Effect of hydrogen on nanomechanical properties of Inconel 625 studied using in-situ electrochemical nanoindentation technique

Chandrahaasan K. Soundararajan, Dong Wang, Alexey Vinogradov

Abstract

In-situ electrochemical nanoindentation (ECNI) experiment is performed to probe the nanomechanical properties of Inconel 625 alloy under a hydrogen environment. The hydrogen effect on various stages of the load-displacement (LD) plot is quantified. The pop-in load, which indicates the onset of a homogenous dislocation nucleation event, is reduced with hydrogen charging, which augers well with the 'Defactant' concept. The hydrogen solute hinders dislocation glide during pop-in (reduced pop-in width), and the resultant glide resistance force is found to be linearly dependent on dissolved hydrogen concentration. We have also quantified the hydrogen-reduced activation barrier for the secondary source by examining the secondary elastic hardening stage from LD data. Hydrogen charging-induced slip line formation and nanohardness variation at different polarizations are explained using a simple diffusion-desorption model. Furthermore, the electron channeling contrast imaging technique is used to study the dislocation patterns around the indents in air and in the hydrogen environment to shed light on the difference in plastic behavior.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Materials and corrosion trends in offshore and subsea oil and gas production10.1038/s41529-017-0003-4 ↗
2. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
3. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
4. Whitney award lecture—1987: hydrogen—the versatile embrittler10.5006/1.3583875 ↗
5. Equilibrium aspects of hydrogen-induced cracking of steels10.1016/0001-6160(74)90061-3 ↗
6. Lattice defects dominating hydrogen-related failure of metals10.1016/j.actamat.2008.06.031 ↗
7. Superabundant vacancy formation in Ni–H alloys10.1016/S0925-8388(01)01603-6 ↗
8. Revisiting hydrogen embrittlement models and hydrogen-induced homogeneous nucleation of dislocations10.1016/j.scriptamat.2009.09.037 ↗
9. Kirchheim · 2014
10. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
11. Examination of hydrogen embrittlement in FeAl by means of in situ electrochemical micropillar compression and nanoindentation techniques10.1016/j.intermet.2010.01.001 ↗
12. In situ electrochemical microcantilever bending test: a new insight into hydrogen enhanced cracking10.1016/j.scriptamat.2017.01.019 ↗
13. Microstructural and micro-mechanical characterization during hydrogen charging: an in situ scanning electron microscopy study10.1016/j.ijhydene.2018.10.128 ↗
14. A. Barnoush, Hydrogen Embrittlement, Revisited by in Situ Electrochemical Nanoindentation, (2007) 288.
15. Electrochemical nanoindentation: a new approach to probe hydrogen/deformation interaction10.1016/j.scriptamat.2006.03.041 ↗
16. Indentation induced dislocation nucleation: the initial yield point10.1016/1359-6454(96)00010-9 ↗
17. The role of dislocation walls for nanoindentation to shallow depths10.1016/j.ijplas.2008.02.003 ↗
18. Effect of solid solution impurities on dislocation nucleation during nanoindentation10.1557/JMR.2005.0244 ↗
19. Correlation between dislocation density and nanomechanical response during nanoindentation10.1016/j.actamat.2011.11.034 ↗
20. Dislocation mechanisms of radius effect on displacement bursts during spherical nanoindentations10.1557/jmr.2012.183 ↗
21. L. Zhang, T. Ohmura, Plasticity Initiation and Evolution during Nanoindentation of an Iron-3% Silicon Crystal, (2014). doi: 10.1103/PhysRevLett.112.145504.10.1103/PhysRevLett.112.145504 ↗
22. Pop-in phenomenon as a fundamental plasticity probed by nanoindentation technique10.3390/ma14081879 ↗
23. Dislocation velocities, dislocation densities, and plastic flow in lithium fluoride crystals10.1063/1.1735121 ↗
24. In situ nanomechanical characterization of hydrogen effects on nickel-based alloy 725 under different metallurgical conditions
25. Probing the effect of hydrogen on elastic properties and plastic deformation in nickel using nanoindentation and ultrasonic methods10.1007/s11837-018-2850-z ↗
26. Antagonist softening and hardening effects of hydrogen investigated using nanoindentation on cyclically pre-strained nickel single crystal10.1016/j.msea.2020.140480 ↗
27. Hydrogen diffusion and trapping in nickel-based alloy 625: an electrochemical permeation study10.1016/j.electacta.2022.140477 ↗
28. Evaluation of hydrogen diffusion and trapping in nickel Alloy 625 by thermal desorption spectroscopy
29. Probing hydrogen effect on nanomechanical properties of X65 pipeline steel using in-situ electrochemical nanoindentation10.1016/j.msea.2021.141819 ↗
30. Pop-in behavior and elastic-to-plastic transition of polycrystalline pure iron during sharp nanoindentation10.1038/s41598-019-51644-5 ↗
31. Effect of electrochemical charging on the hydrogen embrittlement susceptibility of alloy 71810.1016/j.actamat.2019.08.020 ↗
32. Effect of hydrogen-induced surface steps on the nanomechanical behavior of a CoCrFeMnNi high-entropy alloy revealed by in-situ electrochemical nanoindentation10.1016/j.intermet.2019.106605 ↗
33. Nachweis interstitieller Wasserstoffeinlagerung in NiCu-Legierungen auf magnetischem und röntgenographischem Wege10.1515/zna-1968-1220 ↗
34. X-Ray diffraction measurement of the stacking fault energy reduction induced by hydrogen in an AISI 304 steel10.1016/S1359-6462(97)00332-1 ↗
35. K. Johnson, K. Johnson, Contact Mechanics, 1987. https://books.google.com/books?hl=en&lr=&id=Do6WQlUwbpkC&oi=fnd&pg=PR9&ots=grifmyj97X&sig=kZehZTKCh4P_3duAxdcTlzWqhm4. (Accessed 18 August 2022).
36. Elastic property dependence on mobile and trapped hydrogen in Ni-20110.1007/s11837-016-2157-x ↗
37. Electrochemical nanoindentation study on influence of hydrogen on local mechanical properties of Fcc metals at slow strain rate10.2355/isijinternational.ISIJINT-2015-289 ↗
38. Effect of hydrogen on nanomechanical properties in Fe-22Mn-0.6C TWIP steel revealed by in-situ electrochemical nanoindentation10.1016/j.actamat.2018.12.055 ↗
39. J. Hirth, J. Lothe, Theory of Dislocations, (1982).
40. Resolving the hydrogen effect on dislocation nucleation and mobility by electrochemical nanoindentation10.1016/j.scriptamat.2011.12.004 ↗
41. Atomistic simulations of hydrogen effect on dissociation of screw dislocations in nickel10.1016/j.scriptamat.2005.01.044 ↗
42. The impact of hydrogen on mechanical properties; a new in situ nanoindentation testing method
43. Multiscale simulation of surface step effects on nanoindentation10.1016/j.msea.2005.08.198 ↗
44. Influences of surface preparation on nanoindentation pop-in in single-crystal Mo10.1016/j.scriptamat.2011.05.030 ↗
45. Influence of hydrogen on incipient plasticity in CoCrFeMnNi high-entropy alloy10.1016/j.scriptamat.2018.10.010 ↗
46. The impact of a variety of point defects on the inception of plastic deformation in dislocation-free metals10.1016/j.scriptamat.2011.11.028 ↗
47. Analytical approach for pop-in and post-pop-in deformation behavior during nanoindentation: effect of solute Si in interstitial free steel10.1557/s43578-021-00136-2 ↗
48. Understanding the hydrogen effect on pop-in behavior of an equiatomic high-entropy alloy during in-situ nanoindentation10.1016/j.jmst.2021.04.060 ↗
49. Mechanisms of hydrogen-enhanced localized plasticity: an atomistic study using α-Fe as a model system10.1016/j.actamat.2014.01.008 ↗
50. The influence of hydrogen on the plastic deformation ductility, and fracture of nickel in tension10.1016/0001-6160(63)90209-8 ↗
51. Effects of grain size and deformation temperature on hydrogen-enhanced vacancy formation in Ni alloys10.1016/j.actamat.2017.02.016 ↗
52. Hydrogen-induced strain localization and failure of austenitic stainless steels at high hydrogen concentrations10.1016/0956-7151(91)90211-I ↗
53. Hydrogen effects on dislocation activity in austenitic stainless steel10.1016/j.actamat.2006.02.007 ↗
54. Tabor · 2000
55. Gottstein · 2004
56. Indentation size effects in crystalline materials: a law for strain gradient plasticity10.1016/S0022-5096(97)00086-0 ↗
57. Elastic/plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
58. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
59. Indentation size effect in metallic materials: modeling strength from pop-in to macroscopic hardness using geometrically necessary dislocations10.1016/j.actamat.2006.01.036 ↗
60. Formation and time dynamics of hydrogen-induced vacancies in nickel10.1016/j.actamat.2021.117264 ↗
61. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregationII. Experimental evidence and consequences10.1016/j.actamat.2007.05.033 ↗