Electron beam freeform fabrication of Ti6Al4V alloy and the role of post-heat treatment in the microstructure, texture, and mechanical properties
Source abstract
Abstract
Electron beam freeform fabrication (EBF 3) is a promising manufacturing technique to fabricate large-scale and fully-dense metallic components, showing broad potential applications in the aerospace industry. A Ti6Al4V alloy block was produced using the EBF 3 process at an ultra-fast wire feeding rate (3.5 m/min), and the role of post-heat treatments in the microstructure, texture, and mechanical properties was investigated. The results revealed that the as-deposited alloy was characterized by the large columnar prior β grains and the inhomogeneous periodic microstructures. Duplex annealing was considered to be an optimal post-heat treatment candidate to tune the as-deposited microstructure, although the columnar prior β grains maintain. Annealing at 950 ℃ for 1 h followed by air cooling created a unique bimodal microstructure consisting of coarse crab-like primary α and fine lamellar secondary α laths, and then secondary annealing at 630 ℃ for 2 h followed by air cooling facilitated the increased volume fraction of secondary α phase, thereby weakening the α texture. Such microstructure and texture evolution are favorable to a superior and isotropic overall tensile property. The ultimate tensile strength (UTS), yield strength (YS) and tensile fracture elongation (EL) were 889 MPa (transverse direction, TD)/875 MPa (verticle direction, VD), 821 MPa (TD)/801 MPa (TD) and 7.6% (TD)/8.1% (TD), respectively. Overall, the results offer a reasonable reference to the optimization in the microstructure and mechanical performance of EBF 3-ed Ti6Al4V alloy.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Additive manufacturing of metallic components- process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. Additive manufacturing of Ti6Al4V alloy: a review
3. Predicting tensile properties of Ti-6Al-4V produced via directed energy deposition10.1016/j.actamat.2017.05.025 ↗
4. Alleviating plastic anisotropy of boron modified titanium alloy by constructing layered structure via electron beam directed energy deposition
5. Wire-fed electron beam directed energy deposition of Ti-6Al-2Zr-1Mo-1V alloy and the effect of annealing on the microstructure, texture, and anisotropy of tensile properties
6. Microstructure and mechanical properties of Ti-6Al-4V alloy fabricated using electron beam freeform fabrication10.1016/j.vacuum.2019.06.030 ↗
7. Microstructure and mechanical properties of Ti-6Al-4V by electron beam rapid manufacturing10.1016/S1875-5372(14)60083-7 ↗
8. A substrate material and thickness influence on the 3D-printing of Ti-6Al-4V components via wire-feed electron beam additive manufacturing10.1016/j.jmrt.2021.12.024 ↗
9. Effect of substrate condition on wire fed electron beam additive deposition10.1016/j.msea.2022.143448 ↗
10. Effects of heat accumulation on microstructure and mechanical properties of Ti6Al4V alloy deposited by wire arc additive manufacturing
11. Parametric investigation on Ti6Al4V single beads produced by electron beam freeform fabrication: Geometry, microstructure, composition and hardness
12. Heat treatment for metal additive manufacturing10.1016/j.pmatsci.2022.101051 ↗
13. Wire-based additive manufacturing of Ti-6Al-4V using electron beam technique10.3390/ma13153310 ↗
14. Effect of teat treatment on microstructure and tensile properties of Ti-6Al-4V alloy produced by coaxial electron beam wire feeding additive manufacturing10.1007/s11837-021-04712-z ↗
15. Correlation between heat-treated microstructure and mechanical and fretting wear behavior of electron beam freeform-fabricated Ti6Al4V alloy10.1007/s11837-019-03469-w ↗
16. The inhomogeneous microstructure and mechanical properties of Ti-6Al-4V additively manufactured by electron beam freeform fabrication10.1007/s11661-022-06874-0 ↗
17. Columnar to equiaxed transition during β heat treatment in a near β alloy by laser additive manufacture10.1016/j.jmrt.2021.05.057 ↗
18. Refinement of the grain structure of additive manufactured titanium alloys via epitaxial recrystallization enabled by rapid heat treatment10.1016/j.scriptamat.2020.01.027 ↗
19. Additive manufacturing of Ti-6Al-4V components by shaped metal deposition: microstructure and mechanical properties10.1016/j.matdes.2009.11.032 ↗
20. Wire based additive layer manufacturing: comparison of microstructure and mechanical properties of Ti-6Al-4V components fabricated by laser-beam deposition and shaped metal deposition10.1016/j.jmatprotec.2011.01.018 ↗
21. Heterogeneous microstructure evolution in Ti-6Al-4V alloy thin-wall components deposited by plasma arc additive manufacturing10.1016/j.matdes.2018.07.040 ↗
22. Effects of deposition strategies on macro/microstructure and mechanical properties of wire and arc additive manufactured Ti-6Al-4V10.1016/j.msea.2019.03.001 ↗
23. Effect of α texture on the tensile deformation behavior of Ti-6Al-4V alloy produced via electron beam rapid manufacturing10.1016/j.msea.2018.11.012 ↗
24. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
25. Morphology, microstructure, and hardness of titanium (Ti-6Al-4V) blocks deposited by wire-feed additive layer manufacturing (ALM)10.1016/j.msea.2011.10.095 ↗
26. A new recrystallization at semi-coherent micro-lamella and its effect on tensile properties of wire arc additive manufactured titanium alloy10.1016/j.msea.2018.09.076 ↗
27. Grain morphology evolution and texture characterization of wire and arc additive manufactured Ti-6Al-4V10.1016/j.jallcom.2018.07.235 ↗
28. Microstructure evolution of subcritical annealed laser deposited Ti-6Al-4V alloy10.1016/j.matdes.2011.12.016 ↗
29. Texture evolution during sub-critical annealing and its effect on yield strength anisotropy of laser directed energy deposited Ti-6Al-2Zr-1Mo-1V alloy10.1016/j.msea.2022.143556 ↗
30. Thermal expansion properties of laser melting deposited Ti-6.5Al-2Zr-1Mo-1V alloy during α+β zone annealing10.1016/j.matchar.2017.01.019 ↗
31. Evolution of microstructure of full lamellar titanium alloy BT18Y solutionized at α + β phase field
32. On the origin of microstructural banding in Ti-6Al4V wire-arc based high deposition rate additive manufacturing10.1016/j.actamat.2018.12.038 ↗
33. Microstructure and tensile properties of additive manufactured Ti-6Al-4V with refined prior-β grain structure obtained by rapid heat treatment10.1016/j.msea.2021.141271 ↗
34. The influence of microstructural texture and prior beta grain recrystallisation on the deformation behaviour of laser powder bed fusion produced Ti-6Al-4V10.1016/j.msea.2021.141185 ↗
35. Effect of heat treatment on the crystallographic orientation evolution in a near-α titanium alloy Ti6010.1016/j.actamat.2017.04.007 ↗
36. An investigation on the effect of different multi-step heat treatments on the microstructure, texture and mechanical properties of the DED-produced Ti-6Al-4V alloy10.1016/j.matchar.2022.111958 ↗
37. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
38. Microstructure evolution and mechanical properties of wire-feed electron beam additive manufactured Ti-5Al-2Sn-2Zr-4Mo-4Cr alloy with different subtransus heat treatments10.1016/j.matdes.2020.109063 ↗
39. Graded microstructure and mechanical properties of additive manufactured Ti-6Al-4V via electron beam melting10.1016/j.actamat.2015.06.036 ↗
40. Globularization using heat treatment in additively manufactured Ti-6Al-4V for high strength and toughness10.1016/j.actamat.2018.09.064 ↗
41. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
42. Formation mechanism of the α variant and its influence on the tensile properties of laser solid formed Ti-6Al-4V titanium alloy10.1016/j.msea.2017.03.035 ↗
43. On the texture and mechanical property anisotropy of Ti6Al4V alloy fabricated by powder-bed based laser additive manufacturing10.1016/j.vacuum.2020.109732 ↗