tensile properties and deformation behaviors of a new aluminum alloy for high pressure die casting10.1016/j.jmst.2016.02.013 ↗
24. High- and low-cycle fatigue influence of silicon, copper, strontium and iron on hypo-eutectic Al–Si–Cu and Al–Si–Mg cast alloys used in cylinder heads10.1016/j.ijfatigue.2016.02.017 ↗
25. Influence of microstructure on deformation behavior and fracture mode of Al–Mg–Si alloys10.1016/S0921-5093(02)00456-2 ↗
26. Effect of loading condition and stress state on damage evolution of silicon particles in an Al–Si–Mg-base cast alloy10.1007/s11661-002-0117-2 ↗
27. Formation of phases and microstructures in Al–8Si alloys with different Mg content10.3390/ma14040762 ↗
28. Dynamic recrystallization behavior of particle reinforced Mg matrix composites fabricated by stir casting10.1016/j.msea.2012.02.077 ↗
29. Modeling of the dynamic recrystallization behavior of Csf/AZ91D magnesium matrix composites during hot compression process10.1016/j.jallcom.2017.03.010 ↗
30. Effects of reinforced particles on dynamic recrystallization of Mg base alloys during hot extrusion10.1016/S1875-5372(14)60138-7 ↗
31. The diffraction patterns from β″ precipitates in 12 orientations in Al–Mg–Si alloy10.1016/j.scriptamat.2010.01.039 ↗
32. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
33. Influence of predeformation and ageing of an Al–Zn–Mg alloy—II. Modeling of precipitation kinetics and yield stress10.1016/S1359-6454(98)00296-1 ↗
34. Coupled precipitation and yield strength modelling for non-isothermal treatments of a 6061 aluminium alloy10.1016/j.actamat.2013.09.041 ↗
35. A yield strength model for the Al–Mg–Si–Cu alloy AA611110.1016/S1359-6454(03)00028-4 ↗
36. Effects of heat treatments on the microstructure and mechanical properties of a 6061 aluminium alloy10.1016/j.msea.2010.12.011 ↗
37. Modeling the strengthening response to aging process of heat-treatable aluminum alloys containing plate/disc- or rod/needle-shaped precipitates10.1016/S0921-5093(02)00398-2 ↗
38. Process model to predict yield strength of AA6063 alloy10.1016/j.msea.2015.07.070 ↗
39. Modeling the precipitation kinetics and tensile properties in Al–7Si–Mg cast aluminum alloys10.1016/j.msea.2016.12.042 ↗
40. Precipitation strengthening of the aluminum alloy AA611110.1007/s11661-003-0191-0 ↗
41. Effect of equal-channel angular extrusion on mechanical and wear properties of eutectic Al–12Si alloy10.1016/j.matdes.2009.08.004 ↗
42. Hot deformation behavior and processing map of Al–Si–Mg alloys containing different amount of silicon based on Gleebe-3500 hot compression simulation10.1016/j.matdes.2014.08.021 ↗
43. Modelling yield strength of heat treated Al–Si–Mg casting alloys10.1179/1743133611Y.0000000021 ↗
44. Effects of grain size and dislocation density on strain hardening behavior of ultrafine grained AA1050 processed by accumulative roll bonding10.1016/j.jallcom.2015.11.032 ↗